TWO-LAYER CORROSION-RESISTANT STEEL

FIELD: metallurgy of complex-alloy steels, two-layer corrosion-resistant steels in particular; manufacture of heat-exchange apparatus. SUBSTANCE: proposed steel is resistant to corrosion in flow of molten metal agent on base of lead or lead and bismuth alloy and to corrosion cracking of water-and-va...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JAKOVLEV V.A, STEPANOV V.S, KARZOV G.P, TRET'JAKOV N.V, MARKOV V.G, DRAGUNOV JU.G
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JAKOVLEV V.A
STEPANOV V.S
KARZOV G.P
TRET'JAKOV N.V
MARKOV V.G
DRAGUNOV JU.G
description FIELD: metallurgy of complex-alloy steels, two-layer corrosion-resistant steels in particular; manufacture of heat-exchange apparatus. SUBSTANCE: proposed steel is resistant to corrosion in flow of molten metal agent on base of lead or lead and bismuth alloy and to corrosion cracking of water-and-vapor medium at temperature of 500 C. Proposed steel consisting of main and clad layers includes the following components, mass-%: carbon, 0.005- 0/0.04; silicon, 2.20-2.80; manganese, 0.50-1.00; chromium, 14.0-25.5; nickel, 10.5-12.5; molybdenum, 0.8-1.2; titanium, 0.08-0.20 and the remainder being iron which are included in main layer; clad layer contains the following components, mass-%: carbon, 0.005-0.03;silicon, 0.05-0.35; manganese, 1.30-1.17; chromium, 20.0-22.0; nickel, 31.5- 33.0; molybdenum, 3.0-4.0; titanium, 0.05-0.50; copper, 0.01-0.15; niobium, 0.90-1.20 and the remainder being iron at (Nb+2Ti)/C>=35; thickness of clad layer ranges from 0.20 to 0.50 of total thickness of steel. EFFECT: enhanced corrosion resistance of steel. 4 tbl
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2206632C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2206632C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2206632C23</originalsourceid><addsrcrecordid>eNrjZFAOCffX9XGMdA1ScPYPCvIP9vT30w1yDfYMDnH0C1EIDnF19eFhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUZGBmZmxkbORsZEKAEAQoYizw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>TWO-LAYER CORROSION-RESISTANT STEEL</title><source>esp@cenet</source><creator>JAKOVLEV V.A ; STEPANOV V.S ; KARZOV G.P ; TRET'JAKOV N.V ; MARKOV V.G ; DRAGUNOV JU.G</creator><creatorcontrib>JAKOVLEV V.A ; STEPANOV V.S ; KARZOV G.P ; TRET'JAKOV N.V ; MARKOV V.G ; DRAGUNOV JU.G</creatorcontrib><description>FIELD: metallurgy of complex-alloy steels, two-layer corrosion-resistant steels in particular; manufacture of heat-exchange apparatus. SUBSTANCE: proposed steel is resistant to corrosion in flow of molten metal agent on base of lead or lead and bismuth alloy and to corrosion cracking of water-and-vapor medium at temperature of 500 C. Proposed steel consisting of main and clad layers includes the following components, mass-%: carbon, 0.005- 0/0.04; silicon, 2.20-2.80; manganese, 0.50-1.00; chromium, 14.0-25.5; nickel, 10.5-12.5; molybdenum, 0.8-1.2; titanium, 0.08-0.20 and the remainder being iron which are included in main layer; clad layer contains the following components, mass-%: carbon, 0.005-0.03;silicon, 0.05-0.35; manganese, 1.30-1.17; chromium, 20.0-22.0; nickel, 31.5- 33.0; molybdenum, 3.0-4.0; titanium, 0.05-0.50; copper, 0.01-0.15; niobium, 0.90-1.20 and the remainder being iron at (Nb+2Ti)/C&gt;=35; thickness of clad layer ranges from 0.20 to 0.50 of total thickness of steel. EFFECT: enhanced corrosion resistance of steel. 4 tbl</description><edition>7</edition><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; METALLURGY ; PERFORMING OPERATIONS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030620&amp;DB=EPODOC&amp;CC=RU&amp;NR=2206632C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030620&amp;DB=EPODOC&amp;CC=RU&amp;NR=2206632C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JAKOVLEV V.A</creatorcontrib><creatorcontrib>STEPANOV V.S</creatorcontrib><creatorcontrib>KARZOV G.P</creatorcontrib><creatorcontrib>TRET'JAKOV N.V</creatorcontrib><creatorcontrib>MARKOV V.G</creatorcontrib><creatorcontrib>DRAGUNOV JU.G</creatorcontrib><title>TWO-LAYER CORROSION-RESISTANT STEEL</title><description>FIELD: metallurgy of complex-alloy steels, two-layer corrosion-resistant steels in particular; manufacture of heat-exchange apparatus. SUBSTANCE: proposed steel is resistant to corrosion in flow of molten metal agent on base of lead or lead and bismuth alloy and to corrosion cracking of water-and-vapor medium at temperature of 500 C. Proposed steel consisting of main and clad layers includes the following components, mass-%: carbon, 0.005- 0/0.04; silicon, 2.20-2.80; manganese, 0.50-1.00; chromium, 14.0-25.5; nickel, 10.5-12.5; molybdenum, 0.8-1.2; titanium, 0.08-0.20 and the remainder being iron which are included in main layer; clad layer contains the following components, mass-%: carbon, 0.005-0.03;silicon, 0.05-0.35; manganese, 1.30-1.17; chromium, 20.0-22.0; nickel, 31.5- 33.0; molybdenum, 3.0-4.0; titanium, 0.05-0.50; copper, 0.01-0.15; niobium, 0.90-1.20 and the remainder being iron at (Nb+2Ti)/C&gt;=35; thickness of clad layer ranges from 0.20 to 0.50 of total thickness of steel. EFFECT: enhanced corrosion resistance of steel. 4 tbl</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFAOCffX9XGMdA1ScPYPCvIP9vT30w1yDfYMDnH0C1EIDnF19eFhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUZGBmZmxkbORsZEKAEAQoYizw</recordid><startdate>20030620</startdate><enddate>20030620</enddate><creator>JAKOVLEV V.A</creator><creator>STEPANOV V.S</creator><creator>KARZOV G.P</creator><creator>TRET'JAKOV N.V</creator><creator>MARKOV V.G</creator><creator>DRAGUNOV JU.G</creator><scope>EVB</scope></search><sort><creationdate>20030620</creationdate><title>TWO-LAYER CORROSION-RESISTANT STEEL</title><author>JAKOVLEV V.A ; STEPANOV V.S ; KARZOV G.P ; TRET'JAKOV N.V ; MARKOV V.G ; DRAGUNOV JU.G</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2206632C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>JAKOVLEV V.A</creatorcontrib><creatorcontrib>STEPANOV V.S</creatorcontrib><creatorcontrib>KARZOV G.P</creatorcontrib><creatorcontrib>TRET'JAKOV N.V</creatorcontrib><creatorcontrib>MARKOV V.G</creatorcontrib><creatorcontrib>DRAGUNOV JU.G</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JAKOVLEV V.A</au><au>STEPANOV V.S</au><au>KARZOV G.P</au><au>TRET'JAKOV N.V</au><au>MARKOV V.G</au><au>DRAGUNOV JU.G</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>TWO-LAYER CORROSION-RESISTANT STEEL</title><date>2003-06-20</date><risdate>2003</risdate><abstract>FIELD: metallurgy of complex-alloy steels, two-layer corrosion-resistant steels in particular; manufacture of heat-exchange apparatus. SUBSTANCE: proposed steel is resistant to corrosion in flow of molten metal agent on base of lead or lead and bismuth alloy and to corrosion cracking of water-and-vapor medium at temperature of 500 C. Proposed steel consisting of main and clad layers includes the following components, mass-%: carbon, 0.005- 0/0.04; silicon, 2.20-2.80; manganese, 0.50-1.00; chromium, 14.0-25.5; nickel, 10.5-12.5; molybdenum, 0.8-1.2; titanium, 0.08-0.20 and the remainder being iron which are included in main layer; clad layer contains the following components, mass-%: carbon, 0.005-0.03;silicon, 0.05-0.35; manganese, 1.30-1.17; chromium, 20.0-22.0; nickel, 31.5- 33.0; molybdenum, 3.0-4.0; titanium, 0.05-0.50; copper, 0.01-0.15; niobium, 0.90-1.20 and the remainder being iron at (Nb+2Ti)/C&gt;=35; thickness of clad layer ranges from 0.20 to 0.50 of total thickness of steel. EFFECT: enhanced corrosion resistance of steel. 4 tbl</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_RU2206632C2
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
LAYERED PRODUCTS
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
METALLURGY
PERFORMING OPERATIONS
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title TWO-LAYER CORROSION-RESISTANT STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T02%3A43%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JAKOVLEV%20V.A&rft.date=2003-06-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2206632C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true