WATER SOTUABLE-COATING COMPOSITION

Water sol. and nonflammable spray coating compn. (I) Which consisted mainly of carboxyl group-contg. resin and pigment, and having solid 10-40 and volatile material 90-60wt.% such as water sol. amino compd. and solvent was obtained. The solvent consisted of water 10-50, ethyleneglycol. monoethylethe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DAKADA HIROSI, MAKADA RAKUMI, HAYASI MASAKI, HASUI KENGI, SKIMODO KUNIO
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DAKADA HIROSI
MAKADA RAKUMI
HAYASI MASAKI
HASUI KENGI
SKIMODO KUNIO
description Water sol. and nonflammable spray coating compn. (I) Which consisted mainly of carboxyl group-contg. resin and pigment, and having solid 10-40 and volatile material 90-60wt.% such as water sol. amino compd. and solvent was obtained. The solvent consisted of water 10-50, ethyleneglycol. monoethylether 87.5-30 wt.%, and one or a mixt. of alkylacohol, alkylether or alkyl esterified alcohol 2.5-20wt. %, and various additives mixed with I as necessary.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR790000752BB1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR790000752BB1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR790000752BB13</originalsourceid><addsrcrecordid>eNrjZFAKdwxxDVII9g8JdXTycdV19ncM8fRzV3D29w3wD_YM8fT342FgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5B5pYGQGBuauTkZGhMnCoA3oojsQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>WATER SOTUABLE-COATING COMPOSITION</title><source>esp@cenet</source><creator>DAKADA HIROSI ; MAKADA RAKUMI ; HAYASI MASAKI ; HASUI KENGI ; SKIMODO KUNIO</creator><creatorcontrib>DAKADA HIROSI ; MAKADA RAKUMI ; HAYASI MASAKI ; HASUI KENGI ; SKIMODO KUNIO</creatorcontrib><description>Water sol. and nonflammable spray coating compn. (I) Which consisted mainly of carboxyl group-contg. resin and pigment, and having solid 10-40 and volatile material 90-60wt.% such as water sol. amino compd. and solvent was obtained. The solvent consisted of water 10-50, ethyleneglycol. monoethylether 87.5-30 wt.%, and one or a mixt. of alkylacohol, alkylether or alkyl esterified alcohol 2.5-20wt. %, and various additives mixed with I as necessary.</description><language>eng</language><creationdate>1979</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19790629&amp;DB=EPODOC&amp;CC=KR&amp;NR=790000752B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19790629&amp;DB=EPODOC&amp;CC=KR&amp;NR=790000752B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DAKADA HIROSI</creatorcontrib><creatorcontrib>MAKADA RAKUMI</creatorcontrib><creatorcontrib>HAYASI MASAKI</creatorcontrib><creatorcontrib>HASUI KENGI</creatorcontrib><creatorcontrib>SKIMODO KUNIO</creatorcontrib><title>WATER SOTUABLE-COATING COMPOSITION</title><description>Water sol. and nonflammable spray coating compn. (I) Which consisted mainly of carboxyl group-contg. resin and pigment, and having solid 10-40 and volatile material 90-60wt.% such as water sol. amino compd. and solvent was obtained. The solvent consisted of water 10-50, ethyleneglycol. monoethylether 87.5-30 wt.%, and one or a mixt. of alkylacohol, alkylether or alkyl esterified alcohol 2.5-20wt. %, and various additives mixed with I as necessary.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1979</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFAKdwxxDVII9g8JdXTycdV19ncM8fRzV3D29w3wD_YM8fT342FgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5B5pYGQGBuauTkZGhMnCoA3oojsQ</recordid><startdate>19790629</startdate><enddate>19790629</enddate><creator>DAKADA HIROSI</creator><creator>MAKADA RAKUMI</creator><creator>HAYASI MASAKI</creator><creator>HASUI KENGI</creator><creator>SKIMODO KUNIO</creator><scope>EVB</scope></search><sort><creationdate>19790629</creationdate><title>WATER SOTUABLE-COATING COMPOSITION</title><author>DAKADA HIROSI ; MAKADA RAKUMI ; HAYASI MASAKI ; HASUI KENGI ; SKIMODO KUNIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR790000752BB13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1979</creationdate><toplevel>online_resources</toplevel><creatorcontrib>DAKADA HIROSI</creatorcontrib><creatorcontrib>MAKADA RAKUMI</creatorcontrib><creatorcontrib>HAYASI MASAKI</creatorcontrib><creatorcontrib>HASUI KENGI</creatorcontrib><creatorcontrib>SKIMODO KUNIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DAKADA HIROSI</au><au>MAKADA RAKUMI</au><au>HAYASI MASAKI</au><au>HASUI KENGI</au><au>SKIMODO KUNIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>WATER SOTUABLE-COATING COMPOSITION</title><date>1979-06-29</date><risdate>1979</risdate><abstract>Water sol. and nonflammable spray coating compn. (I) Which consisted mainly of carboxyl group-contg. resin and pigment, and having solid 10-40 and volatile material 90-60wt.% such as water sol. amino compd. and solvent was obtained. The solvent consisted of water 10-50, ethyleneglycol. monoethylether 87.5-30 wt.%, and one or a mixt. of alkylacohol, alkylether or alkyl esterified alcohol 2.5-20wt. %, and various additives mixed with I as necessary.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_KR790000752BB1
source esp@cenet
title WATER SOTUABLE-COATING COMPOSITION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T12%3A44%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DAKADA%20HIROSI&rft.date=1979-06-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR790000752BB1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true