METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD
PURPOSE: A method for manufacturing an expanded perlite board is provided to achieve superior quality and to reduce time required for a plasticizing process by including a primary plasticizing process with microwaves. CONSTITUTION: A method for manufacturing an expanded perlite board includes the fo...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; kor |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KIM, KWAN JE LEE, HWA CHAN |
description | PURPOSE: A method for manufacturing an expanded perlite board is provided to achieve superior quality and to reduce time required for a plasticizing process by including a primary plasticizing process with microwaves. CONSTITUTION: A method for manufacturing an expanded perlite board includes the following steps of: mixing 2000 parts by weight of expanded perlite, 450-800 parts by weight of a low temperature binder, and water; molding the mixture with a press molding method; surface-treating the molded product, and applying coating liquid on the surface of the molded product; and completing a product by primarily plasticizing the molded product in a microwave plasticizing furnace and secondarily plasticizing the molded product in a high temperature plasticizing furnace. The low temperature binder is composed of 400-600 parts by weight of sodium silicate and 50-200 parts by weight of a stabilizer based on 2000 parts by weight of the expanded perlite. If a high temperature binder is used for the mixing process, 2000 parts by weight of the expanded perlite, 1,000-1,500 parts by weight of water, and 450-800 parts by weight of a glaze, which is the high temperature binder, are mixed. The molded product is carried by a conveyor carrying method in the completing process. [Reference numerals] (AA) Primary plasticize; (BB) Secondary plasticize; (S101) Mix; (S102) Shape; (S103) Surface treat and coat |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20130068211A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20130068211A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20130068211A3</originalsourceid><addsrcrecordid>eNrjZND3dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcI0IcPRzcXVRCHAN8vEMcVVw8ncMcuFhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfHeQUYGhsYGBmYWRoaGjsbEqQIAmm4mxA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD</title><source>esp@cenet</source><creator>KIM, KWAN JE ; LEE, HWA CHAN</creator><creatorcontrib>KIM, KWAN JE ; LEE, HWA CHAN</creatorcontrib><description>PURPOSE: A method for manufacturing an expanded perlite board is provided to achieve superior quality and to reduce time required for a plasticizing process by including a primary plasticizing process with microwaves. CONSTITUTION: A method for manufacturing an expanded perlite board includes the following steps of: mixing 2000 parts by weight of expanded perlite, 450-800 parts by weight of a low temperature binder, and water; molding the mixture with a press molding method; surface-treating the molded product, and applying coating liquid on the surface of the molded product; and completing a product by primarily plasticizing the molded product in a microwave plasticizing furnace and secondarily plasticizing the molded product in a high temperature plasticizing furnace. The low temperature binder is composed of 400-600 parts by weight of sodium silicate and 50-200 parts by weight of a stabilizer based on 2000 parts by weight of the expanded perlite. If a high temperature binder is used for the mixing process, 2000 parts by weight of the expanded perlite, 1,000-1,500 parts by weight of water, and 450-800 parts by weight of a glaze, which is the high temperature binder, are mixed. The molded product is carried by a conveyor carrying method in the completing process. [Reference numerals] (AA) Primary plasticize; (BB) Secondary plasticize; (S101) Mix; (S102) Shape; (S103) Surface treat and coat</description><language>eng ; kor</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; REFRACTORIES ; SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER ; SLAG ; TRANSPORTING ; TREATMENT OF NATURAL STONE ; WORKING CEMENT, CLAY, OR STONE</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130626&DB=EPODOC&CC=KR&NR=20130068211A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130626&DB=EPODOC&CC=KR&NR=20130068211A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KIM, KWAN JE</creatorcontrib><creatorcontrib>LEE, HWA CHAN</creatorcontrib><title>METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD</title><description>PURPOSE: A method for manufacturing an expanded perlite board is provided to achieve superior quality and to reduce time required for a plasticizing process by including a primary plasticizing process with microwaves. CONSTITUTION: A method for manufacturing an expanded perlite board includes the following steps of: mixing 2000 parts by weight of expanded perlite, 450-800 parts by weight of a low temperature binder, and water; molding the mixture with a press molding method; surface-treating the molded product, and applying coating liquid on the surface of the molded product; and completing a product by primarily plasticizing the molded product in a microwave plasticizing furnace and secondarily plasticizing the molded product in a high temperature plasticizing furnace. The low temperature binder is composed of 400-600 parts by weight of sodium silicate and 50-200 parts by weight of a stabilizer based on 2000 parts by weight of the expanded perlite. If a high temperature binder is used for the mixing process, 2000 parts by weight of the expanded perlite, 1,000-1,500 parts by weight of water, and 450-800 parts by weight of a glaze, which is the high temperature binder, are mixed. The molded product is carried by a conveyor carrying method in the completing process. [Reference numerals] (AA) Primary plasticize; (BB) Secondary plasticize; (S101) Mix; (S102) Shape; (S103) Surface treat and coat</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>REFRACTORIES</subject><subject>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</subject><subject>SLAG</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>WORKING CEMENT, CLAY, OR STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND3dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcI0IcPRzcXVRCHAN8vEMcVVw8ncMcuFhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfHeQUYGhsYGBmYWRoaGjsbEqQIAmm4mxA</recordid><startdate>20130626</startdate><enddate>20130626</enddate><creator>KIM, KWAN JE</creator><creator>LEE, HWA CHAN</creator><scope>EVB</scope></search><sort><creationdate>20130626</creationdate><title>METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD</title><author>KIM, KWAN JE ; LEE, HWA CHAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20130068211A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; kor</language><creationdate>2013</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>REFRACTORIES</topic><topic>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</topic><topic>SLAG</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>WORKING CEMENT, CLAY, OR STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>KIM, KWAN JE</creatorcontrib><creatorcontrib>LEE, HWA CHAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KIM, KWAN JE</au><au>LEE, HWA CHAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD</title><date>2013-06-26</date><risdate>2013</risdate><abstract>PURPOSE: A method for manufacturing an expanded perlite board is provided to achieve superior quality and to reduce time required for a plasticizing process by including a primary plasticizing process with microwaves. CONSTITUTION: A method for manufacturing an expanded perlite board includes the following steps of: mixing 2000 parts by weight of expanded perlite, 450-800 parts by weight of a low temperature binder, and water; molding the mixture with a press molding method; surface-treating the molded product, and applying coating liquid on the surface of the molded product; and completing a product by primarily plasticizing the molded product in a microwave plasticizing furnace and secondarily plasticizing the molded product in a high temperature plasticizing furnace. The low temperature binder is composed of 400-600 parts by weight of sodium silicate and 50-200 parts by weight of a stabilizer based on 2000 parts by weight of the expanded perlite. If a high temperature binder is used for the mixing process, 2000 parts by weight of the expanded perlite, 1,000-1,500 parts by weight of water, and 450-800 parts by weight of a glaze, which is the high temperature binder, are mixed. The molded product is carried by a conveyor carrying method in the completing process. [Reference numerals] (AA) Primary plasticize; (BB) Secondary plasticize; (S101) Mix; (S102) Shape; (S103) Surface treat and coat</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; kor |
recordid | cdi_epo_espacenet_KR20130068211A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY PERFORMING OPERATIONS REFRACTORIES SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER SLAG TRANSPORTING TREATMENT OF NATURAL STONE WORKING CEMENT, CLAY, OR STONE |
title | METHOD FOR MANUFACTURING EXPANDED PERLITE BOARD |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T23%3A34%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KIM,%20KWAN%20JE&rft.date=2013-06-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20130068211A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |