PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH

A phosphorous pentoxide producing method includes forming pre-feed agglomerates containing phosphate ore particles, carbonaceous material particles, and silica particles and heating the pre-feed agglomerates in a reducing or inert atmosphere to an induration temperature from above 900 C to less than...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PACHPOR, SOURABH A, HANDMAN, LAWRENCE M, FOWLER, THEODORE P, TRAINHAM, JAMES A, BLAKE, DAVID B, VIGNOVIC, MARK
Format: Patent
Sprache:eng ; pol
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PACHPOR, SOURABH A
HANDMAN, LAWRENCE M
FOWLER, THEODORE P
TRAINHAM, JAMES A
BLAKE, DAVID B
VIGNOVIC, MARK
description A phosphorous pentoxide producing method includes forming pre-feed agglomerates containing phosphate ore particles, carbonaceous material particles, and silica particles and heating the pre-feed agglomerates in a reducing or inert atmosphere to an induration temperature from above 900 C to less than 1180 C and maintaining the induration temperature for 15 minutes or more. The method includes forming feed agglomerates and increasing a compression strength of the feed agglomerates to above 25 lbf using the heating, the feed agglomerates exhibiting a calcium-to-silica mole ratio less than 1 and a silica-to-(calcium+magnesium) mole ratio greater than 2. A reducing kiln bed is formed using the feed agglomerates, kiln off-gas is generated, and phosphorous pentoxide is collected from the kiln off gas.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_PL3197828TT3</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>PL3197828TT3</sourcerecordid><originalsourceid>FETCH-epo_espacenet_PL3197828TT33</originalsourceid><addsrcrecordid>eNqNyrEKwjAQgOEuDqK-w_kADtrBOobkTAJNLuSuqFMpJU6ihfr-6OADOPx8y7-sxuSIv2XqGBJGoas3CCmT6bSPFgKKI8OgogG-sWBguHhx4KPOqBgNKGtbCpiVIGgKKSOzpwgsGaMVt64W9-Exl83PVbU9o2i3K9OrL_M0jOVZ3n1q6_3p2Bwakbr-5_kAqXE1tw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH</title><source>esp@cenet</source><creator>PACHPOR, SOURABH A ; HANDMAN, LAWRENCE M ; FOWLER, THEODORE P ; TRAINHAM, JAMES A ; BLAKE, DAVID B ; VIGNOVIC, MARK</creator><creatorcontrib>PACHPOR, SOURABH A ; HANDMAN, LAWRENCE M ; FOWLER, THEODORE P ; TRAINHAM, JAMES A ; BLAKE, DAVID B ; VIGNOVIC, MARK</creatorcontrib><description>A phosphorous pentoxide producing method includes forming pre-feed agglomerates containing phosphate ore particles, carbonaceous material particles, and silica particles and heating the pre-feed agglomerates in a reducing or inert atmosphere to an induration temperature from above 900 C to less than 1180 C and maintaining the induration temperature for 15 minutes or more. The method includes forming feed agglomerates and increasing a compression strength of the feed agglomerates to above 25 lbf using the heating, the feed agglomerates exhibiting a calcium-to-silica mole ratio less than 1 and a silica-to-(calcium+magnesium) mole ratio greater than 2. A reducing kiln bed is formed using the feed agglomerates, kiln off-gas is generated, and phosphorous pentoxide is collected from the kiln off gas.</description><language>eng ; pol</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200629&amp;DB=EPODOC&amp;CC=PL&amp;NR=3197828T3$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200629&amp;DB=EPODOC&amp;CC=PL&amp;NR=3197828T3$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PACHPOR, SOURABH A</creatorcontrib><creatorcontrib>HANDMAN, LAWRENCE M</creatorcontrib><creatorcontrib>FOWLER, THEODORE P</creatorcontrib><creatorcontrib>TRAINHAM, JAMES A</creatorcontrib><creatorcontrib>BLAKE, DAVID B</creatorcontrib><creatorcontrib>VIGNOVIC, MARK</creatorcontrib><title>PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH</title><description>A phosphorous pentoxide producing method includes forming pre-feed agglomerates containing phosphate ore particles, carbonaceous material particles, and silica particles and heating the pre-feed agglomerates in a reducing or inert atmosphere to an induration temperature from above 900 C to less than 1180 C and maintaining the induration temperature for 15 minutes or more. The method includes forming feed agglomerates and increasing a compression strength of the feed agglomerates to above 25 lbf using the heating, the feed agglomerates exhibiting a calcium-to-silica mole ratio less than 1 and a silica-to-(calcium+magnesium) mole ratio greater than 2. A reducing kiln bed is formed using the feed agglomerates, kiln off-gas is generated, and phosphorous pentoxide is collected from the kiln off gas.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQgOEuDqK-w_kADtrBOobkTAJNLuSuqFMpJU6ihfr-6OADOPx8y7-sxuSIv2XqGBJGoas3CCmT6bSPFgKKI8OgogG-sWBguHhx4KPOqBgNKGtbCpiVIGgKKSOzpwgsGaMVt64W9-Exl83PVbU9o2i3K9OrL_M0jOVZ3n1q6_3p2Bwakbr-5_kAqXE1tw</recordid><startdate>20200629</startdate><enddate>20200629</enddate><creator>PACHPOR, SOURABH A</creator><creator>HANDMAN, LAWRENCE M</creator><creator>FOWLER, THEODORE P</creator><creator>TRAINHAM, JAMES A</creator><creator>BLAKE, DAVID B</creator><creator>VIGNOVIC, MARK</creator><scope>EVB</scope></search><sort><creationdate>20200629</creationdate><title>PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH</title><author>PACHPOR, SOURABH A ; HANDMAN, LAWRENCE M ; FOWLER, THEODORE P ; TRAINHAM, JAMES A ; BLAKE, DAVID B ; VIGNOVIC, MARK</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_PL3197828TT33</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; pol</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>PACHPOR, SOURABH A</creatorcontrib><creatorcontrib>HANDMAN, LAWRENCE M</creatorcontrib><creatorcontrib>FOWLER, THEODORE P</creatorcontrib><creatorcontrib>TRAINHAM, JAMES A</creatorcontrib><creatorcontrib>BLAKE, DAVID B</creatorcontrib><creatorcontrib>VIGNOVIC, MARK</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PACHPOR, SOURABH A</au><au>HANDMAN, LAWRENCE M</au><au>FOWLER, THEODORE P</au><au>TRAINHAM, JAMES A</au><au>BLAKE, DAVID B</au><au>VIGNOVIC, MARK</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH</title><date>2020-06-29</date><risdate>2020</risdate><abstract>A phosphorous pentoxide producing method includes forming pre-feed agglomerates containing phosphate ore particles, carbonaceous material particles, and silica particles and heating the pre-feed agglomerates in a reducing or inert atmosphere to an induration temperature from above 900 C to less than 1180 C and maintaining the induration temperature for 15 minutes or more. The method includes forming feed agglomerates and increasing a compression strength of the feed agglomerates to above 25 lbf using the heating, the feed agglomerates exhibiting a calcium-to-silica mole ratio less than 1 and a silica-to-(calcium+magnesium) mole ratio greater than 2. A reducing kiln bed is formed using the feed agglomerates, kiln off-gas is generated, and phosphorous pentoxide is collected from the kiln off gas.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; pol
recordid cdi_epo_espacenet_PL3197828TT3
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title PHOSPHOROUS PENTOXIDE PRODUCING METHODS AND SYSTEMS WITH INCREASED AGGLOMERATE COMPRESSION STRENGTH
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-21T09%3A18%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PACHPOR,%20SOURABH%20A&rft.date=2020-06-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EPL3197828TT3%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true