BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME

The present invention is directed to a process for prepaϿng a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160°C to 221°C, adding a block copolymer composition to the bitumen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ROBERT Q. KLUTTZ, KEITH E. STEPHENS
Format: Patent
Sprache:eng ; spa
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ROBERT Q. KLUTTZ
KEITH E. STEPHENS
description The present invention is directed to a process for prepaÏ¿ng a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160°C to 221°C, adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition, and continuing to stir the homogeneous mixture while maintaining the temperature from 180°C to 221°C for a total period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition The block copolymer composition utilized in the process compÏ¿ses one or more block copolymers having at least one monovinylaromatic block and at least one polybutadiene block having a vinyl content of less than 15 mol percent and at least one polybutadiene block having a vinyl content of greater than 25 mol percent. La presente invención se refiere a un proceso para preparar una composición aglutinante bituminosa modificada de polímero en la ausencia sustancial de agentes de reticulación calentando un componente de bitumen en un tanque agitado a una temperatura desde 160°C hasta 221°C, agregando una composición de copolímero de bloque al componente de bitúmen, mientras el componente de bitumen está siendo agitado para formar una mezcla homogénea del componente de bitumen y la composición de copolímero de bloque, y continuar agitando la mezcla homogénea mientras se mantiene la temperatura desde 180°C hasta 221°C por un periodo total desde 4 horas hasta 30 horas, con ello formando una composición aglutinante bituminosa modificada de polímero curada. La composición de copolímero de bloque utilizada en el proceso comprende, uno o más copolímeros de bloque que tiene al menos un bloque monovinilaromático y al menos, un bloque de polibutadieno que tiene un contenido de vinilo de menos de 15 por ciento en mol y al menos, un bloque de polibutadieno que tiene un contenido de vinilo mayor de 25 por ciento mol.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_MX2009011561A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MX2009011561A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_MX2009011561A3</originalsourceid><addsrcrecordid>eNrjZHBw8gwJ9fX08w8NVnDy9HNxDVJw9vcN8A_2DPH091Nw9HNRCAjyd3YNDlZw8w8Csl0DHIM8_dwVQjxcFYIdfV15GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8b4SRgYGlgaGhqZmhozFRigAaTStC</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME</title><source>esp@cenet</source><creator>ROBERT Q. KLUTTZ ; KEITH E. STEPHENS</creator><creatorcontrib>ROBERT Q. KLUTTZ ; KEITH E. STEPHENS</creatorcontrib><description>The present invention is directed to a process for prepaÏ¿ng a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160°C to 221°C, adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition, and continuing to stir the homogeneous mixture while maintaining the temperature from 180°C to 221°C for a total period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition The block copolymer composition utilized in the process compÏ¿ses one or more block copolymers having at least one monovinylaromatic block and at least one polybutadiene block having a vinyl content of less than 15 mol percent and at least one polybutadiene block having a vinyl content of greater than 25 mol percent. La presente invención se refiere a un proceso para preparar una composición aglutinante bituminosa modificada de polímero en la ausencia sustancial de agentes de reticulación calentando un componente de bitumen en un tanque agitado a una temperatura desde 160°C hasta 221°C, agregando una composición de copolímero de bloque al componente de bitúmen, mientras el componente de bitumen está siendo agitado para formar una mezcla homogénea del componente de bitumen y la composición de copolímero de bloque, y continuar agitando la mezcla homogénea mientras se mantiene la temperatura desde 180°C hasta 221°C por un periodo total desde 4 horas hasta 30 horas, con ello formando una composición aglutinante bituminosa modificada de polímero curada. La composición de copolímero de bloque utilizada en el proceso comprende, uno o más copolímeros de bloque que tiene al menos un bloque monovinilaromático y al menos, un bloque de polibutadieno que tiene un contenido de vinilo de menos de 15 por ciento en mol y al menos, un bloque de polibutadieno que tiene un contenido de vinilo mayor de 25 por ciento mol.</description><language>eng ; spa</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091110&amp;DB=EPODOC&amp;CC=MX&amp;NR=2009011561A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76302</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091110&amp;DB=EPODOC&amp;CC=MX&amp;NR=2009011561A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ROBERT Q. KLUTTZ</creatorcontrib><creatorcontrib>KEITH E. STEPHENS</creatorcontrib><title>BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME</title><description>The present invention is directed to a process for prepaÏ¿ng a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160°C to 221°C, adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition, and continuing to stir the homogeneous mixture while maintaining the temperature from 180°C to 221°C for a total period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition The block copolymer composition utilized in the process compÏ¿ses one or more block copolymers having at least one monovinylaromatic block and at least one polybutadiene block having a vinyl content of less than 15 mol percent and at least one polybutadiene block having a vinyl content of greater than 25 mol percent. La presente invención se refiere a un proceso para preparar una composición aglutinante bituminosa modificada de polímero en la ausencia sustancial de agentes de reticulación calentando un componente de bitumen en un tanque agitado a una temperatura desde 160°C hasta 221°C, agregando una composición de copolímero de bloque al componente de bitúmen, mientras el componente de bitumen está siendo agitado para formar una mezcla homogénea del componente de bitumen y la composición de copolímero de bloque, y continuar agitando la mezcla homogénea mientras se mantiene la temperatura desde 180°C hasta 221°C por un periodo total desde 4 horas hasta 30 horas, con ello formando una composición aglutinante bituminosa modificada de polímero curada. La composición de copolímero de bloque utilizada en el proceso comprende, uno o más copolímeros de bloque que tiene al menos un bloque monovinilaromático y al menos, un bloque de polibutadieno que tiene un contenido de vinilo de menos de 15 por ciento en mol y al menos, un bloque de polibutadieno que tiene un contenido de vinilo mayor de 25 por ciento mol.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHBw8gwJ9fX08w8NVnDy9HNxDVJw9vcN8A_2DPH091Nw9HNRCAjyd3YNDlZw8w8Csl0DHIM8_dwVQjxcFYIdfV15GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8b4SRgYGlgaGhqZmhozFRigAaTStC</recordid><startdate>20091110</startdate><enddate>20091110</enddate><creator>ROBERT Q. KLUTTZ</creator><creator>KEITH E. STEPHENS</creator><scope>EVB</scope></search><sort><creationdate>20091110</creationdate><title>BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME</title><author>ROBERT Q. KLUTTZ ; KEITH E. STEPHENS</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_MX2009011561A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; spa</language><creationdate>2009</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>ROBERT Q. KLUTTZ</creatorcontrib><creatorcontrib>KEITH E. STEPHENS</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ROBERT Q. KLUTTZ</au><au>KEITH E. STEPHENS</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME</title><date>2009-11-10</date><risdate>2009</risdate><abstract>The present invention is directed to a process for prepaÏ¿ng a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160°C to 221°C, adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition, and continuing to stir the homogeneous mixture while maintaining the temperature from 180°C to 221°C for a total period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition The block copolymer composition utilized in the process compÏ¿ses one or more block copolymers having at least one monovinylaromatic block and at least one polybutadiene block having a vinyl content of less than 15 mol percent and at least one polybutadiene block having a vinyl content of greater than 25 mol percent. La presente invención se refiere a un proceso para preparar una composición aglutinante bituminosa modificada de polímero en la ausencia sustancial de agentes de reticulación calentando un componente de bitumen en un tanque agitado a una temperatura desde 160°C hasta 221°C, agregando una composición de copolímero de bloque al componente de bitúmen, mientras el componente de bitumen está siendo agitado para formar una mezcla homogénea del componente de bitumen y la composición de copolímero de bloque, y continuar agitando la mezcla homogénea mientras se mantiene la temperatura desde 180°C hasta 221°C por un periodo total desde 4 horas hasta 30 horas, con ello formando una composición aglutinante bituminosa modificada de polímero curada. La composición de copolímero de bloque utilizada en el proceso comprende, uno o más copolímeros de bloque que tiene al menos un bloque monovinilaromático y al menos, un bloque de polibutadieno que tiene un contenido de vinilo de menos de 15 por ciento en mol y al menos, un bloque de polibutadieno que tiene un contenido de vinilo mayor de 25 por ciento mol.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; spa
recordid cdi_epo_espacenet_MX2009011561A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title BITUMINOUS BINDER COMPOSITION AND PROCESS FOR PREPARING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T00%3A43%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ROBERT%20Q.%20KLUTTZ&rft.date=2009-11-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EMX2009011561A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true