PRODUCTION OF MODIFIED POLYESTER YARN

PURPOSE:To obtain the titled yarn of basic dyeable type having high strength, excellent alkali resistance, dyeability and fastness to light of dyed material, by spinning a specific modified polyester under a specific condition and drawing. CONSTITUTION:A modified polyester which is obtained by copol...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATSUMOTO TADAYUKI, MITSUYOSHI TAKEHIKO, SANO KEIZO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MATSUMOTO TADAYUKI
MITSUYOSHI TAKEHIKO
SANO KEIZO
description PURPOSE:To obtain the titled yarn of basic dyeable type having high strength, excellent alkali resistance, dyeability and fastness to light of dyed material, by spinning a specific modified polyester under a specific condition and drawing. CONSTITUTION:A modified polyester which is obtained by copolymerization of an isophthalic acid component containing 1.0-2.0mol% sulfonate group and 0.5-1.9wt% glycol component preferably polyalkylene glycol shown by formula A(CnH2nO)m [A is ClH2l+1O or OH (l is 1-10); n is 2-5; m is 3-100] having 400-6,000mol.wt. and has 82-105 polymerization degree is spun under conditions wherein shear rate (gamma)
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS63120111A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS63120111A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS63120111A3</originalsourceid><addsrcrecordid>eNrjZFANCPJ3CXUO8fT3U_B3U_D1d_F083R1UQjw94l0DQ5xDVKIdAzy42FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWbGhkYGhoaGjsbEqAEAtx4joA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION OF MODIFIED POLYESTER YARN</title><source>esp@cenet</source><creator>MATSUMOTO TADAYUKI ; MITSUYOSHI TAKEHIKO ; SANO KEIZO</creator><creatorcontrib>MATSUMOTO TADAYUKI ; MITSUYOSHI TAKEHIKO ; SANO KEIZO</creatorcontrib><description>PURPOSE:To obtain the titled yarn of basic dyeable type having high strength, excellent alkali resistance, dyeability and fastness to light of dyed material, by spinning a specific modified polyester under a specific condition and drawing. CONSTITUTION:A modified polyester which is obtained by copolymerization of an isophthalic acid component containing 1.0-2.0mol% sulfonate group and 0.5-1.9wt% glycol component preferably polyalkylene glycol shown by formula A(CnH2nO)m [A is ClH2l+1O or OH (l is 1-10); n is 2-5; m is 3-100] having 400-6,000mol.wt. and has 82-105 polymerization degree is spun under conditions wherein shear rate (gamma)&lt;=10 sec&lt;-1&gt;, draft &lt;=250, back pressure of spinneret (rho)&gt;=40kg/cm and shear stress (tau)&lt;=(Q+0.7)X10 dyne/cm (Q is delivery amount g/min per single hole) and drawn to give the aimed yarn.</description><language>eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>1988</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19880524&amp;DB=EPODOC&amp;CC=JP&amp;NR=S63120111A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19880524&amp;DB=EPODOC&amp;CC=JP&amp;NR=S63120111A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MATSUMOTO TADAYUKI</creatorcontrib><creatorcontrib>MITSUYOSHI TAKEHIKO</creatorcontrib><creatorcontrib>SANO KEIZO</creatorcontrib><title>PRODUCTION OF MODIFIED POLYESTER YARN</title><description>PURPOSE:To obtain the titled yarn of basic dyeable type having high strength, excellent alkali resistance, dyeability and fastness to light of dyed material, by spinning a specific modified polyester under a specific condition and drawing. CONSTITUTION:A modified polyester which is obtained by copolymerization of an isophthalic acid component containing 1.0-2.0mol% sulfonate group and 0.5-1.9wt% glycol component preferably polyalkylene glycol shown by formula A(CnH2nO)m [A is ClH2l+1O or OH (l is 1-10); n is 2-5; m is 3-100] having 400-6,000mol.wt. and has 82-105 polymerization degree is spun under conditions wherein shear rate (gamma)&lt;=10 sec&lt;-1&gt;, draft &lt;=250, back pressure of spinneret (rho)&gt;=40kg/cm and shear stress (tau)&lt;=(Q+0.7)X10 dyne/cm (Q is delivery amount g/min per single hole) and drawn to give the aimed yarn.</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1988</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFANCPJ3CXUO8fT3U_B3U_D1d_F083R1UQjw94l0DQ5xDVKIdAzy42FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWbGhkYGhoaGjsbEqAEAtx4joA</recordid><startdate>19880524</startdate><enddate>19880524</enddate><creator>MATSUMOTO TADAYUKI</creator><creator>MITSUYOSHI TAKEHIKO</creator><creator>SANO KEIZO</creator><scope>EVB</scope></search><sort><creationdate>19880524</creationdate><title>PRODUCTION OF MODIFIED POLYESTER YARN</title><author>MATSUMOTO TADAYUKI ; MITSUYOSHI TAKEHIKO ; SANO KEIZO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS63120111A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1988</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>MATSUMOTO TADAYUKI</creatorcontrib><creatorcontrib>MITSUYOSHI TAKEHIKO</creatorcontrib><creatorcontrib>SANO KEIZO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MATSUMOTO TADAYUKI</au><au>MITSUYOSHI TAKEHIKO</au><au>SANO KEIZO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION OF MODIFIED POLYESTER YARN</title><date>1988-05-24</date><risdate>1988</risdate><abstract>PURPOSE:To obtain the titled yarn of basic dyeable type having high strength, excellent alkali resistance, dyeability and fastness to light of dyed material, by spinning a specific modified polyester under a specific condition and drawing. CONSTITUTION:A modified polyester which is obtained by copolymerization of an isophthalic acid component containing 1.0-2.0mol% sulfonate group and 0.5-1.9wt% glycol component preferably polyalkylene glycol shown by formula A(CnH2nO)m [A is ClH2l+1O or OH (l is 1-10); n is 2-5; m is 3-100] having 400-6,000mol.wt. and has 82-105 polymerization degree is spun under conditions wherein shear rate (gamma)&lt;=10 sec&lt;-1&gt;, draft &lt;=250, back pressure of spinneret (rho)&gt;=40kg/cm and shear stress (tau)&lt;=(Q+0.7)X10 dyne/cm (Q is delivery amount g/min per single hole) and drawn to give the aimed yarn.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS63120111A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title PRODUCTION OF MODIFIED POLYESTER YARN
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T21%3A37%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MATSUMOTO%20TADAYUKI&rft.date=1988-05-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS63120111A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true