ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT
PURPOSE:To obtain the title adhesive which has a higher CT value to facilitate the detection of joining accuracy by non-destructive inspection to thereby enable bonding with highest possible accuracy, by incorporating BaCO3 or BaSO4 into an adhesive. CONSTITUTION:10-50wt.% BaCO3 or BaSO4 is incorpor...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OHASHI HIDEKI MARUOKA MINEO |
description | PURPOSE:To obtain the title adhesive which has a higher CT value to facilitate the detection of joining accuracy by non-destructive inspection to thereby enable bonding with highest possible accuracy, by incorporating BaCO3 or BaSO4 into an adhesive. CONSTITUTION:10-50wt.% BaCO3 or BaSO4 is incorporated into an adhesive for an advanced composite material joint, used for joining of advanced compos ite material such as CFRP. The incorporation thereof gives an adhesive with a high CT value to enable the non-destructive inspection of the defects of an adhesive layer by the X-ray CT so that bonding with highest possible accuracy can be realized, thus improving the reliability. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS63215783A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS63215783A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS63215783A3</originalsourceid><addsrcrecordid>eNrjZNBzdPFwDfYMc1Vw8w9ScHQJc_RzdnVRcPb3DfAP9gxxVfB1DHEN8nT0UfDy9_QL4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWbGRoam5hbGjsbEqAEA36gl_w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT</title><source>esp@cenet</source><creator>OHASHI HIDEKI ; MARUOKA MINEO</creator><creatorcontrib>OHASHI HIDEKI ; MARUOKA MINEO</creatorcontrib><description>PURPOSE:To obtain the title adhesive which has a higher CT value to facilitate the detection of joining accuracy by non-destructive inspection to thereby enable bonding with highest possible accuracy, by incorporating BaCO3 or BaSO4 into an adhesive. CONSTITUTION:10-50wt.% BaCO3 or BaSO4 is incorporated into an adhesive for an advanced composite material joint, used for joining of advanced compos ite material such as CFRP. The incorporation thereof gives an adhesive with a high CT value to enable the non-destructive inspection of the defects of an adhesive layer by the X-ray CT so that bonding with highest possible accuracy can be realized, thus improving the reliability.</description><language>eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DYES ; GENERAL PROCESSES OF COMPOUNDING ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS AS ADHESIVES ; WORKING-UP</subject><creationdate>1988</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19880908&DB=EPODOC&CC=JP&NR=S63215783A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19880908&DB=EPODOC&CC=JP&NR=S63215783A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OHASHI HIDEKI</creatorcontrib><creatorcontrib>MARUOKA MINEO</creatorcontrib><title>ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT</title><description>PURPOSE:To obtain the title adhesive which has a higher CT value to facilitate the detection of joining accuracy by non-destructive inspection to thereby enable bonding with highest possible accuracy, by incorporating BaCO3 or BaSO4 into an adhesive. CONSTITUTION:10-50wt.% BaCO3 or BaSO4 is incorporated into an adhesive for an advanced composite material joint, used for joining of advanced compos ite material such as CFRP. The incorporation thereof gives an adhesive with a high CT value to enable the non-destructive inspection of the defects of an adhesive layer by the X-ray CT so that bonding with highest possible accuracy can be realized, thus improving the reliability.</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DYES</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1988</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNBzdPFwDfYMc1Vw8w9ScHQJc_RzdnVRcPb3DfAP9gxxVfB1DHEN8nT0UfDy9_QL4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWbGRoam5hbGjsbEqAEA36gl_w</recordid><startdate>19880908</startdate><enddate>19880908</enddate><creator>OHASHI HIDEKI</creator><creator>MARUOKA MINEO</creator><scope>EVB</scope></search><sort><creationdate>19880908</creationdate><title>ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT</title><author>OHASHI HIDEKI ; MARUOKA MINEO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS63215783A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1988</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DYES</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>OHASHI HIDEKI</creatorcontrib><creatorcontrib>MARUOKA MINEO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OHASHI HIDEKI</au><au>MARUOKA MINEO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT</title><date>1988-09-08</date><risdate>1988</risdate><abstract>PURPOSE:To obtain the title adhesive which has a higher CT value to facilitate the detection of joining accuracy by non-destructive inspection to thereby enable bonding with highest possible accuracy, by incorporating BaCO3 or BaSO4 into an adhesive. CONSTITUTION:10-50wt.% BaCO3 or BaSO4 is incorporated into an adhesive for an advanced composite material joint, used for joining of advanced compos ite material such as CFRP. The incorporation thereof gives an adhesive with a high CT value to enable the non-destructive inspection of the defects of an adhesive layer by the X-ray CT so that bonding with highest possible accuracy can be realized, thus improving the reliability.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JPS63215783A |
source | esp@cenet |
subjects | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G CHEMISTRY COMPOSITIONS BASED THEREON DYES GENERAL PROCESSES OF COMPOUNDING METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ORGANIC MACROMOLECULAR COMPOUNDS PAINTS POLISHES THEIR PREPARATION OR CHEMICAL WORKING-UP USE OF MATERIALS AS ADHESIVES WORKING-UP |
title | ADHESIVE FOR ADVANCED COMPOSITE MATERIAL JOINT |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T10%3A28%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OHASHI%20HIDEKI&rft.date=1988-09-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS63215783A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |