METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING

A process of manufacturing a coated glass with improved anti-fogging property is provided to produce the glass having expression of transition metal oxides by UV ray and improved anti-fogging property by fabricating a coating layer with transition metal oxides such as titanium dioxide, zinc oxide, t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: PARK, HYUN DAL
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PARK, HYUN DAL
description A process of manufacturing a coated glass with improved anti-fogging property is provided to produce the glass having expression of transition metal oxides by UV ray and improved anti-fogging property by fabricating a coating layer with transition metal oxides such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating mode and applying silica solution to the coating layer. The process comprises the steps of: preparing a coating layer from transition metal oxide such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating way; and applying a silica solution to the coating layer by any one selected from flow coating, spin coating and dip coating to form the resulting coating layer. The process further includes addition of pore generating agent to the silica solution to form the porous silica layer. The process includes additional step of heat treating the silica layer under oxidation atmosphere at 100 to 350deg.C for 30 minutes to 2 hours to enhance adhesion between the silica layer and the transition metal oxide layer.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20070013712A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20070013712A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20070013712A3</originalsourceid><addsrcrecordid>eNrjZHDydQ3x8HdRcPMPUvB19At1c3QOCQ1yVfB3U3D2dwzx9HNXcPdxDA5WCPcM8VDw9A0I8g9zdVFw9Avx1HXzd3cHKuBhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfHeQUYGBuYGBobG5oZGjsbEqQIAnaMr5g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING</title><source>esp@cenet</source><creator>PARK, HYUN DAL</creator><creatorcontrib>PARK, HYUN DAL</creatorcontrib><description>A process of manufacturing a coated glass with improved anti-fogging property is provided to produce the glass having expression of transition metal oxides by UV ray and improved anti-fogging property by fabricating a coating layer with transition metal oxides such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating mode and applying silica solution to the coating layer. The process comprises the steps of: preparing a coating layer from transition metal oxide such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating way; and applying a silica solution to the coating layer by any one selected from flow coating, spin coating and dip coating to form the resulting coating layer. The process further includes addition of pore generating agent to the silica solution to form the porous silica layer. The process includes additional step of heat treating the silica layer under oxidation atmosphere at 100 to 350deg.C for 30 minutes to 2 hours to enhance adhesion between the silica layer and the transition metal oxide layer.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070131&amp;DB=EPODOC&amp;CC=KR&amp;NR=20070013712A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070131&amp;DB=EPODOC&amp;CC=KR&amp;NR=20070013712A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PARK, HYUN DAL</creatorcontrib><title>METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING</title><description>A process of manufacturing a coated glass with improved anti-fogging property is provided to produce the glass having expression of transition metal oxides by UV ray and improved anti-fogging property by fabricating a coating layer with transition metal oxides such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating mode and applying silica solution to the coating layer. The process comprises the steps of: preparing a coating layer from transition metal oxide such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating way; and applying a silica solution to the coating layer by any one selected from flow coating, spin coating and dip coating to form the resulting coating layer. The process further includes addition of pore generating agent to the silica solution to form the porous silica layer. The process includes additional step of heat treating the silica layer under oxidation atmosphere at 100 to 350deg.C for 30 minutes to 2 hours to enhance adhesion between the silica layer and the transition metal oxide layer.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDydQ3x8HdRcPMPUvB19At1c3QOCQ1yVfB3U3D2dwzx9HNXcPdxDA5WCPcM8VDw9A0I8g9zdVFw9Avx1HXzd3cHKuBhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfHeQUYGBuYGBobG5oZGjsbEqQIAnaMr5g</recordid><startdate>20070131</startdate><enddate>20070131</enddate><creator>PARK, HYUN DAL</creator><scope>EVB</scope></search><sort><creationdate>20070131</creationdate><title>METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING</title><author>PARK, HYUN DAL</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20070013712A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>PARK, HYUN DAL</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PARK, HYUN DAL</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING</title><date>2007-01-31</date><risdate>2007</risdate><abstract>A process of manufacturing a coated glass with improved anti-fogging property is provided to produce the glass having expression of transition metal oxides by UV ray and improved anti-fogging property by fabricating a coating layer with transition metal oxides such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating mode and applying silica solution to the coating layer. The process comprises the steps of: preparing a coating layer from transition metal oxide such as titanium dioxide, zinc oxide, tin dioxide through vacuum coating way; and applying a silica solution to the coating layer by any one selected from flow coating, spin coating and dip coating to form the resulting coating layer. The process further includes addition of pore generating agent to the silica solution to form the porous silica layer. The process includes additional step of heat treating the silica layer under oxidation atmosphere at 100 to 350deg.C for 30 minutes to 2 hours to enhance adhesion between the silica layer and the transition metal oxide layer.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_KR20070013712A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR MANUFACTURE OF COATING GLASS WITH IMPROVED ANTI-FOGGING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T18%3A03%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PARK,%20HYUN%20DAL&rft.date=2007-01-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20070013712A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true