PROCESS OF PREPARATION OF THE GREEN COSMETICS PIGMENT ON CHROMIC OXIDE BASIS
The process comprises calcining of a homogenised mixture of minimum 99% purity CrO3=H3BO3=S (1:4=0.25) at 900-1050 deg.C over 30-60 minutes. The product is heated at 80-100 deg.C in magnesium or zinc stearate suspension. Washing with successive settling, in water at 50-60 deg.C, filtration, and dryi...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rum |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The process comprises calcining of a homogenised mixture of minimum 99% purity CrO3=H3BO3=S (1:4=0.25) at 900-1050 deg.C over 30-60 minutes. The product is heated at 80-100 deg.C in magnesium or zinc stearate suspension. Washing with successive settling, in water at 50-60 deg.C, filtration, and drying at 120 deg.C, is followed by grinding. |
---|