METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL

FIELD: metallurgy; rolling process; hardening working gauges of steel rolls of section rolling mils. SUBSTANCE: proposed method includes mechanical turning of roll followed by heating it to temperature of 300-370 C at rate of 50-100 C/h. Subsequent hard-facing is performed at rate of 30-40 m/h and d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KHOREV G.A, NIKIFOROV V.V, MONID V.A, TRAJNO A.I, TJAPAEV O.V, ROVKIN A.M, LUTSENKO A.N
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KHOREV G.A
NIKIFOROV V.V
MONID V.A
TRAJNO A.I
TJAPAEV O.V
ROVKIN A.M
LUTSENKO A.N
description FIELD: metallurgy; rolling process; hardening working gauges of steel rolls of section rolling mils. SUBSTANCE: proposed method includes mechanical turning of roll followed by heating it to temperature of 300-370 C at rate of 50-100 C/h. Subsequent hard-facing is performed at rate of 30-40 m/h and density of electric current of 40-45 A/sq mm. Then, heat treatment is performed to temperature of 450-500 C continued for 1.5-2 h. EFFECT: enhanced resistance of rolls. 2 cl, 1 tbl, 6 ex
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2228958C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2228958C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2228958C23</originalsourceid><addsrcrecordid>eNrjZLD0dQ3x8HdR8HdT8HAMcnH18_RzB3GCQ1xdfRSC_H18wDxX5xBPfz8wH6TA19PHh4eBNS0xpziVF0pzMyi4uYY4e-imFuTHpxYXJCan5qWWxAeFGhkZWViaWjgbGROhBAAYkyg6</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL</title><source>esp@cenet</source><creator>KHOREV G.A ; NIKIFOROV V.V ; MONID V.A ; TRAJNO A.I ; TJAPAEV O.V ; ROVKIN A.M ; LUTSENKO A.N</creator><creatorcontrib>KHOREV G.A ; NIKIFOROV V.V ; MONID V.A ; TRAJNO A.I ; TJAPAEV O.V ; ROVKIN A.M ; LUTSENKO A.N</creatorcontrib><description>FIELD: metallurgy; rolling process; hardening working gauges of steel rolls of section rolling mils. SUBSTANCE: proposed method includes mechanical turning of roll followed by heating it to temperature of 300-370 C at rate of 50-100 C/h. Subsequent hard-facing is performed at rate of 30-40 m/h and density of electric current of 40-45 A/sq mm. Then, heat treatment is performed to temperature of 450-500 C continued for 1.5-2 h. EFFECT: enhanced resistance of rolls. 2 cl, 1 tbl, 6 ex</description><edition>7</edition><language>eng ; rus</language><subject>CHEMISTRY ; COMBINED OPERATIONS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MACHINE TOOLS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; UNIVERSAL MACHINE TOOLS</subject><creationdate>2004</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20040520&amp;DB=EPODOC&amp;CC=RU&amp;NR=2228958C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20040520&amp;DB=EPODOC&amp;CC=RU&amp;NR=2228958C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KHOREV G.A</creatorcontrib><creatorcontrib>NIKIFOROV V.V</creatorcontrib><creatorcontrib>MONID V.A</creatorcontrib><creatorcontrib>TRAJNO A.I</creatorcontrib><creatorcontrib>TJAPAEV O.V</creatorcontrib><creatorcontrib>ROVKIN A.M</creatorcontrib><creatorcontrib>LUTSENKO A.N</creatorcontrib><title>METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL</title><description>FIELD: metallurgy; rolling process; hardening working gauges of steel rolls of section rolling mils. SUBSTANCE: proposed method includes mechanical turning of roll followed by heating it to temperature of 300-370 C at rate of 50-100 C/h. Subsequent hard-facing is performed at rate of 30-40 m/h and density of electric current of 40-45 A/sq mm. Then, heat treatment is performed to temperature of 450-500 C continued for 1.5-2 h. EFFECT: enhanced resistance of rolls. 2 cl, 1 tbl, 6 ex</description><subject>CHEMISTRY</subject><subject>COMBINED OPERATIONS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MACHINE TOOLS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>UNIVERSAL MACHINE TOOLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2004</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD0dQ3x8HdR8HdT8HAMcnH18_RzB3GCQ1xdfRSC_H18wDxX5xBPfz8wH6TA19PHh4eBNS0xpziVF0pzMyi4uYY4e-imFuTHpxYXJCan5qWWxAeFGhkZWViaWjgbGROhBAAYkyg6</recordid><startdate>20040520</startdate><enddate>20040520</enddate><creator>KHOREV G.A</creator><creator>NIKIFOROV V.V</creator><creator>MONID V.A</creator><creator>TRAJNO A.I</creator><creator>TJAPAEV O.V</creator><creator>ROVKIN A.M</creator><creator>LUTSENKO A.N</creator><scope>EVB</scope></search><sort><creationdate>20040520</creationdate><title>METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL</title><author>KHOREV G.A ; NIKIFOROV V.V ; MONID V.A ; TRAJNO A.I ; TJAPAEV O.V ; ROVKIN A.M ; LUTSENKO A.N</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2228958C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2004</creationdate><topic>CHEMISTRY</topic><topic>COMBINED OPERATIONS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MACHINE TOOLS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>UNIVERSAL MACHINE TOOLS</topic><toplevel>online_resources</toplevel><creatorcontrib>KHOREV G.A</creatorcontrib><creatorcontrib>NIKIFOROV V.V</creatorcontrib><creatorcontrib>MONID V.A</creatorcontrib><creatorcontrib>TRAJNO A.I</creatorcontrib><creatorcontrib>TJAPAEV O.V</creatorcontrib><creatorcontrib>ROVKIN A.M</creatorcontrib><creatorcontrib>LUTSENKO A.N</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KHOREV G.A</au><au>NIKIFOROV V.V</au><au>MONID V.A</au><au>TRAJNO A.I</au><au>TJAPAEV O.V</au><au>ROVKIN A.M</au><au>LUTSENKO A.N</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL</title><date>2004-05-20</date><risdate>2004</risdate><abstract>FIELD: metallurgy; rolling process; hardening working gauges of steel rolls of section rolling mils. SUBSTANCE: proposed method includes mechanical turning of roll followed by heating it to temperature of 300-370 C at rate of 50-100 C/h. Subsequent hard-facing is performed at rate of 30-40 m/h and density of electric current of 40-45 A/sq mm. Then, heat treatment is performed to temperature of 450-500 C continued for 1.5-2 h. EFFECT: enhanced resistance of rolls. 2 cl, 1 tbl, 6 ex</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2228958C2
source esp@cenet
subjects CHEMISTRY
COMBINED OPERATIONS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MACHINE TOOLS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METAL-WORKING NOT OTHERWISE PROVIDED FOR
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
OTHER WORKING OF METAL
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
UNIVERSAL MACHINE TOOLS
title METHOD OF HARDENING OF STEEL ROLL OF SECTION ROLLING MILL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T13%3A32%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KHOREV%20G.A&rft.date=2004-05-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2228958C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true