BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER
FIELD: nonferrous metallurgy. SUBSTANCE: bipolar electrode has anode part from graphite and cathode part from iron with intermediate contact layer of copper located between them. Intermediate contact layer is made by deposition of copper layer 0.01-2 mm thick by method of electric arc spraying. EFFE...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | RUBEL' O.A GORSHKOV JU.V VAAL I.V RJAPOSOV JU.A BELKIN G.I BELKIN N.A ZHITKOVA T.I SHUNDIKOV O.N BRAGIN V.A LEONOVA K.D |
description | FIELD: nonferrous metallurgy. SUBSTANCE: bipolar electrode has anode part from graphite and cathode part from iron with intermediate contact layer of copper located between them. Intermediate contact layer is made by deposition of copper layer 0.01-2 mm thick by method of electric arc spraying. EFFECT: excluded diffusion and electrochemical processes in graphite pores, increased bipole operate reliability, reduced power consumption. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2207405C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2207405C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2207405C23</originalsourceid><addsrcrecordid>eNrjZNB28gzw93EMUnD1cXUOCfJ3cVXwd1PwdXT3cw32DPWFCftERrkG8TCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQIyMDcxMDU2cjYyKUAAA-HyTL</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER</title><source>esp@cenet</source><creator>RUBEL' O.A ; GORSHKOV JU.V ; VAAL I.V ; RJAPOSOV JU.A ; BELKIN G.I ; BELKIN N.A ; ZHITKOVA T.I ; SHUNDIKOV O.N ; BRAGIN V.A ; LEONOVA K.D</creator><creatorcontrib>RUBEL' O.A ; GORSHKOV JU.V ; VAAL I.V ; RJAPOSOV JU.A ; BELKIN G.I ; BELKIN N.A ; ZHITKOVA T.I ; SHUNDIKOV O.N ; BRAGIN V.A ; LEONOVA K.D</creatorcontrib><description>FIELD: nonferrous metallurgy. SUBSTANCE: bipolar electrode has anode part from graphite and cathode part from iron with intermediate contact layer of copper located between them. Intermediate contact layer is made by deposition of copper layer 0.01-2 mm thick by method of electric arc spraying. EFFECT: excluded diffusion and electrochemical processes in graphite pores, increased bipole operate reliability, reduced power consumption.</description><edition>7</edition><language>eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20030627&DB=EPODOC&CC=RU&NR=2207405C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20030627&DB=EPODOC&CC=RU&NR=2207405C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>RUBEL' O.A</creatorcontrib><creatorcontrib>GORSHKOV JU.V</creatorcontrib><creatorcontrib>VAAL I.V</creatorcontrib><creatorcontrib>RJAPOSOV JU.A</creatorcontrib><creatorcontrib>BELKIN G.I</creatorcontrib><creatorcontrib>BELKIN N.A</creatorcontrib><creatorcontrib>ZHITKOVA T.I</creatorcontrib><creatorcontrib>SHUNDIKOV O.N</creatorcontrib><creatorcontrib>BRAGIN V.A</creatorcontrib><creatorcontrib>LEONOVA K.D</creatorcontrib><title>BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER</title><description>FIELD: nonferrous metallurgy. SUBSTANCE: bipolar electrode has anode part from graphite and cathode part from iron with intermediate contact layer of copper located between them. Intermediate contact layer is made by deposition of copper layer 0.01-2 mm thick by method of electric arc spraying. EFFECT: excluded diffusion and electrochemical processes in graphite pores, increased bipole operate reliability, reduced power consumption.</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNB28gzw93EMUnD1cXUOCfJ3cVXwd1PwdXT3cw32DPWFCftERrkG8TCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQIyMDcxMDU2cjYyKUAAA-HyTL</recordid><startdate>20030627</startdate><enddate>20030627</enddate><creator>RUBEL' O.A</creator><creator>GORSHKOV JU.V</creator><creator>VAAL I.V</creator><creator>RJAPOSOV JU.A</creator><creator>BELKIN G.I</creator><creator>BELKIN N.A</creator><creator>ZHITKOVA T.I</creator><creator>SHUNDIKOV O.N</creator><creator>BRAGIN V.A</creator><creator>LEONOVA K.D</creator><scope>EVB</scope></search><sort><creationdate>20030627</creationdate><title>BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER</title><author>RUBEL' O.A ; GORSHKOV JU.V ; VAAL I.V ; RJAPOSOV JU.A ; BELKIN G.I ; BELKIN N.A ; ZHITKOVA T.I ; SHUNDIKOV O.N ; BRAGIN V.A ; LEONOVA K.D</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2207405C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>RUBEL' O.A</creatorcontrib><creatorcontrib>GORSHKOV JU.V</creatorcontrib><creatorcontrib>VAAL I.V</creatorcontrib><creatorcontrib>RJAPOSOV JU.A</creatorcontrib><creatorcontrib>BELKIN G.I</creatorcontrib><creatorcontrib>BELKIN N.A</creatorcontrib><creatorcontrib>ZHITKOVA T.I</creatorcontrib><creatorcontrib>SHUNDIKOV O.N</creatorcontrib><creatorcontrib>BRAGIN V.A</creatorcontrib><creatorcontrib>LEONOVA K.D</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>RUBEL' O.A</au><au>GORSHKOV JU.V</au><au>VAAL I.V</au><au>RJAPOSOV JU.A</au><au>BELKIN G.I</au><au>BELKIN N.A</au><au>ZHITKOVA T.I</au><au>SHUNDIKOV O.N</au><au>BRAGIN V.A</au><au>LEONOVA K.D</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER</title><date>2003-06-27</date><risdate>2003</risdate><abstract>FIELD: nonferrous metallurgy. SUBSTANCE: bipolar electrode has anode part from graphite and cathode part from iron with intermediate contact layer of copper located between them. Intermediate contact layer is made by deposition of copper layer 0.01-2 mm thick by method of electric arc spraying. EFFECT: excluded diffusion and electrochemical processes in graphite pores, increased bipole operate reliability, reduced power consumption.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_RU2207405C2 |
source | esp@cenet |
subjects | APPARATUS THEREFOR CHEMISTRY ELECTROLYTIC OR ELECTROPHORETIC PROCESSES METALLURGY PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS |
title | BIPOLAR ELECTRODE OF MAGNESIUM ELECTROLYZER |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T20%3A25%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=RUBEL'%20O.A&rft.date=2003-06-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2207405C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |