METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD

FIELD: powder metallurgy, namely production of article of super-hard materials on base of cubic boron nitride, possibly rough working and shock turning of chilled steels, rough working of cast irons, cutting tools, namely cutting inserts, milling cutters, drills. ^ SUBSTANCE: method comprises steps...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TKACHENKO VALERIJ VALER'EVICH, SALTYKOV VLADIMIR ANATOL'EVICH, ANDRIANOV MIKHAIL ALEKSANDROVICH, EZHOV SERGEJ PETROVICH
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TKACHENKO VALERIJ VALER'EVICH
SALTYKOV VLADIMIR ANATOL'EVICH
ANDRIANOV MIKHAIL ALEKSANDROVICH
EZHOV SERGEJ PETROVICH
description FIELD: powder metallurgy, namely production of article of super-hard materials on base of cubic boron nitride, possibly rough working and shock turning of chilled steels, rough working of cast irons, cutting tools, namely cutting inserts, milling cutters, drills. ^ SUBSTANCE: method comprises steps of activating and chemically copper plating powder of cubic boron nitride with fraction size no more than 10 micrometers; then mechanically mixing copper coated powder of cubic boron nitride and titanium powder with fraction size no more than 10 micrometers; subjecting prepared mixture to thermal vacuum treatment according to schedule: soaking at temperature 650 - 980°C and evacuation degree 1 x 10-5 - 5 x 10-5 Hg mm; soaking at 250 - 350°C and evacuation degree 300 -400 Hg mm; soaking at 700 - 900°C and evacuation degree 1 x 10 -5 - 5 x 10 -5 Hg mm; cooling mixture; increasing pressure till atmospheric one and mechanically mixing prepared mixture with aluminum powder. Prepared charge is placed in container and subjected to hot extrusion at 1100 - 1300°C and 3.5 -4.0 GPa for producing compacted product. Then temperature and pressure are lowered. In second variant of invention before thermal vacuum treatment one of alloys Mo -Al, V - Al, Ni - Al is introduced into mixture and hot extrusion is performed at 1100 - 1300°C or 5.0 - 5.5 GPa. ^ EFFECT: increased shock resistance, improved quality of cutting edge, enhanced cutting properties of tip. ^ 7 cl, 1 tbl, 4 ex
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2284247C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2284247C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2284247C23</originalsourceid><addsrcrecordid>eNqNjrEKwjAYhLs4iPoO9wIusaBr8yc1oZpI8mdwKkXiJFqoD-Ija6mzOB0c38fdvHgdNRuvUPuAU_AqkXV7yEPlGvga0XhqEHS0kSvHoMQ8AmxP8A6yinrEKElLkD58Omc5WKVROfVTn9a0gjwjJjKYniyL2bW7DXn1zUWBWjOZde4fbR767pLv-dmGJMSuFOWWxOYP5A2UOT_t</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD</title><source>esp@cenet</source><creator>TKACHENKO VALERIJ VALER'EVICH ; SALTYKOV VLADIMIR ANATOL'EVICH ; ANDRIANOV MIKHAIL ALEKSANDROVICH ; EZHOV SERGEJ PETROVICH</creator><creatorcontrib>TKACHENKO VALERIJ VALER'EVICH ; SALTYKOV VLADIMIR ANATOL'EVICH ; ANDRIANOV MIKHAIL ALEKSANDROVICH ; EZHOV SERGEJ PETROVICH</creatorcontrib><description>FIELD: powder metallurgy, namely production of article of super-hard materials on base of cubic boron nitride, possibly rough working and shock turning of chilled steels, rough working of cast irons, cutting tools, namely cutting inserts, milling cutters, drills. ^ SUBSTANCE: method comprises steps of activating and chemically copper plating powder of cubic boron nitride with fraction size no more than 10 micrometers; then mechanically mixing copper coated powder of cubic boron nitride and titanium powder with fraction size no more than 10 micrometers; subjecting prepared mixture to thermal vacuum treatment according to schedule: soaking at temperature 650 - 980°C and evacuation degree 1 x 10-5 - 5 x 10-5 Hg mm; soaking at 250 - 350°C and evacuation degree 300 -400 Hg mm; soaking at 700 - 900°C and evacuation degree 1 x 10 -5 - 5 x 10 -5 Hg mm; cooling mixture; increasing pressure till atmospheric one and mechanically mixing prepared mixture with aluminum powder. Prepared charge is placed in container and subjected to hot extrusion at 1100 - 1300°C and 3.5 -4.0 GPa for producing compacted product. Then temperature and pressure are lowered. In second variant of invention before thermal vacuum treatment one of alloys Mo -Al, V - Al, Ni - Al is introduced into mixture and hot extrusion is performed at 1100 - 1300°C or 5.0 - 5.5 GPa. ^ EFFECT: increased shock resistance, improved quality of cutting edge, enhanced cutting properties of tip. ^ 7 cl, 1 tbl, 4 ex</description><language>eng ; rus</language><subject>ARTIFICIAL STONE ; CASTING ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMBINED OPERATIONS ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; MACHINE TOOLS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; METALLURGY ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; POWDER METALLURGY ; REFRACTORIES ; SLAG ; TRANSPORTING ; TREATMENT OF NATURAL STONE ; UNIVERSAL MACHINE TOOLS ; WORKING METALLIC POWDER</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060927&amp;DB=EPODOC&amp;CC=RU&amp;NR=2284247C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060927&amp;DB=EPODOC&amp;CC=RU&amp;NR=2284247C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TKACHENKO VALERIJ VALER'EVICH</creatorcontrib><creatorcontrib>SALTYKOV VLADIMIR ANATOL'EVICH</creatorcontrib><creatorcontrib>ANDRIANOV MIKHAIL ALEKSANDROVICH</creatorcontrib><creatorcontrib>EZHOV SERGEJ PETROVICH</creatorcontrib><title>METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD</title><description>FIELD: powder metallurgy, namely production of article of super-hard materials on base of cubic boron nitride, possibly rough working and shock turning of chilled steels, rough working of cast irons, cutting tools, namely cutting inserts, milling cutters, drills. ^ SUBSTANCE: method comprises steps of activating and chemically copper plating powder of cubic boron nitride with fraction size no more than 10 micrometers; then mechanically mixing copper coated powder of cubic boron nitride and titanium powder with fraction size no more than 10 micrometers; subjecting prepared mixture to thermal vacuum treatment according to schedule: soaking at temperature 650 - 980°C and evacuation degree 1 x 10-5 - 5 x 10-5 Hg mm; soaking at 250 - 350°C and evacuation degree 300 -400 Hg mm; soaking at 700 - 900°C and evacuation degree 1 x 10 -5 - 5 x 10 -5 Hg mm; cooling mixture; increasing pressure till atmospheric one and mechanically mixing prepared mixture with aluminum powder. Prepared charge is placed in container and subjected to hot extrusion at 1100 - 1300°C and 3.5 -4.0 GPa for producing compacted product. Then temperature and pressure are lowered. In second variant of invention before thermal vacuum treatment one of alloys Mo -Al, V - Al, Ni - Al is introduced into mixture and hot extrusion is performed at 1100 - 1300°C or 5.0 - 5.5 GPa. ^ EFFECT: increased shock resistance, improved quality of cutting edge, enhanced cutting properties of tip. ^ 7 cl, 1 tbl, 4 ex</description><subject>ARTIFICIAL STONE</subject><subject>CASTING</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMBINED OPERATIONS</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>MACHINE TOOLS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>METALLURGY</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>UNIVERSAL MACHINE TOOLS</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjrEKwjAYhLs4iPoO9wIusaBr8yc1oZpI8mdwKkXiJFqoD-Ija6mzOB0c38fdvHgdNRuvUPuAU_AqkXV7yEPlGvga0XhqEHS0kSvHoMQ8AmxP8A6yinrEKElLkD58Omc5WKVROfVTn9a0gjwjJjKYniyL2bW7DXn1zUWBWjOZde4fbR767pLv-dmGJMSuFOWWxOYP5A2UOT_t</recordid><startdate>20060927</startdate><enddate>20060927</enddate><creator>TKACHENKO VALERIJ VALER'EVICH</creator><creator>SALTYKOV VLADIMIR ANATOL'EVICH</creator><creator>ANDRIANOV MIKHAIL ALEKSANDROVICH</creator><creator>EZHOV SERGEJ PETROVICH</creator><scope>EVB</scope></search><sort><creationdate>20060927</creationdate><title>METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD</title><author>TKACHENKO VALERIJ VALER'EVICH ; SALTYKOV VLADIMIR ANATOL'EVICH ; ANDRIANOV MIKHAIL ALEKSANDROVICH ; EZHOV SERGEJ PETROVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2284247C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2006</creationdate><topic>ARTIFICIAL STONE</topic><topic>CASTING</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMBINED OPERATIONS</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>MACHINE TOOLS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>METALLURGY</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>UNIVERSAL MACHINE TOOLS</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>TKACHENKO VALERIJ VALER'EVICH</creatorcontrib><creatorcontrib>SALTYKOV VLADIMIR ANATOL'EVICH</creatorcontrib><creatorcontrib>ANDRIANOV MIKHAIL ALEKSANDROVICH</creatorcontrib><creatorcontrib>EZHOV SERGEJ PETROVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TKACHENKO VALERIJ VALER'EVICH</au><au>SALTYKOV VLADIMIR ANATOL'EVICH</au><au>ANDRIANOV MIKHAIL ALEKSANDROVICH</au><au>EZHOV SERGEJ PETROVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD</title><date>2006-09-27</date><risdate>2006</risdate><abstract>FIELD: powder metallurgy, namely production of article of super-hard materials on base of cubic boron nitride, possibly rough working and shock turning of chilled steels, rough working of cast irons, cutting tools, namely cutting inserts, milling cutters, drills. ^ SUBSTANCE: method comprises steps of activating and chemically copper plating powder of cubic boron nitride with fraction size no more than 10 micrometers; then mechanically mixing copper coated powder of cubic boron nitride and titanium powder with fraction size no more than 10 micrometers; subjecting prepared mixture to thermal vacuum treatment according to schedule: soaking at temperature 650 - 980°C and evacuation degree 1 x 10-5 - 5 x 10-5 Hg mm; soaking at 250 - 350°C and evacuation degree 300 -400 Hg mm; soaking at 700 - 900°C and evacuation degree 1 x 10 -5 - 5 x 10 -5 Hg mm; cooling mixture; increasing pressure till atmospheric one and mechanically mixing prepared mixture with aluminum powder. Prepared charge is placed in container and subjected to hot extrusion at 1100 - 1300°C and 3.5 -4.0 GPa for producing compacted product. Then temperature and pressure are lowered. In second variant of invention before thermal vacuum treatment one of alloys Mo -Al, V - Al, Ni - Al is introduced into mixture and hot extrusion is performed at 1100 - 1300°C or 5.0 - 5.5 GPa. ^ EFFECT: increased shock resistance, improved quality of cutting edge, enhanced cutting properties of tip. ^ 7 cl, 1 tbl, 4 ex</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2284247C2
source esp@cenet
subjects ARTIFICIAL STONE
CASTING
CEMENTS
CERAMICS
CHEMISTRY
COMBINED OPERATIONS
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
MACHINE TOOLS
MAKING METALLIC POWDER
MANUFACTURE OF ARTICLES FROM METALLIC POWDER
METAL-WORKING NOT OTHERWISE PROVIDED FOR
METALLURGY
OTHER WORKING OF METAL
PERFORMING OPERATIONS
POWDER METALLURGY
REFRACTORIES
SLAG
TRANSPORTING
TREATMENT OF NATURAL STONE
UNIVERSAL MACHINE TOOLS
WORKING METALLIC POWDER
title METHOD FOR PRODUCING BLANK OF SHOCK RESISTANT CUTTING TIP ON BASE OF CUBIC BORON NITRIDE AND SHOCK RESISTANT CUTTING TIP PRODUCED BY SUCH METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T22%3A58%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TKACHENKO%20VALERIJ%20VALER'EVICH&rft.date=2006-09-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2284247C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true