GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES

According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Kyle Christopher HOFF, Adam James ELLISON, DEMARTINO, Steven Edward
Format: Patent
Sprache:eng ; spa
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Kyle Christopher HOFF
Adam James ELLISON
DEMARTINO, Steven Edward
description According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article. De acuerdo con una modalidad, un artículo de vidrio puede incluir un cuerpo de vidrio que tiene una primera superficie y una segunda superficie opuesta a la primera superficie; la primera superficie y la segunda superficie tienen cada una un radio de curvatura; la primera superficie del cuerpo de vidrio comprende una población defectuosa que se extiende desde la primera superficie en un espesor del cuerpo de vidrio con una profundidad máxima de la falla inicial Ai; la primera superficie del cuerpo de vidrio puede estar grabada a una profundidad menor que o igual a aproximadamente 25 % de la profundidad máxima de la falla inicial Ai de la población defectuosa presente en la primera superficie; cuando el artículo de vidrío está bajo carga compresiva uniaxial, por lo menos una porción de la primera superficie está en tensión y una resistencia compresiva uniaxial del artículo de vidrio es mayor que o igual a 90 % de una resistencia compresiva uniaxial de un artículo de vidrio sin fallas.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_MX2017002898A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MX2017002898A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_MX2017002898A3</originalsourceid><addsrcrecordid>eNrjZPBy93EMDlZwDArxdPZxBTL8XBR8XUM8_F2CFdz8gxQ8fQOC_MM8_dwVQjxcFYJcfTwdnTx9PEMiFfzdFFD18jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeN8IIwNDcwMDIwtLC0djohQBAK9-LeA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES</title><source>esp@cenet</source><creator>Kyle Christopher HOFF ; Adam James ELLISON ; DEMARTINO, Steven Edward</creator><creatorcontrib>Kyle Christopher HOFF ; Adam James ELLISON ; DEMARTINO, Steven Edward</creatorcontrib><description>According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article. De acuerdo con una modalidad, un artículo de vidrio puede incluir un cuerpo de vidrio que tiene una primera superficie y una segunda superficie opuesta a la primera superficie; la primera superficie y la segunda superficie tienen cada una un radio de curvatura; la primera superficie del cuerpo de vidrio comprende una población defectuosa que se extiende desde la primera superficie en un espesor del cuerpo de vidrio con una profundidad máxima de la falla inicial Ai; la primera superficie del cuerpo de vidrio puede estar grabada a una profundidad menor que o igual a aproximadamente 25 % de la profundidad máxima de la falla inicial Ai de la población defectuosa presente en la primera superficie; cuando el artículo de vidrío está bajo carga compresiva uniaxial, por lo menos una porción de la primera superficie está en tensión y una resistencia compresiva uniaxial del artículo de vidrio es mayor que o igual a 90 % de una resistencia compresiva uniaxial de un artículo de vidrio sin fallas.</description><language>eng ; spa</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171011&amp;DB=EPODOC&amp;CC=MX&amp;NR=2017002898A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25569,76552</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171011&amp;DB=EPODOC&amp;CC=MX&amp;NR=2017002898A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Kyle Christopher HOFF</creatorcontrib><creatorcontrib>Adam James ELLISON</creatorcontrib><creatorcontrib>DEMARTINO, Steven Edward</creatorcontrib><title>GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES</title><description>According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article. De acuerdo con una modalidad, un artículo de vidrio puede incluir un cuerpo de vidrio que tiene una primera superficie y una segunda superficie opuesta a la primera superficie; la primera superficie y la segunda superficie tienen cada una un radio de curvatura; la primera superficie del cuerpo de vidrio comprende una población defectuosa que se extiende desde la primera superficie en un espesor del cuerpo de vidrio con una profundidad máxima de la falla inicial Ai; la primera superficie del cuerpo de vidrio puede estar grabada a una profundidad menor que o igual a aproximadamente 25 % de la profundidad máxima de la falla inicial Ai de la población defectuosa presente en la primera superficie; cuando el artículo de vidrío está bajo carga compresiva uniaxial, por lo menos una porción de la primera superficie está en tensión y una resistencia compresiva uniaxial del artículo de vidrio es mayor que o igual a 90 % de una resistencia compresiva uniaxial de un artículo de vidrio sin fallas.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPBy93EMDlZwDArxdPZxBTL8XBR8XUM8_F2CFdz8gxQ8fQOC_MM8_dwVQjxcFYJcfTwdnTx9PEMiFfzdFFD18jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeN8IIwNDcwMDIwtLC0djohQBAK9-LeA</recordid><startdate>20171011</startdate><enddate>20171011</enddate><creator>Kyle Christopher HOFF</creator><creator>Adam James ELLISON</creator><creator>DEMARTINO, Steven Edward</creator><scope>EVB</scope></search><sort><creationdate>20171011</creationdate><title>GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES</title><author>Kyle Christopher HOFF ; Adam James ELLISON ; DEMARTINO, Steven Edward</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_MX2017002898A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; spa</language><creationdate>2017</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>Kyle Christopher HOFF</creatorcontrib><creatorcontrib>Adam James ELLISON</creatorcontrib><creatorcontrib>DEMARTINO, Steven Edward</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Kyle Christopher HOFF</au><au>Adam James ELLISON</au><au>DEMARTINO, Steven Edward</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES</title><date>2017-10-11</date><risdate>2017</risdate><abstract>According to one embodiment, a glass article may include a glass body having a first surface and a second surface opposite the first surface. The first surface and the second surface each have a radius of curvature. The first surface of the glass body comprises a flaw population extending from the first surface into a thickness of the glass body with a maximum initial flaw depth Ai. The first surface of the glass body may be etched to a depth less than or equal to about 25% of the maximum initial flaw depth Ai of the flaw population present in the first surface. When the glass article is under uniaxial compressive loading, at least a portion of the first surface is in tension and a uniaxial compressive strength of the glass article is greater than or equal to 90% of a uniaxial compressive strength of a flaw-free glass article. De acuerdo con una modalidad, un artículo de vidrio puede incluir un cuerpo de vidrio que tiene una primera superficie y una segunda superficie opuesta a la primera superficie; la primera superficie y la segunda superficie tienen cada una un radio de curvatura; la primera superficie del cuerpo de vidrio comprende una población defectuosa que se extiende desde la primera superficie en un espesor del cuerpo de vidrio con una profundidad máxima de la falla inicial Ai; la primera superficie del cuerpo de vidrio puede estar grabada a una profundidad menor que o igual a aproximadamente 25 % de la profundidad máxima de la falla inicial Ai de la población defectuosa presente en la primera superficie; cuando el artículo de vidrío está bajo carga compresiva uniaxial, por lo menos una porción de la primera superficie está en tensión y una resistencia compresiva uniaxial del artículo de vidrio es mayor que o igual a 90 % de una resistencia compresiva uniaxial de un artículo de vidrio sin fallas.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; spa
recordid cdi_epo_espacenet_MX2017002898A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title GLASS ARTICLES AND METHODS FOR IMPROVING THE RELIABILITY OF GLASS ARTICLES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-15T16%3A54%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Kyle%20Christopher%20HOFF&rft.date=2017-10-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EMX2017002898A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true