Manufacturing method of graphite oxide for heater

The present invention relates to a method for preparing graphite oxide for a heating unit, which comprises the steps of: firing and pulverizing conventional graphite ore to prepare high-purity graphite powder; introducing sulfuric acid, nitric acid and potassium nitrate powder into a reactor to obta...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: YOO, SI HUNG
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YOO, SI HUNG
description The present invention relates to a method for preparing graphite oxide for a heating unit, which comprises the steps of: firing and pulverizing conventional graphite ore to prepare high-purity graphite powder; introducing sulfuric acid, nitric acid and potassium nitrate powder into a reactor to obtain a mixed acid and introducing the high-purity graphite powder to the reactor, followed by mixing; aging the mixture agitated in the reactor; heating the aged mixture to carry out reaction and introducing distilled water to carry out cooling; filtering and dehydrating the cooled mixture to obtain graphite oxide paste; and neutralizing the graphite oxide paste to pH 7-8. 본 발명의 일 실시예에 따른 발열체용 산화흑연의 제조방법은, 일반흑연광물을 소성 및 분쇄하여 고순도의 흑연분말을 준비하는 과정; 반응기에 황산, 질산 및 질산칼륨 분말을 투입하여 혼합산을 제조하고 상기 고순도의 흑연분말을 상기 반응기에 투입하여 믹싱하는 과정; 상기 반응기에서 교반한 혼합물을 숙성시키는 과정: 상기 숙성된 혼합물을 가열하여 반응시킨 후 증류수를 투입하여 냉각시키는 과정; 상기 냉각된 혼합물을 필터링하고 탈수하여 산화흑연 페이스트를 제조하는 과정; 및 상기 제조된 산화흑연 페이스트를 pH 7~8로 중화시키는 과정을 포함한다.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20160121232A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20160121232A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20160121232A3</originalsourceid><addsrcrecordid>eNrjZDD0TcwrTUtMLiktysxLV8hNLcnIT1HIT1NIL0osyMgsSVXIr8hMSVVIyy9SyEhNLEkt4mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5BRgaGZgaGRoZGxkaOxsSpAgBHHixz</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Manufacturing method of graphite oxide for heater</title><source>esp@cenet</source><creator>YOO, SI HUNG</creator><creatorcontrib>YOO, SI HUNG</creatorcontrib><description>The present invention relates to a method for preparing graphite oxide for a heating unit, which comprises the steps of: firing and pulverizing conventional graphite ore to prepare high-purity graphite powder; introducing sulfuric acid, nitric acid and potassium nitrate powder into a reactor to obtain a mixed acid and introducing the high-purity graphite powder to the reactor, followed by mixing; aging the mixture agitated in the reactor; heating the aged mixture to carry out reaction and introducing distilled water to carry out cooling; filtering and dehydrating the cooled mixture to obtain graphite oxide paste; and neutralizing the graphite oxide paste to pH 7-8. 본 발명의 일 실시예에 따른 발열체용 산화흑연의 제조방법은, 일반흑연광물을 소성 및 분쇄하여 고순도의 흑연분말을 준비하는 과정; 반응기에 황산, 질산 및 질산칼륨 분말을 투입하여 혼합산을 제조하고 상기 고순도의 흑연분말을 상기 반응기에 투입하여 믹싱하는 과정; 상기 반응기에서 교반한 혼합물을 숙성시키는 과정: 상기 숙성된 혼합물을 가열하여 반응시킨 후 증류수를 투입하여 냉각시키는 과정; 상기 냉각된 혼합물을 필터링하고 탈수하여 산화흑연 페이스트를 제조하는 과정; 및 상기 제조된 산화흑연 페이스트를 pH 7~8로 중화시키는 과정을 포함한다.</description><language>eng ; kor</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; ELECTRIC HEATING ; ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR ; ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161019&amp;DB=EPODOC&amp;CC=KR&amp;NR=20160121232A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161019&amp;DB=EPODOC&amp;CC=KR&amp;NR=20160121232A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YOO, SI HUNG</creatorcontrib><title>Manufacturing method of graphite oxide for heater</title><description>The present invention relates to a method for preparing graphite oxide for a heating unit, which comprises the steps of: firing and pulverizing conventional graphite ore to prepare high-purity graphite powder; introducing sulfuric acid, nitric acid and potassium nitrate powder into a reactor to obtain a mixed acid and introducing the high-purity graphite powder to the reactor, followed by mixing; aging the mixture agitated in the reactor; heating the aged mixture to carry out reaction and introducing distilled water to carry out cooling; filtering and dehydrating the cooled mixture to obtain graphite oxide paste; and neutralizing the graphite oxide paste to pH 7-8. 본 발명의 일 실시예에 따른 발열체용 산화흑연의 제조방법은, 일반흑연광물을 소성 및 분쇄하여 고순도의 흑연분말을 준비하는 과정; 반응기에 황산, 질산 및 질산칼륨 분말을 투입하여 혼합산을 제조하고 상기 고순도의 흑연분말을 상기 반응기에 투입하여 믹싱하는 과정; 상기 반응기에서 교반한 혼합물을 숙성시키는 과정: 상기 숙성된 혼합물을 가열하여 반응시킨 후 증류수를 투입하여 냉각시키는 과정; 상기 냉각된 혼합물을 필터링하고 탈수하여 산화흑연 페이스트를 제조하는 과정; 및 상기 제조된 산화흑연 페이스트를 pH 7~8로 중화시키는 과정을 포함한다.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>ELECTRIC HEATING</subject><subject>ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD0TcwrTUtMLiktysxLV8hNLcnIT1HIT1NIL0osyMgsSVXIr8hMSVVIyy9SyEhNLEkt4mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5BRgaGZgaGRoZGxkaOxsSpAgBHHixz</recordid><startdate>20161019</startdate><enddate>20161019</enddate><creator>YOO, SI HUNG</creator><scope>EVB</scope></search><sort><creationdate>20161019</creationdate><title>Manufacturing method of graphite oxide for heater</title><author>YOO, SI HUNG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20160121232A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; kor</language><creationdate>2016</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>ELECTRIC HEATING</topic><topic>ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>YOO, SI HUNG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YOO, SI HUNG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Manufacturing method of graphite oxide for heater</title><date>2016-10-19</date><risdate>2016</risdate><abstract>The present invention relates to a method for preparing graphite oxide for a heating unit, which comprises the steps of: firing and pulverizing conventional graphite ore to prepare high-purity graphite powder; introducing sulfuric acid, nitric acid and potassium nitrate powder into a reactor to obtain a mixed acid and introducing the high-purity graphite powder to the reactor, followed by mixing; aging the mixture agitated in the reactor; heating the aged mixture to carry out reaction and introducing distilled water to carry out cooling; filtering and dehydrating the cooled mixture to obtain graphite oxide paste; and neutralizing the graphite oxide paste to pH 7-8. 본 발명의 일 실시예에 따른 발열체용 산화흑연의 제조방법은, 일반흑연광물을 소성 및 분쇄하여 고순도의 흑연분말을 준비하는 과정; 반응기에 황산, 질산 및 질산칼륨 분말을 투입하여 혼합산을 제조하고 상기 고순도의 흑연분말을 상기 반응기에 투입하여 믹싱하는 과정; 상기 반응기에서 교반한 혼합물을 숙성시키는 과정: 상기 숙성된 혼합물을 가열하여 반응시킨 후 증류수를 투입하여 냉각시키는 과정; 상기 냉각된 혼합물을 필터링하고 탈수하여 산화흑연 페이스트를 제조하는 과정; 및 상기 제조된 산화흑연 페이스트를 pH 7~8로 중화시키는 과정을 포함한다.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; kor
recordid cdi_epo_espacenet_KR20160121232A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
ELECTRIC HEATING
ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR
ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Manufacturing method of graphite oxide for heater
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T13%3A31%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YOO,%20SI%20HUNG&rft.date=2016-10-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20160121232A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true