REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF

product containing a small amount of free silicon and a preparation method thereof. The reaction- bonded. SiC jproduct includes the following' components in parts by weight: 20-30 parts of purified water, 25-35 parts of Sic micropowder, 40-65 parts of SiC coarse particles, 6- 10 parts of carbon...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SIYU SONG, XIA REN, YONGLIAN QI, YANZHE LIU, YUN REN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SIYU SONG
XIA REN
YONGLIAN QI
YANZHE LIU
YUN REN
description product containing a small amount of free silicon and a preparation method thereof. The reaction- bonded. SiC jproduct includes the following' components in parts by weight: 20-30 parts of purified water, 25-35 parts of Sic micropowder, 40-65 parts of SiC coarse particles, 6- 10 parts of carbon black, and 1.1-2.3 parts of binding agent. The content of free silicon in the reaction-bonded SiC product obtained by the present invention is less than or equal to 4%. Upon testing, the bulk density of a green body is 2.38-2.48 g/cm3, the bulk density of a finished product is 3.07-3.12 g/cm3, the bending strength at 20 degrees Celsius is about 270-300 MPa, and the bending strength at 1,200 degrees Celsius is about 290-330 MPa. The preparation strength, bulk density and bending strength at different temperatures of the green body are greatly improved.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_NL2036773A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>NL2036773A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_NL2036773A3</originalsourceid><addsrcrecordid>eNqFzLEKwjAQxvEuDqI-g_cCBbFg5zO52EB6V9LrXKrESbRQ3x8juDt9y-_7r4trJDTqhcuzsCULvTfQRbGDUTDCip49X6BvMQTAVgZWEAcuEmUbfDaAbPOHOoz4TUFL2ogFbSiSuG2xuk-PJe1-uyn2jtQ0ZZpfY1rm6Zae6T1yOB6qU11XWP0XHxIWMyI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF</title><source>esp@cenet</source><creator>SIYU SONG ; XIA REN ; YONGLIAN QI ; YANZHE LIU ; YUN REN</creator><creatorcontrib>SIYU SONG ; XIA REN ; YONGLIAN QI ; YANZHE LIU ; YUN REN</creatorcontrib><description>product containing a small amount of free silicon and a preparation method thereof. The reaction- bonded. SiC jproduct includes the following' components in parts by weight: 20-30 parts of purified water, 25-35 parts of Sic micropowder, 40-65 parts of SiC coarse particles, 6- 10 parts of carbon black, and 1.1-2.3 parts of binding agent. The content of free silicon in the reaction-bonded SiC product obtained by the present invention is less than or equal to 4%. Upon testing, the bulk density of a green body is 2.38-2.48 g/cm3, the bulk density of a finished product is 3.07-3.12 g/cm3, the bending strength at 20 degrees Celsius is about 270-300 MPa, and the bending strength at 1,200 degrees Celsius is about 290-330 MPa. The preparation strength, bulk density and bending strength at different temperatures of the green body are greatly improved.</description><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241125&amp;DB=EPODOC&amp;CC=NL&amp;NR=2036773A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241125&amp;DB=EPODOC&amp;CC=NL&amp;NR=2036773A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SIYU SONG</creatorcontrib><creatorcontrib>XIA REN</creatorcontrib><creatorcontrib>YONGLIAN QI</creatorcontrib><creatorcontrib>YANZHE LIU</creatorcontrib><creatorcontrib>YUN REN</creatorcontrib><title>REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF</title><description>product containing a small amount of free silicon and a preparation method thereof. The reaction- bonded. SiC jproduct includes the following' components in parts by weight: 20-30 parts of purified water, 25-35 parts of Sic micropowder, 40-65 parts of SiC coarse particles, 6- 10 parts of carbon black, and 1.1-2.3 parts of binding agent. The content of free silicon in the reaction-bonded SiC product obtained by the present invention is less than or equal to 4%. Upon testing, the bulk density of a green body is 2.38-2.48 g/cm3, the bulk density of a finished product is 3.07-3.12 g/cm3, the bending strength at 20 degrees Celsius is about 270-300 MPa, and the bending strength at 1,200 degrees Celsius is about 290-330 MPa. The preparation strength, bulk density and bending strength at different temperatures of the green body are greatly improved.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFzLEKwjAQxvEuDqI-g_cCBbFg5zO52EB6V9LrXKrESbRQ3x8juDt9y-_7r4trJDTqhcuzsCULvTfQRbGDUTDCip49X6BvMQTAVgZWEAcuEmUbfDaAbPOHOoz4TUFL2ogFbSiSuG2xuk-PJe1-uyn2jtQ0ZZpfY1rm6Zae6T1yOB6qU11XWP0XHxIWMyI</recordid><startdate>20241125</startdate><enddate>20241125</enddate><creator>SIYU SONG</creator><creator>XIA REN</creator><creator>YONGLIAN QI</creator><creator>YANZHE LIU</creator><creator>YUN REN</creator><scope>EVB</scope></search><sort><creationdate>20241125</creationdate><title>REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF</title><author>SIYU SONG ; XIA REN ; YONGLIAN QI ; YANZHE LIU ; YUN REN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_NL2036773A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SIYU SONG</creatorcontrib><creatorcontrib>XIA REN</creatorcontrib><creatorcontrib>YONGLIAN QI</creatorcontrib><creatorcontrib>YANZHE LIU</creatorcontrib><creatorcontrib>YUN REN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SIYU SONG</au><au>XIA REN</au><au>YONGLIAN QI</au><au>YANZHE LIU</au><au>YUN REN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF</title><date>2024-11-25</date><risdate>2024</risdate><abstract>product containing a small amount of free silicon and a preparation method thereof. The reaction- bonded. SiC jproduct includes the following' components in parts by weight: 20-30 parts of purified water, 25-35 parts of Sic micropowder, 40-65 parts of SiC coarse particles, 6- 10 parts of carbon black, and 1.1-2.3 parts of binding agent. The content of free silicon in the reaction-bonded SiC product obtained by the present invention is less than or equal to 4%. Upon testing, the bulk density of a green body is 2.38-2.48 g/cm3, the bulk density of a finished product is 3.07-3.12 g/cm3, the bending strength at 20 degrees Celsius is about 270-300 MPa, and the bending strength at 1,200 degrees Celsius is about 290-330 MPa. The preparation strength, bulk density and bending strength at different temperatures of the green body are greatly improved.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_NL2036773A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title REACTION-BONDED SIC PRODUCT CONTAINING SMALL AMOUNT OF FREE SILICON AND PREPARATION METHOD THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T03%3A46%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SIYU%20SONG&rft.date=2024-11-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ENL2036773A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true