MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS
A method for producing depressed index optical fibers is provided to obtain both advantages of a soot deposition process and those of a rod-in-tube process while needing no long processing time and preventing contamination of a preform. A method for producing depressed index optical fibers comprises...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WU FENGQING PECKHAM DAVID BARISH ERIC L LINGLE ROBERT JR |
description | A method for producing depressed index optical fibers is provided to obtain both advantages of a soot deposition process and those of a rod-in-tube process while needing no long processing time and preventing contamination of a preform. A method for producing depressed index optical fibers comprises the steps of: (a) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a first soot gas mixture in a first vapor axis deposition(VAD) torch, and (ii) forming a first soot flame to ignite the first soot glass mixture and to produce a first glass soot in a first vapor axis deposition(VAD) torch; (b) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a second soot gas mixture in a second vapor axis deposition torch, and (ii) forming a second soot flame to ignite the second soot glass mixture and to produce a second glass soot in a second vapor axis deposition torch; (c) depositing the first glass soot to allow the first VAD torch to form a first soot, and allowing the first VAD torch to precede the second VAD torch so that the second glass soot is deposited on the first glass soot, while optionally orienting a support bar to the first and second VAD torches; (d) moving the support bar to the torches from the starting point to the end point so as to form a double layer of soot; (g) heating the double layer of soot to cause the soot to be closely inserted into a glass bar; (h) inserting the glass bar into a glass pipe containing fluorine-doped glass; and (i) heating the glass pipe to collapse the glass pipe around the glass bar. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20070090747A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20070090747A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20070090747A3</originalsourceid><addsrcrecordid>eNrjZND1dfQLdXN0DgkNclXwd1NwcQ0Icg0OdnVR8PRzcY1Q8A8I8XR29FFw83RyDQrmYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXx3kFGBgbmBgaWBuYm5o7GxKkCAEvoJkY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS</title><source>esp@cenet</source><creator>WU FENGQING ; PECKHAM DAVID ; BARISH ERIC L ; LINGLE ROBERT JR</creator><creatorcontrib>WU FENGQING ; PECKHAM DAVID ; BARISH ERIC L ; LINGLE ROBERT JR</creatorcontrib><description>A method for producing depressed index optical fibers is provided to obtain both advantages of a soot deposition process and those of a rod-in-tube process while needing no long processing time and preventing contamination of a preform. A method for producing depressed index optical fibers comprises the steps of: (a) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a first soot gas mixture in a first vapor axis deposition(VAD) torch, and (ii) forming a first soot flame to ignite the first soot glass mixture and to produce a first glass soot in a first vapor axis deposition(VAD) torch; (b) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a second soot gas mixture in a second vapor axis deposition torch, and (ii) forming a second soot flame to ignite the second soot glass mixture and to produce a second glass soot in a second vapor axis deposition torch; (c) depositing the first glass soot to allow the first VAD torch to form a first soot, and allowing the first VAD torch to precede the second VAD torch so that the second glass soot is deposited on the first glass soot, while optionally orienting a support bar to the first and second VAD torches; (d) moving the support bar to the torches from the starting point to the end point so as to form a double layer of soot; (g) heating the double layer of soot to cause the soot to be closely inserted into a glass bar; (h) inserting the glass bar into a glass pipe containing fluorine-doped glass; and (i) heating the glass pipe to collapse the glass pipe around the glass bar.</description><language>eng</language><subject>CHEMISTRY ; GLASS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20070906&DB=EPODOC&CC=KR&NR=20070090747A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20070906&DB=EPODOC&CC=KR&NR=20070090747A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WU FENGQING</creatorcontrib><creatorcontrib>PECKHAM DAVID</creatorcontrib><creatorcontrib>BARISH ERIC L</creatorcontrib><creatorcontrib>LINGLE ROBERT JR</creatorcontrib><title>MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS</title><description>A method for producing depressed index optical fibers is provided to obtain both advantages of a soot deposition process and those of a rod-in-tube process while needing no long processing time and preventing contamination of a preform. A method for producing depressed index optical fibers comprises the steps of: (a) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a first soot gas mixture in a first vapor axis deposition(VAD) torch, and (ii) forming a first soot flame to ignite the first soot glass mixture and to produce a first glass soot in a first vapor axis deposition(VAD) torch; (b) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a second soot gas mixture in a second vapor axis deposition torch, and (ii) forming a second soot flame to ignite the second soot glass mixture and to produce a second glass soot in a second vapor axis deposition torch; (c) depositing the first glass soot to allow the first VAD torch to form a first soot, and allowing the first VAD torch to precede the second VAD torch so that the second glass soot is deposited on the first glass soot, while optionally orienting a support bar to the first and second VAD torches; (d) moving the support bar to the torches from the starting point to the end point so as to form a double layer of soot; (g) heating the double layer of soot to cause the soot to be closely inserted into a glass bar; (h) inserting the glass bar into a glass pipe containing fluorine-doped glass; and (i) heating the glass pipe to collapse the glass pipe around the glass bar.</description><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND1dfQLdXN0DgkNclXwd1NwcQ0Icg0OdnVR8PRzcY1Q8A8I8XR29FFw83RyDQrmYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXx3kFGBgbmBgaWBuYm5o7GxKkCAEvoJkY</recordid><startdate>20070906</startdate><enddate>20070906</enddate><creator>WU FENGQING</creator><creator>PECKHAM DAVID</creator><creator>BARISH ERIC L</creator><creator>LINGLE ROBERT JR</creator><scope>EVB</scope></search><sort><creationdate>20070906</creationdate><title>MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS</title><author>WU FENGQING ; PECKHAM DAVID ; BARISH ERIC L ; LINGLE ROBERT JR</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20070090747A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><toplevel>online_resources</toplevel><creatorcontrib>WU FENGQING</creatorcontrib><creatorcontrib>PECKHAM DAVID</creatorcontrib><creatorcontrib>BARISH ERIC L</creatorcontrib><creatorcontrib>LINGLE ROBERT JR</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WU FENGQING</au><au>PECKHAM DAVID</au><au>BARISH ERIC L</au><au>LINGLE ROBERT JR</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS</title><date>2007-09-06</date><risdate>2007</risdate><abstract>A method for producing depressed index optical fibers is provided to obtain both advantages of a soot deposition process and those of a rod-in-tube process while needing no long processing time and preventing contamination of a preform. A method for producing depressed index optical fibers comprises the steps of: (a) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a first soot gas mixture in a first vapor axis deposition(VAD) torch, and (ii) forming a first soot flame to ignite the first soot glass mixture and to produce a first glass soot in a first vapor axis deposition(VAD) torch; (b) causing at least one free precursor gas flow and fuel gas flow to flow together with to form a second soot gas mixture in a second vapor axis deposition torch, and (ii) forming a second soot flame to ignite the second soot glass mixture and to produce a second glass soot in a second vapor axis deposition torch; (c) depositing the first glass soot to allow the first VAD torch to form a first soot, and allowing the first VAD torch to precede the second VAD torch so that the second glass soot is deposited on the first glass soot, while optionally orienting a support bar to the first and second VAD torches; (d) moving the support bar to the torches from the starting point to the end point so as to form a double layer of soot; (g) heating the double layer of soot to cause the soot to be closely inserted into a glass bar; (h) inserting the glass bar into a glass pipe containing fluorine-doped glass; and (i) heating the glass pipe to collapse the glass pipe around the glass bar.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_KR20070090747A |
source | esp@cenet |
subjects | CHEMISTRY GLASS MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES METALLURGY MINERAL OR SLAG WOOL |
title | MANUFACTURE OF DEPRESSED INDEX OPTICAL FIBERS |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T22%3A00%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WU%20FENGQING&rft.date=2007-09-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20070090747A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |