Manufacturing Method and Apparatus for Powder Activator Admixture including Ferro-nickel Slag Fine Powder

The present invention relates to a method and an apparatus for preparing a powder activation admixture including ferronickel slag fine powder. The method of the present invention comprises: a first grinding step of primarily grinding a raw material; a second grinding step of secondarily grinding fin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HWANG JUN PHIL, LEE CHANG HONG
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The present invention relates to a method and an apparatus for preparing a powder activation admixture including ferronickel slag fine powder. The method of the present invention comprises: a first grinding step of primarily grinding a raw material; a second grinding step of secondarily grinding fine powder ground and divided in the first grinding step; a third grinding step of thirdly grinding the fine powder ground and divided in the second grinding step; and a step of generating mixed fine powder of a third brain by mixing the fine powder of first and second brains divided by being completed with the second and second grinding steps. According to the present invention, specialized performance and differentiated specialized performance of a raw material are improved, and economic feasibility (cost-effectiveness) is enhanced in an aspect of developing an alternative cement admixture, and an aspect of verifying applicability for mass-utilization and distribution is excellent to maximize the utilization of ferronickel slag, thereby increasing a recycling rate of the ferronickel slag and minimizing disposal costs of the ferronickel slag. 본 발명은 페로니켈 슬래그 미분말을 포함하는 분말 활성화 혼화재의 제조 방법 및 장치에 관한 것으로, 원재료를 1차로 분쇄하는 제1 분쇄 단계, 상기 제1 분쇄 단계에서 분쇄되어 분급된 미분말을 2차로 분쇄하는 제2 분쇄 단계, 상기 제2 분쇄 단계에서 분쇄되어 분급된 미분말을 3차로 분쇄하는 제3 분쇄 단계, 및 상기 제2 및 제3 분쇄 단계를 거쳐 분급된 상기 제1 및 제2 브레인의 미분말을 혼합하여 제3 브레인의 혼합 미분말을 생성하는 단계를 포함하는 페로니켈 슬래그 미분말을 포함하는 분말 활성화 혼화재의 제조 방법이 제공되며, 시멘트 치환 대체 혼화재의 개발 측면에서 원소재의 특화성능, 차별화 특화성능 개선, 경제성(가성비) 증진, 대량활용 보급을 위한 적용성 검증의 측면에서 우수하기 때문에 페로니켈 슬래그에 대한 활용도를 최대화함으로써 페로니켈 슬래그의 재활용률을 높임과 동시에 페로니켈 슬래그의 폐처분 비용을 최소화할 수 있는 효과가 있다.