SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME

Provided is a seamless steel pipe which has excellent SSC resistance, while being suppressed in strength variation in the circumferential direction and in the axial direction. A seamless steel pipe according to one embodiment of the present invention contains, in mass%, 0.21-0.35% of C, 0.10-0.50% o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Yuji ARAI, Keisuke FURO, Atsushi SOMA, Kouji YAMANE, Kamitani HIROKI, Takenori KURAMOTO, Yosuke TATEBAYASHI
Format: Patent
Sprache:eng ; spa
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Yuji ARAI
Keisuke FURO
Atsushi SOMA
Kouji YAMANE
Kamitani HIROKI
Takenori KURAMOTO
Yosuke TATEBAYASHI
description Provided is a seamless steel pipe which has excellent SSC resistance, while being suppressed in strength variation in the circumferential direction and in the axial direction. A seamless steel pipe according to one embodiment of the present invention contains, in mass%, 0.21-0.35% of C, 0.10-0.50% of Si, 0.05-1.00% of Mn, 0.025% or less of P, 0.010% or less of S, 0.005-0.100% of Al, 0.010% or less of N, 0.05-1.50% of Cr, 0.10-1.50% of Mo, 0.010-0.050% of Nb, 0.0003-0.0050% of B and 0.002-0.050% of Ti, with the balance made up of Fe and impurities. With respect to the main body region of this seamless steel pipe, the crystal grain size number of prior austenite crystal grains in accordance with ASTM E112 is 7.0 or more; the difference between the maximum value and the minimum value of the crystal grain size number is 1.0 or less; the yield strength is 655 MPa or more but less than 862 MPa; and the difference between the maximum value and the minimum value of the tensile strength is 27.6 MPa or less. Se proporciona un tubo de acero sin costura que tiene una excelente resistencia a SSC con variación de resistencia en una dirección circunferencial y una dirección axial suprimida. El tubo de acero sin costura de la presente modalidad consiste de, en % en masa, C: 0.21 a 0.35%, Si: 0.10 a 0.50%, Mn: 0.05 a 1.00%, P: 0.025% o menos, S: 0.010% o menos, Al: 0.005 a 0.100%, N: 0.010% o menos, Cr: 0.05 a 1.50%, Mo: 0.10 a 1.50%, Nb: 0.010 a 0.050%, B: 0.0003 a 0.0050%, y Ti: 0.002 a 0.050%, el resto siendo Fe e impurezas. En una región del cuerpo principal del tubo de acero sin costura, un número de tamaño de grano de austenita previo conforme a ASTM E112 es de 7.0 o más, una diferencia entre un valor máximo y un valor mínimo del número de tamaño de grano es de 1.0 o menos, el límite elástico es de 655 a menos de 862 MPa, y una diferencia entre un valor máximo y un valor mínimo de resistencia a la tracción es de 27.6 MPa o menos.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_MX2018014000A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MX2018014000A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_MX2018014000A3</originalsourceid><addsrcrecordid>eNrjZDAMdnX09XENDlYIDnF19VEI8AxwVXD0c1HwdQ3x8HdRcPMPUggI8ncJdfb0c1cIdvR15WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8b4RRgaGFgaGJgYGBo7GRCkCAIRwJrY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME</title><source>esp@cenet</source><creator>Yuji ARAI ; Keisuke FURO ; Atsushi SOMA ; Kouji YAMANE ; Kamitani HIROKI ; Takenori KURAMOTO ; Yosuke TATEBAYASHI</creator><creatorcontrib>Yuji ARAI ; Keisuke FURO ; Atsushi SOMA ; Kouji YAMANE ; Kamitani HIROKI ; Takenori KURAMOTO ; Yosuke TATEBAYASHI</creatorcontrib><description>Provided is a seamless steel pipe which has excellent SSC resistance, while being suppressed in strength variation in the circumferential direction and in the axial direction. A seamless steel pipe according to one embodiment of the present invention contains, in mass%, 0.21-0.35% of C, 0.10-0.50% of Si, 0.05-1.00% of Mn, 0.025% or less of P, 0.010% or less of S, 0.005-0.100% of Al, 0.010% or less of N, 0.05-1.50% of Cr, 0.10-1.50% of Mo, 0.010-0.050% of Nb, 0.0003-0.0050% of B and 0.002-0.050% of Ti, with the balance made up of Fe and impurities. With respect to the main body region of this seamless steel pipe, the crystal grain size number of prior austenite crystal grains in accordance with ASTM E112 is 7.0 or more; the difference between the maximum value and the minimum value of the crystal grain size number is 1.0 or less; the yield strength is 655 MPa or more but less than 862 MPa; and the difference between the maximum value and the minimum value of the tensile strength is 27.6 MPa or less. Se proporciona un tubo de acero sin costura que tiene una excelente resistencia a SSC con variación de resistencia en una dirección circunferencial y una dirección axial suprimida. El tubo de acero sin costura de la presente modalidad consiste de, en % en masa, C: 0.21 a 0.35%, Si: 0.10 a 0.50%, Mn: 0.05 a 1.00%, P: 0.025% o menos, S: 0.010% o menos, Al: 0.005 a 0.100%, N: 0.010% o menos, Cr: 0.05 a 1.50%, Mo: 0.10 a 1.50%, Nb: 0.010 a 0.050%, B: 0.0003 a 0.0050%, y Ti: 0.002 a 0.050%, el resto siendo Fe e impurezas. En una región del cuerpo principal del tubo de acero sin costura, un número de tamaño de grano de austenita previo conforme a ASTM E112 es de 7.0 o más, una diferencia entre un valor máximo y un valor mínimo del número de tamaño de grano es de 1.0 o menos, el límite elástico es de 655 a menos de 862 MPa, y una diferencia entre un valor máximo y un valor mínimo de resistencia a la tracción es de 27.6 MPa o menos.</description><language>eng ; spa</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190401&amp;DB=EPODOC&amp;CC=MX&amp;NR=2018014000A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190401&amp;DB=EPODOC&amp;CC=MX&amp;NR=2018014000A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Yuji ARAI</creatorcontrib><creatorcontrib>Keisuke FURO</creatorcontrib><creatorcontrib>Atsushi SOMA</creatorcontrib><creatorcontrib>Kouji YAMANE</creatorcontrib><creatorcontrib>Kamitani HIROKI</creatorcontrib><creatorcontrib>Takenori KURAMOTO</creatorcontrib><creatorcontrib>Yosuke TATEBAYASHI</creatorcontrib><title>SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME</title><description>Provided is a seamless steel pipe which has excellent SSC resistance, while being suppressed in strength variation in the circumferential direction and in the axial direction. A seamless steel pipe according to one embodiment of the present invention contains, in mass%, 0.21-0.35% of C, 0.10-0.50% of Si, 0.05-1.00% of Mn, 0.025% or less of P, 0.010% or less of S, 0.005-0.100% of Al, 0.010% or less of N, 0.05-1.50% of Cr, 0.10-1.50% of Mo, 0.010-0.050% of Nb, 0.0003-0.0050% of B and 0.002-0.050% of Ti, with the balance made up of Fe and impurities. With respect to the main body region of this seamless steel pipe, the crystal grain size number of prior austenite crystal grains in accordance with ASTM E112 is 7.0 or more; the difference between the maximum value and the minimum value of the crystal grain size number is 1.0 or less; the yield strength is 655 MPa or more but less than 862 MPa; and the difference between the maximum value and the minimum value of the tensile strength is 27.6 MPa or less. Se proporciona un tubo de acero sin costura que tiene una excelente resistencia a SSC con variación de resistencia en una dirección circunferencial y una dirección axial suprimida. El tubo de acero sin costura de la presente modalidad consiste de, en % en masa, C: 0.21 a 0.35%, Si: 0.10 a 0.50%, Mn: 0.05 a 1.00%, P: 0.025% o menos, S: 0.010% o menos, Al: 0.005 a 0.100%, N: 0.010% o menos, Cr: 0.05 a 1.50%, Mo: 0.10 a 1.50%, Nb: 0.010 a 0.050%, B: 0.0003 a 0.0050%, y Ti: 0.002 a 0.050%, el resto siendo Fe e impurezas. En una región del cuerpo principal del tubo de acero sin costura, un número de tamaño de grano de austenita previo conforme a ASTM E112 es de 7.0 o más, una diferencia entre un valor máximo y un valor mínimo del número de tamaño de grano es de 1.0 o menos, el límite elástico es de 655 a menos de 862 MPa, y una diferencia entre un valor máximo y un valor mínimo de resistencia a la tracción es de 27.6 MPa o menos.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAMdnX09XENDlYIDnF19VEI8AxwVXD0c1HwdQ3x8HdRcPMPUggI8ncJdfb0c1cIdvR15WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8b4RRgaGFgaGJgYGBo7GRCkCAIRwJrY</recordid><startdate>20190401</startdate><enddate>20190401</enddate><creator>Yuji ARAI</creator><creator>Keisuke FURO</creator><creator>Atsushi SOMA</creator><creator>Kouji YAMANE</creator><creator>Kamitani HIROKI</creator><creator>Takenori KURAMOTO</creator><creator>Yosuke TATEBAYASHI</creator><scope>EVB</scope></search><sort><creationdate>20190401</creationdate><title>SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME</title><author>Yuji ARAI ; Keisuke FURO ; Atsushi SOMA ; Kouji YAMANE ; Kamitani HIROKI ; Takenori KURAMOTO ; Yosuke TATEBAYASHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_MX2018014000A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; spa</language><creationdate>2019</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Yuji ARAI</creatorcontrib><creatorcontrib>Keisuke FURO</creatorcontrib><creatorcontrib>Atsushi SOMA</creatorcontrib><creatorcontrib>Kouji YAMANE</creatorcontrib><creatorcontrib>Kamitani HIROKI</creatorcontrib><creatorcontrib>Takenori KURAMOTO</creatorcontrib><creatorcontrib>Yosuke TATEBAYASHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Yuji ARAI</au><au>Keisuke FURO</au><au>Atsushi SOMA</au><au>Kouji YAMANE</au><au>Kamitani HIROKI</au><au>Takenori KURAMOTO</au><au>Yosuke TATEBAYASHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME</title><date>2019-04-01</date><risdate>2019</risdate><abstract>Provided is a seamless steel pipe which has excellent SSC resistance, while being suppressed in strength variation in the circumferential direction and in the axial direction. A seamless steel pipe according to one embodiment of the present invention contains, in mass%, 0.21-0.35% of C, 0.10-0.50% of Si, 0.05-1.00% of Mn, 0.025% or less of P, 0.010% or less of S, 0.005-0.100% of Al, 0.010% or less of N, 0.05-1.50% of Cr, 0.10-1.50% of Mo, 0.010-0.050% of Nb, 0.0003-0.0050% of B and 0.002-0.050% of Ti, with the balance made up of Fe and impurities. With respect to the main body region of this seamless steel pipe, the crystal grain size number of prior austenite crystal grains in accordance with ASTM E112 is 7.0 or more; the difference between the maximum value and the minimum value of the crystal grain size number is 1.0 or less; the yield strength is 655 MPa or more but less than 862 MPa; and the difference between the maximum value and the minimum value of the tensile strength is 27.6 MPa or less. Se proporciona un tubo de acero sin costura que tiene una excelente resistencia a SSC con variación de resistencia en una dirección circunferencial y una dirección axial suprimida. El tubo de acero sin costura de la presente modalidad consiste de, en % en masa, C: 0.21 a 0.35%, Si: 0.10 a 0.50%, Mn: 0.05 a 1.00%, P: 0.025% o menos, S: 0.010% o menos, Al: 0.005 a 0.100%, N: 0.010% o menos, Cr: 0.05 a 1.50%, Mo: 0.10 a 1.50%, Nb: 0.010 a 0.050%, B: 0.0003 a 0.0050%, y Ti: 0.002 a 0.050%, el resto siendo Fe e impurezas. En una región del cuerpo principal del tubo de acero sin costura, un número de tamaño de grano de austenita previo conforme a ASTM E112 es de 7.0 o más, una diferencia entre un valor máximo y un valor mínimo del número de tamaño de grano es de 1.0 o menos, el límite elástico es de 655 a menos de 862 MPa, y una diferencia entre un valor máximo y un valor mínimo de resistencia a la tracción es de 27.6 MPa o menos.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; spa
recordid cdi_epo_espacenet_MX2018014000A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title SEAMLESS STEEL PIPE AND METHOD FOR PRODUCING SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-29T14%3A19%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Yuji%20ARAI&rft.date=2019-04-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EMX2018014000A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true