PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE

The process comprises a technique yielding high-purity barium carbonate for production of phosphatic laser glasses. A reactive barium chloride solution in de-mineralised water of 13.5 per cent concentration has added to it, by mixing and heating at 70-80 deg.C 12-15 g of ammonium sulphocyanide per 1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: JIANU VALENTIN, RO
Format: Patent
Sprache:eng ; rum
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JIANU VALENTIN, RO
description The process comprises a technique yielding high-purity barium carbonate for production of phosphatic laser glasses. A reactive barium chloride solution in de-mineralised water of 13.5 per cent concentration has added to it, by mixing and heating at 70-80 deg.C 12-15 g of ammonium sulphocyanide per 100 kg of BaCl2.2H20. The resulting solution then receives at boiling pt. 5ml of pyridine per 100 litres of solution with final cooling and filtration to remove the precipitate.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_RO102430A2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>RO102430A2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_RO102430A23</originalsourceid><addsrcrecordid>eNrjZHALCPJ3dg0OVnDzD1IIcnUJdfb0c1cI8XBVcPb3C3H1C1Hw9FNwDvL39Q_w8A9yVfD09wsGCTk5BnmG-io4e_j4B3m6uPIwsKYl5hSn8kJpbgZ5N9cQZw_d1IL8-NTigsTk1LzUkvggf0MDIxNjA0cjY8IqAPqPK2M</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE</title><source>esp@cenet</source><creator>JIANU VALENTIN, RO</creator><creatorcontrib>JIANU VALENTIN, RO</creatorcontrib><description>The process comprises a technique yielding high-purity barium carbonate for production of phosphatic laser glasses. A reactive barium chloride solution in de-mineralised water of 13.5 per cent concentration has added to it, by mixing and heating at 70-80 deg.C 12-15 g of ammonium sulphocyanide per 100 kg of BaCl2.2H20. The resulting solution then receives at boiling pt. 5ml of pyridine per 100 litres of solution with final cooling and filtration to remove the precipitate.</description><edition>4</edition><language>eng ; rum</language><subject>CHEMISTRY ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>1991</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19911011&amp;DB=EPODOC&amp;CC=RO&amp;NR=102430A2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19911011&amp;DB=EPODOC&amp;CC=RO&amp;NR=102430A2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JIANU VALENTIN, RO</creatorcontrib><title>PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE</title><description>The process comprises a technique yielding high-purity barium carbonate for production of phosphatic laser glasses. A reactive barium chloride solution in de-mineralised water of 13.5 per cent concentration has added to it, by mixing and heating at 70-80 deg.C 12-15 g of ammonium sulphocyanide per 100 kg of BaCl2.2H20. The resulting solution then receives at boiling pt. 5ml of pyridine per 100 litres of solution with final cooling and filtration to remove the precipitate.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1991</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHALCPJ3dg0OVnDzD1IIcnUJdfb0c1cI8XBVcPb3C3H1C1Hw9FNwDvL39Q_w8A9yVfD09wsGCTk5BnmG-io4e_j4B3m6uPIwsKYl5hSn8kJpbgZ5N9cQZw_d1IL8-NTigsTk1LzUkvggf0MDIxNjA0cjY8IqAPqPK2M</recordid><startdate>19911011</startdate><enddate>19911011</enddate><creator>JIANU VALENTIN, RO</creator><scope>EVB</scope></search><sort><creationdate>19911011</creationdate><title>PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE</title><author>JIANU VALENTIN, RO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_RO102430A23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rum</language><creationdate>1991</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>JIANU VALENTIN, RO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JIANU VALENTIN, RO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE</title><date>1991-10-11</date><risdate>1991</risdate><abstract>The process comprises a technique yielding high-purity barium carbonate for production of phosphatic laser glasses. A reactive barium chloride solution in de-mineralised water of 13.5 per cent concentration has added to it, by mixing and heating at 70-80 deg.C 12-15 g of ammonium sulphocyanide per 100 kg of BaCl2.2H20. The resulting solution then receives at boiling pt. 5ml of pyridine per 100 litres of solution with final cooling and filtration to remove the precipitate.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rum
recordid cdi_epo_espacenet_RO102430A2
source esp@cenet
subjects CHEMISTRY
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
METALLURGY
title PROCESS FOR REDUCING THE CONTENT IN CROMOPHORE IONS IN BARIUM CHLORIDE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-16T05%3A30%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JIANU%20VALENTIN,%20RO&rft.date=1991-10-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ERO102430A2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true