METHOD OF MANUFACTURING SPONGE IRON

metallurgy. SUBSTANCE: method includes direct reduction of ground material containing iron oxide with reducing gas formed in melting and falsifying zone from carbon carriers and oxygen-containing gas. Reducing gas contains from 20 to 100 g/Ncu.m of dust at carbon content ranging from 30 to 70 mas.%...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: VALLNER FELIKS, GENNARI UDO, KEPPLINGER LEOPOL'D VERNER
Format: Patent
Sprache:eng ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator VALLNER FELIKS
GENNARI UDO
KEPPLINGER LEOPOL'D VERNER
description metallurgy. SUBSTANCE: method includes direct reduction of ground material containing iron oxide with reducing gas formed in melting and falsifying zone from carbon carriers and oxygen-containing gas. Reducing gas contains from 20 to 100 g/Ncu.m of dust at carbon content ranging from 30 to 70 mas.% of material containing iron oxide is subjected to action of reducing gas during period of time which exceeds period required for complete reduction, thus making it possible to obtain sponge iron at increased content of carbon. EFFECT: enhanced efficiency. 6 cl, 3 dwg, 5 tbl, 1 ex
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RU2176672C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RU2176672C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RU2176672C23</originalsourceid><addsrcrecordid>eNrjZFD2dQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1cIDvD3c3dV8Azy9-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUaG5mZm5kbORsZEKAEAHg4iiA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MANUFACTURING SPONGE IRON</title><source>esp@cenet</source><creator>VALLNER FELIKS ; GENNARI UDO ; KEPPLINGER LEOPOL'D VERNER</creator><creatorcontrib>VALLNER FELIKS ; GENNARI UDO ; KEPPLINGER LEOPOL'D VERNER</creatorcontrib><description>metallurgy. SUBSTANCE: method includes direct reduction of ground material containing iron oxide with reducing gas formed in melting and falsifying zone from carbon carriers and oxygen-containing gas. Reducing gas contains from 20 to 100 g/Ncu.m of dust at carbon content ranging from 30 to 70 mas.% of material containing iron oxide is subjected to action of reducing gas during period of time which exceeds period required for complete reduction, thus making it possible to obtain sponge iron at increased content of carbon. EFFECT: enhanced efficiency. 6 cl, 3 dwg, 5 tbl, 1 ex</description><edition>7</edition><language>eng ; rus</language><subject>CHEMISTRY ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20011210&amp;DB=EPODOC&amp;CC=RU&amp;NR=2176672C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20011210&amp;DB=EPODOC&amp;CC=RU&amp;NR=2176672C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>VALLNER FELIKS</creatorcontrib><creatorcontrib>GENNARI UDO</creatorcontrib><creatorcontrib>KEPPLINGER LEOPOL'D VERNER</creatorcontrib><title>METHOD OF MANUFACTURING SPONGE IRON</title><description>metallurgy. SUBSTANCE: method includes direct reduction of ground material containing iron oxide with reducing gas formed in melting and falsifying zone from carbon carriers and oxygen-containing gas. Reducing gas contains from 20 to 100 g/Ncu.m of dust at carbon content ranging from 30 to 70 mas.% of material containing iron oxide is subjected to action of reducing gas during period of time which exceeds period required for complete reduction, thus making it possible to obtain sponge iron at increased content of carbon. EFFECT: enhanced efficiency. 6 cl, 3 dwg, 5 tbl, 1 ex</description><subject>CHEMISTRY</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD2dQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1cIDvD3c3dV8Azy9-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFBoUaG5mZm5kbORsZEKAEAHg4iiA</recordid><startdate>20011210</startdate><enddate>20011210</enddate><creator>VALLNER FELIKS</creator><creator>GENNARI UDO</creator><creator>KEPPLINGER LEOPOL'D VERNER</creator><scope>EVB</scope></search><sort><creationdate>20011210</creationdate><title>METHOD OF MANUFACTURING SPONGE IRON</title><author>VALLNER FELIKS ; GENNARI UDO ; KEPPLINGER LEOPOL'D VERNER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RU2176672C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rus</language><creationdate>2001</creationdate><topic>CHEMISTRY</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><toplevel>online_resources</toplevel><creatorcontrib>VALLNER FELIKS</creatorcontrib><creatorcontrib>GENNARI UDO</creatorcontrib><creatorcontrib>KEPPLINGER LEOPOL'D VERNER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>VALLNER FELIKS</au><au>GENNARI UDO</au><au>KEPPLINGER LEOPOL'D VERNER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MANUFACTURING SPONGE IRON</title><date>2001-12-10</date><risdate>2001</risdate><abstract>metallurgy. SUBSTANCE: method includes direct reduction of ground material containing iron oxide with reducing gas formed in melting and falsifying zone from carbon carriers and oxygen-containing gas. Reducing gas contains from 20 to 100 g/Ncu.m of dust at carbon content ranging from 30 to 70 mas.% of material containing iron oxide is subjected to action of reducing gas during period of time which exceeds period required for complete reduction, thus making it possible to obtain sponge iron at increased content of carbon. EFFECT: enhanced efficiency. 6 cl, 3 dwg, 5 tbl, 1 ex</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rus
recordid cdi_epo_espacenet_RU2176672C2
source esp@cenet
subjects CHEMISTRY
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
title METHOD OF MANUFACTURING SPONGE IRON
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T01%3A50%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=VALLNER%20FELIKS&rft.date=2001-12-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERU2176672C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true