METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING
FIELD: possibility for selecting modes of restoring worn parts by electric contact surfacing. ^ SUBSTANCE: method comprises steps of surfacing additive wire onto sample and measuring deformation of additive wire; detecting joining zone by extracting from contact surface area surface portions without...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; rus |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | NAFIKOV MARAT ZAKIEVICH |
description | FIELD: possibility for selecting modes of restoring worn parts by electric contact surfacing. ^ SUBSTANCE: method comprises steps of surfacing additive wire onto sample and measuring deformation of additive wire; detecting joining zone by extracting from contact surface area surface portions without said joint; measuring as deformation parameters of additive wire width of surfaced bead and summed axial deformation of additive wire for determining percentage axial deformation of wire; determining size of contact land between additive metal and sample while taking into account real values of additive wire upsetting at side of sample and at side of roller; determining boundary of zone of welded joint formation in range of contact land while taking into account tension stresses occurring in cross sections of plastically deformed additive wire to be compared with limit creep of additive metal at given temperature. ^ EFFECT: improved accuracy of detecting zone of surfacing formation. ^ 5 dwg, 3 ex |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2278009C1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2278009C1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2278009C13</originalsourceid><addsrcrecordid>eNrjZIj1dQ3x8HdRcPMPUnBxDXF1DvH0c1eI8vdzVfB3U_Dy9_QD8YFMoDpHHwVnf0ewgnDPEA8FJ8dgVwXHEAVXH6C2IE9noKxfiKNziEJwaJCbozNQHQ8Da1piTnEqL5TmZlBwcw1x9tBNLciPTy0uSExOzUstiQ8KNTIytzAwsHQ2NCZCCQBEEzHc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING</title><source>esp@cenet</source><creator>NAFIKOV MARAT ZAKIEVICH</creator><creatorcontrib>NAFIKOV MARAT ZAKIEVICH</creatorcontrib><description>FIELD: possibility for selecting modes of restoring worn parts by electric contact surfacing. ^ SUBSTANCE: method comprises steps of surfacing additive wire onto sample and measuring deformation of additive wire; detecting joining zone by extracting from contact surface area surface portions without said joint; measuring as deformation parameters of additive wire width of surfaced bead and summed axial deformation of additive wire for determining percentage axial deformation of wire; determining size of contact land between additive metal and sample while taking into account real values of additive wire upsetting at side of sample and at side of roller; determining boundary of zone of welded joint formation in range of contact land while taking into account tension stresses occurring in cross sections of plastically deformed additive wire to be compared with limit creep of additive metal at given temperature. ^ EFFECT: improved accuracy of detecting zone of surfacing formation. ^ 5 dwg, 3 ex</description><language>eng ; rus</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20060620&DB=EPODOC&CC=RU&NR=2278009C1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20060620&DB=EPODOC&CC=RU&NR=2278009C1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NAFIKOV MARAT ZAKIEVICH</creatorcontrib><title>METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING</title><description>FIELD: possibility for selecting modes of restoring worn parts by electric contact surfacing. ^ SUBSTANCE: method comprises steps of surfacing additive wire onto sample and measuring deformation of additive wire; detecting joining zone by extracting from contact surface area surface portions without said joint; measuring as deformation parameters of additive wire width of surfaced bead and summed axial deformation of additive wire for determining percentage axial deformation of wire; determining size of contact land between additive metal and sample while taking into account real values of additive wire upsetting at side of sample and at side of roller; determining boundary of zone of welded joint formation in range of contact land while taking into account tension stresses occurring in cross sections of plastically deformed additive wire to be compared with limit creep of additive metal at given temperature. ^ EFFECT: improved accuracy of detecting zone of surfacing formation. ^ 5 dwg, 3 ex</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZIj1dQ3x8HdRcPMPUnBxDXF1DvH0c1eI8vdzVfB3U_Dy9_QD8YFMoDpHHwVnf0ewgnDPEA8FJ8dgVwXHEAVXH6C2IE9noKxfiKNziEJwaJCbozNQHQ8Da1piTnEqL5TmZlBwcw1x9tBNLciPTy0uSExOzUstiQ8KNTIytzAwsHQ2NCZCCQBEEzHc</recordid><startdate>20060620</startdate><enddate>20060620</enddate><creator>NAFIKOV MARAT ZAKIEVICH</creator><scope>EVB</scope></search><sort><creationdate>20060620</creationdate><title>METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING</title><author>NAFIKOV MARAT ZAKIEVICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2278009C13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2006</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>NAFIKOV MARAT ZAKIEVICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NAFIKOV MARAT ZAKIEVICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING</title><date>2006-06-20</date><risdate>2006</risdate><abstract>FIELD: possibility for selecting modes of restoring worn parts by electric contact surfacing. ^ SUBSTANCE: method comprises steps of surfacing additive wire onto sample and measuring deformation of additive wire; detecting joining zone by extracting from contact surface area surface portions without said joint; measuring as deformation parameters of additive wire width of surfaced bead and summed axial deformation of additive wire for determining percentage axial deformation of wire; determining size of contact land between additive metal and sample while taking into account real values of additive wire upsetting at side of sample and at side of roller; determining boundary of zone of welded joint formation in range of contact land while taking into account tension stresses occurring in cross sections of plastically deformed additive wire to be compared with limit creep of additive metal at given temperature. ^ EFFECT: improved accuracy of detecting zone of surfacing formation. ^ 5 dwg, 3 ex</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; rus |
recordid | cdi_epo_espacenet_RU2278009C1 |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | METHOD FOR DETECTING ZONE OF JOINING OF METAL COATING WITH BASE AT ELECTRIC CONTACT SURFACING |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T03%3A07%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NAFIKOV%20MARAT%20ZAKIEVICH&rft.date=2006-06-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2278009C1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |