PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM

Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NATAL Manuel A. W, HOSSIENY Nemat
Format: Patent
Sprache:eng ; spa
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NATAL Manuel A. W
HOSSIENY Nemat
description Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam. Las microesferas de poli(láctida) expandidas (PLA) se elaboran presurizando microesferas de PLA con dióxido de carbono a aproximadamente temperatura ambiente, calentando las microesferas a presión a 90 °C a 160 °C para saturar y cristalizar parcialmente las microesferas, y luego despresurizando y enfriando las microesferas. Las microesferas de PLA contienen una mezcla de PLLA y PDLA en ciertas proporciones. Las microesferas son útiles para elaborar espuma expandida de microesferas.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_MX2021002313A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MX2021002313A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_MX2021002313A3</originalsourceid><addsrcrecordid>eNrjZDAKCPJ3dg0OVnDzDwJhX08_d4UAf59IH0fnEE8XVwXXiABHPxdXFwUnV0cXoApHXx4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8bYWRgZGhgYGRsaOxoTJQiALgDJwk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM</title><source>esp@cenet</source><creator>NATAL Manuel A. W ; HOSSIENY Nemat</creator><creatorcontrib>NATAL Manuel A. W ; HOSSIENY Nemat</creatorcontrib><description>Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam. Las microesferas de poli(láctida) expandidas (PLA) se elaboran presurizando microesferas de PLA con dióxido de carbono a aproximadamente temperatura ambiente, calentando las microesferas a presión a 90 °C a 160 °C para saturar y cristalizar parcialmente las microesferas, y luego despresurizando y enfriando las microesferas. Las microesferas de PLA contienen una mezcla de PLLA y PDLA en ciertas proporciones. Las microesferas son útiles para elaborar espuma expandida de microesferas.</description><language>eng ; spa</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210428&amp;DB=EPODOC&amp;CC=MX&amp;NR=2021002313A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210428&amp;DB=EPODOC&amp;CC=MX&amp;NR=2021002313A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NATAL Manuel A. W</creatorcontrib><creatorcontrib>HOSSIENY Nemat</creatorcontrib><title>PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM</title><description>Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam. Las microesferas de poli(láctida) expandidas (PLA) se elaboran presurizando microesferas de PLA con dióxido de carbono a aproximadamente temperatura ambiente, calentando las microesferas a presión a 90 °C a 160 °C para saturar y cristalizar parcialmente las microesferas, y luego despresurizando y enfriando las microesferas. Las microesferas de PLA contienen una mezcla de PLLA y PDLA en ciertas proporciones. Las microesferas son útiles para elaborar espuma expandida de microesferas.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAKCPJ3dg0OVnDzDwJhX08_d4UAf59IH0fnEE8XVwXXiABHPxdXFwUnV0cXoApHXx4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8bYWRgZGhgYGRsaOxoTJQiALgDJwk</recordid><startdate>20210428</startdate><enddate>20210428</enddate><creator>NATAL Manuel A. W</creator><creator>HOSSIENY Nemat</creator><scope>EVB</scope></search><sort><creationdate>20210428</creationdate><title>PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM</title><author>NATAL Manuel A. W ; HOSSIENY Nemat</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_MX2021002313A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; spa</language><creationdate>2021</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>NATAL Manuel A. W</creatorcontrib><creatorcontrib>HOSSIENY Nemat</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NATAL Manuel A. W</au><au>HOSSIENY Nemat</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM</title><date>2021-04-28</date><risdate>2021</risdate><abstract>Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam. Las microesferas de poli(láctida) expandidas (PLA) se elaboran presurizando microesferas de PLA con dióxido de carbono a aproximadamente temperatura ambiente, calentando las microesferas a presión a 90 °C a 160 °C para saturar y cristalizar parcialmente las microesferas, y luego despresurizando y enfriando las microesferas. Las microesferas de PLA contienen una mezcla de PLLA y PDLA en ciertas proporciones. Las microesferas son útiles para elaborar espuma expandida de microesferas.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; spa
recordid cdi_epo_espacenet_MX2021002313A
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
GENERAL PROCESSES OF COMPOUNDING
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title PROCESS FOR FORMING POLYLACTIDE EXPANDED BEAD FOAM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T11%3A32%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NATAL%20Manuel%20A.%20W&rft.date=2021-04-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EMX2021002313A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true