Method for improving crack resistance of recycled concrete
A method for improving the crack resistance of recycled concrete, which relates to the technical field of concrete. In this method, slag powder, anti-crack composite fiber and silica fume are added into recycled concrete to prepare anti-crack recycled concrete to improve the anti-crack performance....
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | GUAN Qiaoyan |
description | A method for improving the crack resistance of recycled concrete, which relates to the technical field of concrete. In this method, slag powder, anti-crack composite fiber and silica fume are added into recycled concrete to prepare anti-crack recycled concrete to improve the anti-crack performance. The anti-crack recycled concrete comprises the following components in parts by weight: 200-250 parts of cement, 150-200 parts of water, 550-650 parts of recycled coarse aggregate, 500-600 parts of recycled fine aggregate, 40-70 parts of slag powder, 80-100 parts of anti-crack composite fiber and 4-8 parts of silica fume. According to the invention, the slag powder, the anti-crack composite fiber and the silica fume are added into the recycled concrete to prepare the anti-crack recycled concrete, so as to improve the anti-crack performance of the recycled concrete, and the compressive strength is up to 59.6MPa and the splitting tensile strength is up to 5.3MPa. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_LU501385B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>LU501385B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_LU501385B13</originalsourceid><addsrcrecordid>eNrjZLDyTS3JyE9RSMsvUsjMLSjKL8vMS1dILkpMzlYoSi3OLC5JzEtOVchPA_KSK5NzUlMUkvPzkotSS1J5GFjTEnOKU3mhNDeDvJtriLOHbmpBfnxqcUFicmpeakm8T6ipgaGxhamToTFhFQDSgi54</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for improving crack resistance of recycled concrete</title><source>esp@cenet</source><creator>GUAN Qiaoyan</creator><creatorcontrib>GUAN Qiaoyan</creatorcontrib><description>A method for improving the crack resistance of recycled concrete, which relates to the technical field of concrete. In this method, slag powder, anti-crack composite fiber and silica fume are added into recycled concrete to prepare anti-crack recycled concrete to improve the anti-crack performance. The anti-crack recycled concrete comprises the following components in parts by weight: 200-250 parts of cement, 150-200 parts of water, 550-650 parts of recycled coarse aggregate, 500-600 parts of recycled fine aggregate, 40-70 parts of slag powder, 80-100 parts of anti-crack composite fiber and 4-8 parts of silica fume. According to the invention, the slag powder, the anti-crack composite fiber and the silica fume are added into the recycled concrete to prepare the anti-crack recycled concrete, so as to improve the anti-crack performance of the recycled concrete, and the compressive strength is up to 59.6MPa and the splitting tensile strength is up to 5.3MPa.</description><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220810&DB=EPODOC&CC=LU&NR=501385B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220810&DB=EPODOC&CC=LU&NR=501385B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GUAN Qiaoyan</creatorcontrib><title>Method for improving crack resistance of recycled concrete</title><description>A method for improving the crack resistance of recycled concrete, which relates to the technical field of concrete. In this method, slag powder, anti-crack composite fiber and silica fume are added into recycled concrete to prepare anti-crack recycled concrete to improve the anti-crack performance. The anti-crack recycled concrete comprises the following components in parts by weight: 200-250 parts of cement, 150-200 parts of water, 550-650 parts of recycled coarse aggregate, 500-600 parts of recycled fine aggregate, 40-70 parts of slag powder, 80-100 parts of anti-crack composite fiber and 4-8 parts of silica fume. According to the invention, the slag powder, the anti-crack composite fiber and the silica fume are added into the recycled concrete to prepare the anti-crack recycled concrete, so as to improve the anti-crack performance of the recycled concrete, and the compressive strength is up to 59.6MPa and the splitting tensile strength is up to 5.3MPa.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDyTS3JyE9RSMsvUsjMLSjKL8vMS1dILkpMzlYoSi3OLC5JzEtOVchPA_KSK5NzUlMUkvPzkotSS1J5GFjTEnOKU3mhNDeDvJtriLOHbmpBfnxqcUFicmpeakm8T6ipgaGxhamToTFhFQDSgi54</recordid><startdate>20220810</startdate><enddate>20220810</enddate><creator>GUAN Qiaoyan</creator><scope>EVB</scope></search><sort><creationdate>20220810</creationdate><title>Method for improving crack resistance of recycled concrete</title><author>GUAN Qiaoyan</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_LU501385B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2022</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>GUAN Qiaoyan</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GUAN Qiaoyan</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for improving crack resistance of recycled concrete</title><date>2022-08-10</date><risdate>2022</risdate><abstract>A method for improving the crack resistance of recycled concrete, which relates to the technical field of concrete. In this method, slag powder, anti-crack composite fiber and silica fume are added into recycled concrete to prepare anti-crack recycled concrete to improve the anti-crack performance. The anti-crack recycled concrete comprises the following components in parts by weight: 200-250 parts of cement, 150-200 parts of water, 550-650 parts of recycled coarse aggregate, 500-600 parts of recycled fine aggregate, 40-70 parts of slag powder, 80-100 parts of anti-crack composite fiber and 4-8 parts of silica fume. According to the invention, the slag powder, the anti-crack composite fiber and the silica fume are added into the recycled concrete to prepare the anti-crack recycled concrete, so as to improve the anti-crack performance of the recycled concrete, and the compressive strength is up to 59.6MPa and the splitting tensile strength is up to 5.3MPa.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_LU501385B1 |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | Method for improving crack resistance of recycled concrete |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T11%3A49%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GUAN%20Qiaoyan&rft.date=2022-08-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ELU501385B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |