PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY
PURPOSE:To reduce the rate of breaking of a mild steel wire rod and to always keep the electrical conductivity at more than a specified value by using C and Mn for regulating the strength, adjusting the composition to obtain the specified value of the electrical conductivity (calculated value) and l...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KATO YOSHIO OBARA SHIGEO |
description | PURPOSE:To reduce the rate of breaking of a mild steel wire rod and to always keep the electrical conductivity at more than a specified value by using C and Mn for regulating the strength, adjusting the composition to obtain the specified value of the electrical conductivity (calculated value) and limiting the cooling rate after winding. CONSTITUTION:Low-C steel consisting of |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS6256520A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS6256520A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS6256520A3</originalsourceid><addsrcrecordid>eNqNjDEKwkAQANNYiPqH_YAgkaRf9zZmZb0LlzNRmxDkrEQD8f8YxAdYTTHDzJNr5Z05URBnwRVwFDVQB2aFVjzDJKHERuwe-EysyjaA8djiTlTCBdAaYGUKXggVyNnvrZncMpnd-8cYVz8uEig4ULmOw6uL49Df4jO-u0NV52mWZ-kGt38kHwRVMdM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY</title><source>esp@cenet</source><creator>KATO YOSHIO ; OBARA SHIGEO</creator><creatorcontrib>KATO YOSHIO ; OBARA SHIGEO</creatorcontrib><description><![CDATA[PURPOSE:To reduce the rate of breaking of a mild steel wire rod and to always keep the electrical conductivity at more than a specified value by using C and Mn for regulating the strength, adjusting the composition to obtain the specified value of the electrical conductivity (calculated value) and limiting the cooling rate after winding. CONSTITUTION:Low-C steel consisting of <=0.15% C, <=0.03% Si, <=0.40% Mn, <=0.025% P, <=0.025% S, <=0.05% Cu, <=0.05% Ni, <=0.10% Cr, <=0.080% sol Al, <=40ppm N, the balance iron and inevitable impurities and having the electrical conductivity, rhoeq, satisfying the following equation is used; rhoeq (calculated value) (=13.3Si+6.66Mn+16.66P+10S+2.85Cu+2.5Ni+5Cr+11.2 sol Al)<=4.0. The steel having the composition is hot-rolled, then wound at 750-950 deg.C and cooled after winding at the cooling rate of 2-7 deg.C/sec. A steel wire having excellent drawability and conductivity can be obtained by this method.]]></description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1987</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19870312&DB=EPODOC&CC=JP&NR=S6256520A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19870312&DB=EPODOC&CC=JP&NR=S6256520A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KATO YOSHIO</creatorcontrib><creatorcontrib>OBARA SHIGEO</creatorcontrib><title>PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY</title><description><![CDATA[PURPOSE:To reduce the rate of breaking of a mild steel wire rod and to always keep the electrical conductivity at more than a specified value by using C and Mn for regulating the strength, adjusting the composition to obtain the specified value of the electrical conductivity (calculated value) and limiting the cooling rate after winding. CONSTITUTION:Low-C steel consisting of <=0.15% C, <=0.03% Si, <=0.40% Mn, <=0.025% P, <=0.025% S, <=0.05% Cu, <=0.05% Ni, <=0.10% Cr, <=0.080% sol Al, <=40ppm N, the balance iron and inevitable impurities and having the electrical conductivity, rhoeq, satisfying the following equation is used; rhoeq (calculated value) (=13.3Si+6.66Mn+16.66P+10S+2.85Cu+2.5Ni+5Cr+11.2 sol Al)<=4.0. The steel having the composition is hot-rolled, then wound at 750-950 deg.C and cooled after winding at the cooling rate of 2-7 deg.C/sec. A steel wire having excellent drawability and conductivity can be obtained by this method.]]></description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1987</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEKwkAQANNYiPqH_YAgkaRf9zZmZb0LlzNRmxDkrEQD8f8YxAdYTTHDzJNr5Z05URBnwRVwFDVQB2aFVjzDJKHERuwe-EysyjaA8djiTlTCBdAaYGUKXggVyNnvrZncMpnd-8cYVz8uEig4ULmOw6uL49Df4jO-u0NV52mWZ-kGt38kHwRVMdM</recordid><startdate>19870312</startdate><enddate>19870312</enddate><creator>KATO YOSHIO</creator><creator>OBARA SHIGEO</creator><scope>EVB</scope></search><sort><creationdate>19870312</creationdate><title>PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY</title><author>KATO YOSHIO ; OBARA SHIGEO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS6256520A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1987</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KATO YOSHIO</creatorcontrib><creatorcontrib>OBARA SHIGEO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KATO YOSHIO</au><au>OBARA SHIGEO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY</title><date>1987-03-12</date><risdate>1987</risdate><abstract><![CDATA[PURPOSE:To reduce the rate of breaking of a mild steel wire rod and to always keep the electrical conductivity at more than a specified value by using C and Mn for regulating the strength, adjusting the composition to obtain the specified value of the electrical conductivity (calculated value) and limiting the cooling rate after winding. CONSTITUTION:Low-C steel consisting of <=0.15% C, <=0.03% Si, <=0.40% Mn, <=0.025% P, <=0.025% S, <=0.05% Cu, <=0.05% Ni, <=0.10% Cr, <=0.080% sol Al, <=40ppm N, the balance iron and inevitable impurities and having the electrical conductivity, rhoeq, satisfying the following equation is used; rhoeq (calculated value) (=13.3Si+6.66Mn+16.66P+10S+2.85Cu+2.5Ni+5Cr+11.2 sol Al)<=4.0. The steel having the composition is hot-rolled, then wound at 750-950 deg.C and cooled after winding at the cooling rate of 2-7 deg.C/sec. A steel wire having excellent drawability and conductivity can be obtained by this method.]]></abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JPS6256520A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | PRODUCTION OF MILD STEEL WIRE ROD HAVING EXCELLENT DRAWABILITY AND ELECTRICAL CONDUCTIVITY |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T04%3A05%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KATO%20YOSHIO&rft.date=1987-03-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS6256520A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |