METHOD OF OBTAINING SPONGE OR PIG IRON

PCT No. PCT/AU92/00489 Sec. 371 Date Apr. 19, 1994 Sec. 102(e) Date Apr. 19, 1992 PCT Filed Sep. 17, 1992 PCT Pub. No. WO93/06251 PCT Pub. Date Apr. 1, 1993.A process for smelting iron-containing source material in a reactor containing a slag bath, includes generating heating and reducing conditions...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FLOYD JOHN M, CHARD IAN L, BALDOCK BRIAN R
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FLOYD JOHN M
CHARD IAN L
BALDOCK BRIAN R
description PCT No. PCT/AU92/00489 Sec. 371 Date Apr. 19, 1994 Sec. 102(e) Date Apr. 19, 1992 PCT Filed Sep. 17, 1992 PCT Pub. No. WO93/06251 PCT Pub. Date Apr. 1, 1993.A process for smelting iron-containing source material in a reactor containing a slag bath, includes generating heating and reducing conditions in at least one reducing region of the bath by injection of fuel/reductant and oxygen-containing gas by at least one top submerged lance. The source material is fed to the reactor together with additional reductant and with flux at or adjacent the at least one reducing region so as to be subjected to smelting reduction, using coal as the additional reductant. The rates of injection of oxygen and fuel/reductant are controlled to achieve required and sufficient reducing conditions by providing the injected gas with an oxygen content from about 40% to about 100% sufficient for a degree of combustion of the fuel/reductant of from about 40% to about 50%. The CO and H2 generated by the smelting operation, as well as carbon dust carried out of the bath by combustion gases, are subjected to post-combustion in the reactor, enabling efficient heating of the bath while preventing re-oxidization of the bath contents.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_PL170853BB1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>PL170853BB1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_PL170853BB13</originalsourceid><addsrcrecordid>eNrjZFDzdQ3x8HdR8HdT8HcKcfT08_RzVwgO8Pdzd1XwD1II8HRX8Azy9-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfEBPobmBhamxk5OhsZEKAEAZ2AjDw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF OBTAINING SPONGE OR PIG IRON</title><source>esp@cenet</source><creator>FLOYD JOHN M ; CHARD IAN L ; BALDOCK BRIAN R</creator><creatorcontrib>FLOYD JOHN M ; CHARD IAN L ; BALDOCK BRIAN R</creatorcontrib><description>PCT No. PCT/AU92/00489 Sec. 371 Date Apr. 19, 1994 Sec. 102(e) Date Apr. 19, 1992 PCT Filed Sep. 17, 1992 PCT Pub. No. WO93/06251 PCT Pub. Date Apr. 1, 1993.A process for smelting iron-containing source material in a reactor containing a slag bath, includes generating heating and reducing conditions in at least one reducing region of the bath by injection of fuel/reductant and oxygen-containing gas by at least one top submerged lance. The source material is fed to the reactor together with additional reductant and with flux at or adjacent the at least one reducing region so as to be subjected to smelting reduction, using coal as the additional reductant. The rates of injection of oxygen and fuel/reductant are controlled to achieve required and sufficient reducing conditions by providing the injected gas with an oxygen content from about 40% to about 100% sufficient for a degree of combustion of the fuel/reductant of from about 40% to about 50%. The CO and H2 generated by the smelting operation, as well as carbon dust carried out of the bath by combustion gases, are subjected to post-combustion in the reactor, enabling efficient heating of the bath while preventing re-oxidization of the bath contents.</description><edition>6</edition><language>eng</language><subject>CHEMISTRY ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON</subject><creationdate>1997</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970131&amp;DB=EPODOC&amp;CC=PL&amp;NR=170853B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970131&amp;DB=EPODOC&amp;CC=PL&amp;NR=170853B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FLOYD JOHN M</creatorcontrib><creatorcontrib>CHARD IAN L</creatorcontrib><creatorcontrib>BALDOCK BRIAN R</creatorcontrib><title>METHOD OF OBTAINING SPONGE OR PIG IRON</title><description>PCT No. PCT/AU92/00489 Sec. 371 Date Apr. 19, 1994 Sec. 102(e) Date Apr. 19, 1992 PCT Filed Sep. 17, 1992 PCT Pub. No. WO93/06251 PCT Pub. Date Apr. 1, 1993.A process for smelting iron-containing source material in a reactor containing a slag bath, includes generating heating and reducing conditions in at least one reducing region of the bath by injection of fuel/reductant and oxygen-containing gas by at least one top submerged lance. The source material is fed to the reactor together with additional reductant and with flux at or adjacent the at least one reducing region so as to be subjected to smelting reduction, using coal as the additional reductant. The rates of injection of oxygen and fuel/reductant are controlled to achieve required and sufficient reducing conditions by providing the injected gas with an oxygen content from about 40% to about 100% sufficient for a degree of combustion of the fuel/reductant of from about 40% to about 50%. The CO and H2 generated by the smelting operation, as well as carbon dust carried out of the bath by combustion gases, are subjected to post-combustion in the reactor, enabling efficient heating of the bath while preventing re-oxidization of the bath contents.</description><subject>CHEMISTRY</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1997</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDzdQ3x8HdR8HdT8HcKcfT08_RzVwgO8Pdzd1XwD1II8HRX8Azy9-NhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfEBPobmBhamxk5OhsZEKAEAZ2AjDw</recordid><startdate>19970131</startdate><enddate>19970131</enddate><creator>FLOYD JOHN M</creator><creator>CHARD IAN L</creator><creator>BALDOCK BRIAN R</creator><scope>EVB</scope></search><sort><creationdate>19970131</creationdate><title>METHOD OF OBTAINING SPONGE OR PIG IRON</title><author>FLOYD JOHN M ; CHARD IAN L ; BALDOCK BRIAN R</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_PL170853BB13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1997</creationdate><topic>CHEMISTRY</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><toplevel>online_resources</toplevel><creatorcontrib>FLOYD JOHN M</creatorcontrib><creatorcontrib>CHARD IAN L</creatorcontrib><creatorcontrib>BALDOCK BRIAN R</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FLOYD JOHN M</au><au>CHARD IAN L</au><au>BALDOCK BRIAN R</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF OBTAINING SPONGE OR PIG IRON</title><date>1997-01-31</date><risdate>1997</risdate><abstract>PCT No. PCT/AU92/00489 Sec. 371 Date Apr. 19, 1994 Sec. 102(e) Date Apr. 19, 1992 PCT Filed Sep. 17, 1992 PCT Pub. No. WO93/06251 PCT Pub. Date Apr. 1, 1993.A process for smelting iron-containing source material in a reactor containing a slag bath, includes generating heating and reducing conditions in at least one reducing region of the bath by injection of fuel/reductant and oxygen-containing gas by at least one top submerged lance. The source material is fed to the reactor together with additional reductant and with flux at or adjacent the at least one reducing region so as to be subjected to smelting reduction, using coal as the additional reductant. The rates of injection of oxygen and fuel/reductant are controlled to achieve required and sufficient reducing conditions by providing the injected gas with an oxygen content from about 40% to about 100% sufficient for a degree of combustion of the fuel/reductant of from about 40% to about 50%. The CO and H2 generated by the smelting operation, as well as carbon dust carried out of the bath by combustion gases, are subjected to post-combustion in the reactor, enabling efficient heating of the bath while preventing re-oxidization of the bath contents.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_PL170853BB1
source esp@cenet
subjects CHEMISTRY
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
title METHOD OF OBTAINING SPONGE OR PIG IRON
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T17%3A46%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FLOYD%20JOHN%20M&rft.date=1997-01-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EPL170853BB1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true