Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation

The invention relates to technologies for thin and ultrathin semimetallic microwire production in glass insulation.The process for obtaining bismuth semimetallic microwire in molybdenum glass insulation consists in the extension of the finished microwire heated up to the temperature at which the rat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: POPOV Ion, NIKOLAEVA Albina, ŢURCAN Ana, BODIUL Pavel, GHIŢU Dumitru
Format: Patent
Sprache:eng ; rum ; rus
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator POPOV Ion
NIKOLAEVA Albina
ŢURCAN Ana
BODIUL Pavel
GHIŢU Dumitru
description The invention relates to technologies for thin and ultrathin semimetallic microwire production in glass insulation.The process for obtaining bismuth semimetallic microwire in molybdenum glass insulation consists in the extension of the finished microwire heated up to the temperature at which the ratio between the viscosity factors of the bismuth semimetallic microwire and of the molybdenum glass ηm/ηs attains the value of 0,2. Invenţia se referă la tehnologiile de producere a microfirului fin şi extrafin în izolaţie de sticlă.Procedeul de obţinere a microfirelor semimetalice de bismut în izolaţie de sticlă de molibden constă în întinderea microfirului confecţionat încălzit până la temperatura la care raportul coeficienţilor de viscozitate a microfirului de bismut şi a sticlei de molibden ηm/ηs atinge valoarea de 0,2. Изобретение относится к технологиям производства тонких и сверхтонких полуметаллических микропроводов в стеклянной изоляции.Способ получения полуметаллического микропровода из висмута в молибденовой стеклянной изоляции состоит в растягивании готового микропровода, нагретого до температуры, при которой соотношение между коэффициентами вязкости полуметаллического микропровода из висмута и молибденового стекла ηm/ηs достигает значения 0,2.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_MD3579C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MD3579C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_MD3579C23</originalsourceid><addsrcrecordid>eNqFzLEKAjEMgOEuDqI-gpAXcPEQcT4VF0HQ_Whr7i7QJEfTIr69Du5O__DBP3f3W9aIZtBrBg3Fk5AMEMi4lhEMmRiLT4kiMMWsL8oIJMCa3uGJUhmG5L8DEqvJF1JZulnvk-Hq14Vbn0-P9rLBSTu0yUcULN312Oz2h3bb_PMPHA835A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation</title><source>esp@cenet</source><creator>POPOV Ion ; NIKOLAEVA Albina ; ŢURCAN Ana ; BODIUL Pavel ; GHIŢU Dumitru</creator><creatorcontrib>POPOV Ion ; NIKOLAEVA Albina ; ŢURCAN Ana ; BODIUL Pavel ; GHIŢU Dumitru</creatorcontrib><description>The invention relates to technologies for thin and ultrathin semimetallic microwire production in glass insulation.The process for obtaining bismuth semimetallic microwire in molybdenum glass insulation consists in the extension of the finished microwire heated up to the temperature at which the ratio between the viscosity factors of the bismuth semimetallic microwire and of the molybdenum glass ηm/ηs attains the value of 0,2. Invenţia se referă la tehnologiile de producere a microfirului fin şi extrafin în izolaţie de sticlă.Procedeul de obţinere a microfirelor semimetalice de bismut în izolaţie de sticlă de molibden constă în întinderea microfirului confecţionat încălzit până la temperatura la care raportul coeficienţilor de viscozitate a microfirului de bismut şi a sticlei de molibden ηm/ηs atinge valoarea de 0,2. Изобретение относится к технологиям производства тонких и сверхтонких полуметаллических микропроводов в стеклянной изоляции.Способ получения полуметаллического микропровода из висмута в молибденовой стеклянной изоляции состоит в растягивании готового микропровода, нагретого до температуры, при которой соотношение между коэффициентами вязкости полуметаллического микропровода из висмута и молибденового стекла ηm/ηs достигает значения 0,2.</description><language>eng ; rum ; rus</language><subject>BASIC ELECTRIC ELEMENTS ; CABLES ; CONDUCTORS ; ELECTRICITY ; INSULATORS ; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20081130&amp;DB=EPODOC&amp;CC=MD&amp;NR=3579C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20081130&amp;DB=EPODOC&amp;CC=MD&amp;NR=3579C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>POPOV Ion</creatorcontrib><creatorcontrib>NIKOLAEVA Albina</creatorcontrib><creatorcontrib>ŢURCAN Ana</creatorcontrib><creatorcontrib>BODIUL Pavel</creatorcontrib><creatorcontrib>GHIŢU Dumitru</creatorcontrib><title>Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation</title><description>The invention relates to technologies for thin and ultrathin semimetallic microwire production in glass insulation.The process for obtaining bismuth semimetallic microwire in molybdenum glass insulation consists in the extension of the finished microwire heated up to the temperature at which the ratio between the viscosity factors of the bismuth semimetallic microwire and of the molybdenum glass ηm/ηs attains the value of 0,2. Invenţia se referă la tehnologiile de producere a microfirului fin şi extrafin în izolaţie de sticlă.Procedeul de obţinere a microfirelor semimetalice de bismut în izolaţie de sticlă de molibden constă în întinderea microfirului confecţionat încălzit până la temperatura la care raportul coeficienţilor de viscozitate a microfirului de bismut şi a sticlei de molibden ηm/ηs atinge valoarea de 0,2. Изобретение относится к технологиям производства тонких и сверхтонких полуметаллических микропроводов в стеклянной изоляции.Способ получения полуметаллического микропровода из висмута в молибденовой стеклянной изоляции состоит в растягивании готового микропровода, нагретого до температуры, при которой соотношение между коэффициентами вязкости полуметаллического микропровода из висмута и молибденового стекла ηm/ηs достигает значения 0,2.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CABLES</subject><subject>CONDUCTORS</subject><subject>ELECTRICITY</subject><subject>INSULATORS</subject><subject>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFzLEKAjEMgOEuDqI-gpAXcPEQcT4VF0HQ_Whr7i7QJEfTIr69Du5O__DBP3f3W9aIZtBrBg3Fk5AMEMi4lhEMmRiLT4kiMMWsL8oIJMCa3uGJUhmG5L8DEqvJF1JZulnvk-Hq14Vbn0-P9rLBSTu0yUcULN312Oz2h3bb_PMPHA835A</recordid><startdate>20081130</startdate><enddate>20081130</enddate><creator>POPOV Ion</creator><creator>NIKOLAEVA Albina</creator><creator>ŢURCAN Ana</creator><creator>BODIUL Pavel</creator><creator>GHIŢU Dumitru</creator><scope>EVB</scope></search><sort><creationdate>20081130</creationdate><title>Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation</title><author>POPOV Ion ; NIKOLAEVA Albina ; ŢURCAN Ana ; BODIUL Pavel ; GHIŢU Dumitru</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_MD3579C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; rum ; rus</language><creationdate>2008</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CABLES</topic><topic>CONDUCTORS</topic><topic>ELECTRICITY</topic><topic>INSULATORS</topic><topic>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</topic><toplevel>online_resources</toplevel><creatorcontrib>POPOV Ion</creatorcontrib><creatorcontrib>NIKOLAEVA Albina</creatorcontrib><creatorcontrib>ŢURCAN Ana</creatorcontrib><creatorcontrib>BODIUL Pavel</creatorcontrib><creatorcontrib>GHIŢU Dumitru</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>POPOV Ion</au><au>NIKOLAEVA Albina</au><au>ŢURCAN Ana</au><au>BODIUL Pavel</au><au>GHIŢU Dumitru</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation</title><date>2008-11-30</date><risdate>2008</risdate><abstract>The invention relates to technologies for thin and ultrathin semimetallic microwire production in glass insulation.The process for obtaining bismuth semimetallic microwire in molybdenum glass insulation consists in the extension of the finished microwire heated up to the temperature at which the ratio between the viscosity factors of the bismuth semimetallic microwire and of the molybdenum glass ηm/ηs attains the value of 0,2. Invenţia se referă la tehnologiile de producere a microfirului fin şi extrafin în izolaţie de sticlă.Procedeul de obţinere a microfirelor semimetalice de bismut în izolaţie de sticlă de molibden constă în întinderea microfirului confecţionat încălzit până la temperatura la care raportul coeficienţilor de viscozitate a microfirului de bismut şi a sticlei de molibden ηm/ηs atinge valoarea de 0,2. Изобретение относится к технологиям производства тонких и сверхтонких полуметаллических микропроводов в стеклянной изоляции.Способ получения полуметаллического микропровода из висмута в молибденовой стеклянной изоляции состоит в растягивании готового микропровода, нагретого до температуры, при которой соотношение между коэффициентами вязкости полуметаллического микропровода из висмута и молибденового стекла ηm/ηs достигает значения 0,2.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; rum ; rus
recordid cdi_epo_espacenet_MD3579C2
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CABLES
CONDUCTORS
ELECTRICITY
INSULATORS
SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES
title Process for obtaining bismuth semimetallic microwire in molybdenum glass insulation
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T21%3A58%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=POPOV%20Ion&rft.date=2008-11-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EMD3579C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true