WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME

PURPOSE: Wrinkle resistivity improved security paper and a manufacturing method thereof are provided to bridge-bond fibers and resins by dipping wet paper in a creasing prevention aqueous solution or to form strong cross-linked bond between fibers of paper with compounds by heat, light or electrical...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEE, SONG MIN, JOUNG, YANG JIN, HEO, YONG DAE, KIM, TAE YOUNG, KIM, DUC KI
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LEE, SONG MIN
JOUNG, YANG JIN
HEO, YONG DAE
KIM, TAE YOUNG
KIM, DUC KI
description PURPOSE: Wrinkle resistivity improved security paper and a manufacturing method thereof are provided to bridge-bond fibers and resins by dipping wet paper in a creasing prevention aqueous solution or to form strong cross-linked bond between fibers of paper with compounds by heat, light or electrical effect etc. CONSTITUTION: A manufacturing method for wrinkle resistivity improved security paper comprises following steps. A paper stock is manufactured by using natural fibers (S10). A stencil paper is manufactured by adding the predetermined amount of monomer solution having a double bond into the paper stock in order to bridge-react to the cellulose molecules of natural fibers and press-drying the same (S10). The stencil paper is dipped in a creasing prevention surface process aqueous solution (S30). Thermal, infrared rays or electromagnetic waves are treated so that cross-link bond between the cellulose molecules of the stencil paper and the creasing prevention surface process aqueous solution is formed and hardened (S40). [Reference numerals] (AA) Start; (BB) End; (S10) Manufacture paper stock; (S20) Add monomer solution having a double bond into the paper stock; (S30) Dip wet paper into monomer solution having a double bond; (S40) Treat heat, infrared rays or electromagnetic waves
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20130117974A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20130117974A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20130117974A3</originalsourceid><addsrcrecordid>eNrjZHAN9_Tz9nHVDXIN9gwO8QxzVQh2dQ4N8gyJVAhwDHANUnD0c1HwdQ3x8HdRcPMPUvB19At1c3QOASrxc1cI8QCqd_R15WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5BRgaGxgaGhuaW5iaOxsSpAgBLxy0J</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME</title><source>esp@cenet</source><creator>LEE, SONG MIN ; JOUNG, YANG JIN ; HEO, YONG DAE ; KIM, TAE YOUNG ; KIM, DUC KI</creator><creatorcontrib>LEE, SONG MIN ; JOUNG, YANG JIN ; HEO, YONG DAE ; KIM, TAE YOUNG ; KIM, DUC KI</creatorcontrib><description>PURPOSE: Wrinkle resistivity improved security paper and a manufacturing method thereof are provided to bridge-bond fibers and resins by dipping wet paper in a creasing prevention aqueous solution or to form strong cross-linked bond between fibers of paper with compounds by heat, light or electrical effect etc. CONSTITUTION: A manufacturing method for wrinkle resistivity improved security paper comprises following steps. A paper stock is manufactured by using natural fibers (S10). A stencil paper is manufactured by adding the predetermined amount of monomer solution having a double bond into the paper stock in order to bridge-react to the cellulose molecules of natural fibers and press-drying the same (S10). The stencil paper is dipped in a creasing prevention surface process aqueous solution (S30). Thermal, infrared rays or electromagnetic waves are treated so that cross-link bond between the cellulose molecules of the stencil paper and the creasing prevention surface process aqueous solution is formed and hardened (S40). [Reference numerals] (AA) Start; (BB) End; (S10) Manufacture paper stock; (S20) Add monomer solution having a double bond into the paper stock; (S30) Dip wet paper into monomer solution having a double bond; (S40) Treat heat, infrared rays or electromagnetic waves</description><language>eng ; kor</language><subject>IMPREGNATING OR COATING OF PAPER ; PAPER NOT OTHERWISE PROVIDED FOR ; PAPER-MAKING ; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D ; PRODUCTION OF CELLULOSE ; PULP COMPOSITIONS ; TEXTILES ; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131029&amp;DB=EPODOC&amp;CC=KR&amp;NR=20130117974A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131029&amp;DB=EPODOC&amp;CC=KR&amp;NR=20130117974A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LEE, SONG MIN</creatorcontrib><creatorcontrib>JOUNG, YANG JIN</creatorcontrib><creatorcontrib>HEO, YONG DAE</creatorcontrib><creatorcontrib>KIM, TAE YOUNG</creatorcontrib><creatorcontrib>KIM, DUC KI</creatorcontrib><title>WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME</title><description>PURPOSE: Wrinkle resistivity improved security paper and a manufacturing method thereof are provided to bridge-bond fibers and resins by dipping wet paper in a creasing prevention aqueous solution or to form strong cross-linked bond between fibers of paper with compounds by heat, light or electrical effect etc. CONSTITUTION: A manufacturing method for wrinkle resistivity improved security paper comprises following steps. A paper stock is manufactured by using natural fibers (S10). A stencil paper is manufactured by adding the predetermined amount of monomer solution having a double bond into the paper stock in order to bridge-react to the cellulose molecules of natural fibers and press-drying the same (S10). The stencil paper is dipped in a creasing prevention surface process aqueous solution (S30). Thermal, infrared rays or electromagnetic waves are treated so that cross-link bond between the cellulose molecules of the stencil paper and the creasing prevention surface process aqueous solution is formed and hardened (S40). [Reference numerals] (AA) Start; (BB) End; (S10) Manufacture paper stock; (S20) Add monomer solution having a double bond into the paper stock; (S30) Dip wet paper into monomer solution having a double bond; (S40) Treat heat, infrared rays or electromagnetic waves</description><subject>IMPREGNATING OR COATING OF PAPER</subject><subject>PAPER NOT OTHERWISE PROVIDED FOR</subject><subject>PAPER-MAKING</subject><subject>PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D</subject><subject>PRODUCTION OF CELLULOSE</subject><subject>PULP COMPOSITIONS</subject><subject>TEXTILES</subject><subject>TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAN9_Tz9nHVDXIN9gwO8QxzVQh2dQ4N8gyJVAhwDHANUnD0c1HwdQ3x8HdRcPMPUvB19At1c3QOASrxc1cI8QCqd_R15WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8d5BRgaGxgaGhuaW5iaOxsSpAgBLxy0J</recordid><startdate>20131029</startdate><enddate>20131029</enddate><creator>LEE, SONG MIN</creator><creator>JOUNG, YANG JIN</creator><creator>HEO, YONG DAE</creator><creator>KIM, TAE YOUNG</creator><creator>KIM, DUC KI</creator><scope>EVB</scope></search><sort><creationdate>20131029</creationdate><title>WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME</title><author>LEE, SONG MIN ; JOUNG, YANG JIN ; HEO, YONG DAE ; KIM, TAE YOUNG ; KIM, DUC KI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20130117974A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; kor</language><creationdate>2013</creationdate><topic>IMPREGNATING OR COATING OF PAPER</topic><topic>PAPER NOT OTHERWISE PROVIDED FOR</topic><topic>PAPER-MAKING</topic><topic>PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D</topic><topic>PRODUCTION OF CELLULOSE</topic><topic>PULP COMPOSITIONS</topic><topic>TEXTILES</topic><topic>TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G</topic><toplevel>online_resources</toplevel><creatorcontrib>LEE, SONG MIN</creatorcontrib><creatorcontrib>JOUNG, YANG JIN</creatorcontrib><creatorcontrib>HEO, YONG DAE</creatorcontrib><creatorcontrib>KIM, TAE YOUNG</creatorcontrib><creatorcontrib>KIM, DUC KI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LEE, SONG MIN</au><au>JOUNG, YANG JIN</au><au>HEO, YONG DAE</au><au>KIM, TAE YOUNG</au><au>KIM, DUC KI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME</title><date>2013-10-29</date><risdate>2013</risdate><abstract>PURPOSE: Wrinkle resistivity improved security paper and a manufacturing method thereof are provided to bridge-bond fibers and resins by dipping wet paper in a creasing prevention aqueous solution or to form strong cross-linked bond between fibers of paper with compounds by heat, light or electrical effect etc. CONSTITUTION: A manufacturing method for wrinkle resistivity improved security paper comprises following steps. A paper stock is manufactured by using natural fibers (S10). A stencil paper is manufactured by adding the predetermined amount of monomer solution having a double bond into the paper stock in order to bridge-react to the cellulose molecules of natural fibers and press-drying the same (S10). The stencil paper is dipped in a creasing prevention surface process aqueous solution (S30). Thermal, infrared rays or electromagnetic waves are treated so that cross-link bond between the cellulose molecules of the stencil paper and the creasing prevention surface process aqueous solution is formed and hardened (S40). [Reference numerals] (AA) Start; (BB) End; (S10) Manufacture paper stock; (S20) Add monomer solution having a double bond into the paper stock; (S30) Dip wet paper into monomer solution having a double bond; (S40) Treat heat, infrared rays or electromagnetic waves</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; kor
recordid cdi_epo_espacenet_KR20130117974A
source esp@cenet
subjects IMPREGNATING OR COATING OF PAPER
PAPER NOT OTHERWISE PROVIDED FOR
PAPER-MAKING
PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D
PRODUCTION OF CELLULOSE
PULP COMPOSITIONS
TEXTILES
TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G
title WINKLE-RESISTIVE SECURITY PAPER AND METHOD FOR MANUFACTURING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T15%3A28%3A21IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LEE,%20SONG%20MIN&rft.date=2013-10-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20130117974A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true