SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD

PURPOSE: A synthesizing method for cobalt oxide from waste hard metals and cobalt oxide manufactured by the method are provided to obtain high purity cobalt oxide having excellent dispersibility and crystalline and a particle size of 10-100 nano meters. CONSTITUTION: A synthesizing method for cobalt...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KIM, KYUNG JA, CHO, WOO SEOK, PEE, JAE HWAN
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KIM, KYUNG JA
CHO, WOO SEOK
PEE, JAE HWAN
description PURPOSE: A synthesizing method for cobalt oxide from waste hard metals and cobalt oxide manufactured by the method are provided to obtain high purity cobalt oxide having excellent dispersibility and crystalline and a particle size of 10-100 nano meters. CONSTITUTION: A synthesizing method for cobalt oxide from waste hard metals comprises the following steps: heating waste hard metals and zinc in a crucible at less than the boiling point of the zinc; volatilizing the zinc component by heating the waste hard metals and zinc at a specific temperature; pulverizing tungsten carbide-cobalt lump after cooling the crucible; acid processing the tungsten carbide-cobalt powder using phosphoric acid and removing remaining zinc(Zn); acid processing the tungsten carbide-cobalt powder using hydrochloric acid solution; dissolving cobalt (Co) in the hydrochloric acid solution; manufacturing Co(OH) by adding alkali solution to the hydrochloric acid solution until pH becomes 7-14; selectively separating Co(OH)2 by filtering and centrifuging the hydrochloric acid solution; dispersing Co(OH)2 into distilled water; adding hydrogen peroxide to the dispersed Co(OH)2; and heating the solution in which the hydrogen peroxide is added at 120-500 deg. Celsius.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20120084439A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20120084439A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20120084439A3</originalsourceid><addsrcrecordid>eNrjZMgOjvQL8XAN9ozy9HNX8HUN8fB3UfB3U3D2d3L0CVHwj_B0cVVwC_L3VQh3DA5xVXB29XX1C3F1UXB2DHICyTn6uaAq9nX0C3VzdA4JDQKqcopUAJoONZeHgTUtMac4lRdKczMou7mGOHvophbkx6cWFyQmp-allsR7BxkZGBoZGFiYmBhbOhoTpwoAcWk25w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD</title><source>esp@cenet</source><creator>KIM, KYUNG JA ; CHO, WOO SEOK ; PEE, JAE HWAN</creator><creatorcontrib>KIM, KYUNG JA ; CHO, WOO SEOK ; PEE, JAE HWAN</creatorcontrib><description>PURPOSE: A synthesizing method for cobalt oxide from waste hard metals and cobalt oxide manufactured by the method are provided to obtain high purity cobalt oxide having excellent dispersibility and crystalline and a particle size of 10-100 nano meters. CONSTITUTION: A synthesizing method for cobalt oxide from waste hard metals comprises the following steps: heating waste hard metals and zinc in a crucible at less than the boiling point of the zinc; volatilizing the zinc component by heating the waste hard metals and zinc at a specific temperature; pulverizing tungsten carbide-cobalt lump after cooling the crucible; acid processing the tungsten carbide-cobalt powder using phosphoric acid and removing remaining zinc(Zn); acid processing the tungsten carbide-cobalt powder using hydrochloric acid solution; dissolving cobalt (Co) in the hydrochloric acid solution; manufacturing Co(OH) by adding alkali solution to the hydrochloric acid solution until pH becomes 7-14; selectively separating Co(OH)2 by filtering and centrifuging the hydrochloric acid solution; dispersing Co(OH)2 into distilled water; adding hydrogen peroxide to the dispersed Co(OH)2; and heating the solution in which the hydrogen peroxide is added at 120-500 deg. Celsius.</description><language>eng ; kor</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; DISPOSAL OF SOLID WASTE ; INORGANIC CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; RECLAMATION OF CONTAMINED SOIL SOIL ; TRANSPORTING</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120730&amp;DB=EPODOC&amp;CC=KR&amp;NR=20120084439A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120730&amp;DB=EPODOC&amp;CC=KR&amp;NR=20120084439A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KIM, KYUNG JA</creatorcontrib><creatorcontrib>CHO, WOO SEOK</creatorcontrib><creatorcontrib>PEE, JAE HWAN</creatorcontrib><title>SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD</title><description>PURPOSE: A synthesizing method for cobalt oxide from waste hard metals and cobalt oxide manufactured by the method are provided to obtain high purity cobalt oxide having excellent dispersibility and crystalline and a particle size of 10-100 nano meters. CONSTITUTION: A synthesizing method for cobalt oxide from waste hard metals comprises the following steps: heating waste hard metals and zinc in a crucible at less than the boiling point of the zinc; volatilizing the zinc component by heating the waste hard metals and zinc at a specific temperature; pulverizing tungsten carbide-cobalt lump after cooling the crucible; acid processing the tungsten carbide-cobalt powder using phosphoric acid and removing remaining zinc(Zn); acid processing the tungsten carbide-cobalt powder using hydrochloric acid solution; dissolving cobalt (Co) in the hydrochloric acid solution; manufacturing Co(OH) by adding alkali solution to the hydrochloric acid solution until pH becomes 7-14; selectively separating Co(OH)2 by filtering and centrifuging the hydrochloric acid solution; dispersing Co(OH)2 into distilled water; adding hydrogen peroxide to the dispersed Co(OH)2; and heating the solution in which the hydrogen peroxide is added at 120-500 deg. Celsius.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>DISPOSAL OF SOLID WASTE</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>RECLAMATION OF CONTAMINED SOIL SOIL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZMgOjvQL8XAN9ozy9HNX8HUN8fB3UfB3U3D2d3L0CVHwj_B0cVVwC_L3VQh3DA5xVXB29XX1C3F1UXB2DHICyTn6uaAq9nX0C3VzdA4JDQKqcopUAJoONZeHgTUtMac4lRdKczMou7mGOHvophbkx6cWFyQmp-allsR7BxkZGBoZGFiYmBhbOhoTpwoAcWk25w</recordid><startdate>20120730</startdate><enddate>20120730</enddate><creator>KIM, KYUNG JA</creator><creator>CHO, WOO SEOK</creator><creator>PEE, JAE HWAN</creator><scope>EVB</scope></search><sort><creationdate>20120730</creationdate><title>SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD</title><author>KIM, KYUNG JA ; CHO, WOO SEOK ; PEE, JAE HWAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20120084439A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; kor</language><creationdate>2012</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>DISPOSAL OF SOLID WASTE</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>RECLAMATION OF CONTAMINED SOIL SOIL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KIM, KYUNG JA</creatorcontrib><creatorcontrib>CHO, WOO SEOK</creatorcontrib><creatorcontrib>PEE, JAE HWAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KIM, KYUNG JA</au><au>CHO, WOO SEOK</au><au>PEE, JAE HWAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD</title><date>2012-07-30</date><risdate>2012</risdate><abstract>PURPOSE: A synthesizing method for cobalt oxide from waste hard metals and cobalt oxide manufactured by the method are provided to obtain high purity cobalt oxide having excellent dispersibility and crystalline and a particle size of 10-100 nano meters. CONSTITUTION: A synthesizing method for cobalt oxide from waste hard metals comprises the following steps: heating waste hard metals and zinc in a crucible at less than the boiling point of the zinc; volatilizing the zinc component by heating the waste hard metals and zinc at a specific temperature; pulverizing tungsten carbide-cobalt lump after cooling the crucible; acid processing the tungsten carbide-cobalt powder using phosphoric acid and removing remaining zinc(Zn); acid processing the tungsten carbide-cobalt powder using hydrochloric acid solution; dissolving cobalt (Co) in the hydrochloric acid solution; manufacturing Co(OH) by adding alkali solution to the hydrochloric acid solution until pH becomes 7-14; selectively separating Co(OH)2 by filtering and centrifuging the hydrochloric acid solution; dispersing Co(OH)2 into distilled water; adding hydrogen peroxide to the dispersed Co(OH)2; and heating the solution in which the hydrogen peroxide is added at 120-500 deg. Celsius.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; kor
recordid cdi_epo_espacenet_KR20120084439A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
DISPOSAL OF SOLID WASTE
INORGANIC CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
RECLAMATION OF CONTAMINED SOIL SOIL
TRANSPORTING
title SYNTHESIZING METHOD OF COBALT OXIDE FROM WASTE CEMENTED CARBIDE AND COBALT OXIDE MANUFACTURED BY THE METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T06%3A29%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KIM,%20KYUNG%20JA&rft.date=2012-07-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20120084439A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true