MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME

A method for manufacturing a porous polyketone membrane according to the present invention comprises the steps of: mixing polyketone and a diluent at a temperature of 190-270°C to manufacture a dope solution; applying the manufactured dope solution on a support, rapidly solidifying the solution usin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JOO SUNGWOOK, MUN JIHUN, SUNGIL JEON, HONG SANGHWUI, CHAE JIHUN, HOU JIAN, BYUN KWANGHYUN
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JOO SUNGWOOK
MUN JIHUN
SUNGIL JEON
HONG SANGHWUI
CHAE JIHUN
HOU JIAN
BYUN KWANGHYUN
description A method for manufacturing a porous polyketone membrane according to the present invention comprises the steps of: mixing polyketone and a diluent at a temperature of 190-270°C to manufacture a dope solution; applying the manufactured dope solution on a support, rapidly solidifying the solution using an aqueous coolant containing at least one selected from a group consisting of water and an organic solvent at 4-70°C, and manufacturing a porous polyketone membrane by a heat-induced separation method; and extracting and removing the diluent from the porous membrane. According to the present invention, a porous polyketone membrane excellent in chemical resistance and heat resistance can be manufactured. 본 발명에 따른 폴리케톤 다공성막의 제조방법은 폴리케톤 및 희석제를 190 내지 270℃의 온도에서 혼합하여 도프(dope) 용액을 제조하는 단계; 제조된 상기 도프 용액을 지지체 상에 도포하고 4 내지 70℃의, 물 및 유기용매로 이루어진 군에서 선택되는 1 이상을 포함하는 수성 냉매를 이용하여 급속 고형화하여 열유도상분리법으로 폴리케톤 다공성막을 제조하는 단계; 및 상기 다공성막으로부터 희석제를 추출하여 제거하는 단계;를 포함하는 것을 특징으로 한다.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR101984059BB1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR101984059BB1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR101984059BB13</originalsourceid><addsrcrecordid>eNrjZJjo6-gX6uboHBIa5OnnruDrGuLh76Lg76YQ4O8T6e0a4u_nCmQG-YcGA-V8nYIcwXycUo5-LsjSbj6OIQrBHq6uIQohkQGuCHUIW11dFEKDQVaHeLgqBDv6uvIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUknjvIEMDQ0sLEwNTSycnQ2PiVAEAEmlCdA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME</title><source>esp@cenet</source><creator>JOO SUNGWOOK ; MUN JIHUN ; SUNGIL JEON ; HONG SANGHWUI ; CHAE JIHUN ; HOU JIAN ; BYUN KWANGHYUN</creator><creatorcontrib>JOO SUNGWOOK ; MUN JIHUN ; SUNGIL JEON ; HONG SANGHWUI ; CHAE JIHUN ; HOU JIAN ; BYUN KWANGHYUN</creatorcontrib><description>A method for manufacturing a porous polyketone membrane according to the present invention comprises the steps of: mixing polyketone and a diluent at a temperature of 190-270°C to manufacture a dope solution; applying the manufactured dope solution on a support, rapidly solidifying the solution using an aqueous coolant containing at least one selected from a group consisting of water and an organic solvent at 4-70°C, and manufacturing a porous polyketone membrane by a heat-induced separation method; and extracting and removing the diluent from the porous membrane. According to the present invention, a porous polyketone membrane excellent in chemical resistance and heat resistance can be manufactured. 본 발명에 따른 폴리케톤 다공성막의 제조방법은 폴리케톤 및 희석제를 190 내지 270℃의 온도에서 혼합하여 도프(dope) 용액을 제조하는 단계; 제조된 상기 도프 용액을 지지체 상에 도포하고 4 내지 70℃의, 물 및 유기용매로 이루어진 군에서 선택되는 1 이상을 포함하는 수성 냉매를 이용하여 급속 고형화하여 열유도상분리법으로 폴리케톤 다공성막을 제조하는 단계; 및 상기 다공성막으로부터 희석제를 추출하여 제거하는 단계;를 포함하는 것을 특징으로 한다.</description><language>eng ; kor</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; GENERAL PROCESSES OF COMPOUNDING ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; SEPARATION ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING-UP</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190530&amp;DB=EPODOC&amp;CC=KR&amp;NR=101984059B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190530&amp;DB=EPODOC&amp;CC=KR&amp;NR=101984059B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JOO SUNGWOOK</creatorcontrib><creatorcontrib>MUN JIHUN</creatorcontrib><creatorcontrib>SUNGIL JEON</creatorcontrib><creatorcontrib>HONG SANGHWUI</creatorcontrib><creatorcontrib>CHAE JIHUN</creatorcontrib><creatorcontrib>HOU JIAN</creatorcontrib><creatorcontrib>BYUN KWANGHYUN</creatorcontrib><title>MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME</title><description>A method for manufacturing a porous polyketone membrane according to the present invention comprises the steps of: mixing polyketone and a diluent at a temperature of 190-270°C to manufacture a dope solution; applying the manufactured dope solution on a support, rapidly solidifying the solution using an aqueous coolant containing at least one selected from a group consisting of water and an organic solvent at 4-70°C, and manufacturing a porous polyketone membrane by a heat-induced separation method; and extracting and removing the diluent from the porous membrane. According to the present invention, a porous polyketone membrane excellent in chemical resistance and heat resistance can be manufactured. 본 발명에 따른 폴리케톤 다공성막의 제조방법은 폴리케톤 및 희석제를 190 내지 270℃의 온도에서 혼합하여 도프(dope) 용액을 제조하는 단계; 제조된 상기 도프 용액을 지지체 상에 도포하고 4 내지 70℃의, 물 및 유기용매로 이루어진 군에서 선택되는 1 이상을 포함하는 수성 냉매를 이용하여 급속 고형화하여 열유도상분리법으로 폴리케톤 다공성막을 제조하는 단계; 및 상기 다공성막으로부터 희석제를 추출하여 제거하는 단계;를 포함하는 것을 특징으로 한다.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>SEPARATION</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJjo6-gX6uboHBIa5OnnruDrGuLh76Lg76YQ4O8T6e0a4u_nCmQG-YcGA-V8nYIcwXycUo5-LsjSbj6OIQrBHq6uIQohkQGuCHUIW11dFEKDQVaHeLgqBDv6uvIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUknjvIEMDQ0sLEwNTSycnQ2PiVAEAEmlCdA</recordid><startdate>20190530</startdate><enddate>20190530</enddate><creator>JOO SUNGWOOK</creator><creator>MUN JIHUN</creator><creator>SUNGIL JEON</creator><creator>HONG SANGHWUI</creator><creator>CHAE JIHUN</creator><creator>HOU JIAN</creator><creator>BYUN KWANGHYUN</creator><scope>EVB</scope></search><sort><creationdate>20190530</creationdate><title>MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME</title><author>JOO SUNGWOOK ; MUN JIHUN ; SUNGIL JEON ; HONG SANGHWUI ; CHAE JIHUN ; HOU JIAN ; BYUN KWANGHYUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR101984059BB13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; kor</language><creationdate>2019</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>SEPARATION</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>JOO SUNGWOOK</creatorcontrib><creatorcontrib>MUN JIHUN</creatorcontrib><creatorcontrib>SUNGIL JEON</creatorcontrib><creatorcontrib>HONG SANGHWUI</creatorcontrib><creatorcontrib>CHAE JIHUN</creatorcontrib><creatorcontrib>HOU JIAN</creatorcontrib><creatorcontrib>BYUN KWANGHYUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JOO SUNGWOOK</au><au>MUN JIHUN</au><au>SUNGIL JEON</au><au>HONG SANGHWUI</au><au>CHAE JIHUN</au><au>HOU JIAN</au><au>BYUN KWANGHYUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME</title><date>2019-05-30</date><risdate>2019</risdate><abstract>A method for manufacturing a porous polyketone membrane according to the present invention comprises the steps of: mixing polyketone and a diluent at a temperature of 190-270°C to manufacture a dope solution; applying the manufactured dope solution on a support, rapidly solidifying the solution using an aqueous coolant containing at least one selected from a group consisting of water and an organic solvent at 4-70°C, and manufacturing a porous polyketone membrane by a heat-induced separation method; and extracting and removing the diluent from the porous membrane. According to the present invention, a porous polyketone membrane excellent in chemical resistance and heat resistance can be manufactured. 본 발명에 따른 폴리케톤 다공성막의 제조방법은 폴리케톤 및 희석제를 190 내지 270℃의 온도에서 혼합하여 도프(dope) 용액을 제조하는 단계; 제조된 상기 도프 용액을 지지체 상에 도포하고 4 내지 70℃의, 물 및 유기용매로 이루어진 군에서 선택되는 1 이상을 포함하는 수성 냉매를 이용하여 급속 고형화하여 열유도상분리법으로 폴리케톤 다공성막을 제조하는 단계; 및 상기 다공성막으로부터 희석제를 추출하여 제거하는 단계;를 포함하는 것을 특징으로 한다.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; kor
recordid cdi_epo_espacenet_KR101984059BB1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
GENERAL PROCESSES OF COMPOUNDING
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
SEPARATION
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING-UP
title MANUFACTURING METHOD OF POLYKETONE POROUS MEMBRANE POLYKETONE POROUS MEMBRANE AND POLYKETONE FLAT SHEET TYPE MEMBRANE MANUFACTURED USING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-10T03%3A19%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JOO%20SUNGWOOK&rft.date=2019-05-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR101984059BB1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true