REDUCING METHOD FOR CHROMIUM ORE

PURPOSE:To reduce chromium ore at a low cost and high degree by adding a binder to a pulverized powder mixture composed of the chromium ore and carbonaceous reducing agent, molding the mixture to a lump shape, forming a protective film on the surface and subjecting the molding to a heating treatment...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MINAGAWA TSUTOMU, UEMURA TADASHI, SASABE KIICHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MINAGAWA TSUTOMU
UEMURA TADASHI
SASABE KIICHIRO
description PURPOSE:To reduce chromium ore at a low cost and high degree by adding a binder to a pulverized powder mixture composed of the chromium ore and carbonaceous reducing agent, molding the mixture to a lump shape, forming a protective film on the surface and subjecting the molding to a heating treatment in a tunnel kiln. CONSTITUTION:The pulverized powder mixture preferably sized about =80% is thus obtd.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS62256938A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS62256938A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS62256938A3</originalsourceid><addsrcrecordid>eNrjZFAIcnUJdfb0c1fwdQ3x8HdRcPMPUnD2CPL39Qz1VfAPcuVhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfFeAcFmRkamZpbGFo7GxKgBAPalIjQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>REDUCING METHOD FOR CHROMIUM ORE</title><source>esp@cenet</source><creator>MINAGAWA TSUTOMU ; UEMURA TADASHI ; SASABE KIICHIRO</creator><creatorcontrib>MINAGAWA TSUTOMU ; UEMURA TADASHI ; SASABE KIICHIRO</creatorcontrib><description>PURPOSE:To reduce chromium ore at a low cost and high degree by adding a binder to a pulverized powder mixture composed of the chromium ore and carbonaceous reducing agent, molding the mixture to a lump shape, forming a protective film on the surface and subjecting the molding to a heating treatment in a tunnel kiln. CONSTITUTION:The pulverized powder mixture preferably sized about &lt;=100mesh is prepd. by mixing the chromium ore powder and carbonaceous reducing agent powder such as coke and coal. The compounding ratio of the above-mentioned carbonaceous reducing agent is specified to the theoretical ratio or the ratio slightly in excess thereof. The binder such as bentonite or CMC is added to the pulverized powder mixture and the mixture is molded to the lump shape sized about 10-300mm. The protective film which prevents the intrusion of an oxidizable combustion gas is formed by using pulverized powder such as Cr2O2, SiC and fly ash on the surface of the resulted molding. The coated molding is heated to 1,200-1,500 deg.C and reduced in the tunnel kiln. The reduced chromium ore having high reducibility of about &gt;=80% is thus obtd.</description><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1987</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19871109&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62256938A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19871109&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62256938A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MINAGAWA TSUTOMU</creatorcontrib><creatorcontrib>UEMURA TADASHI</creatorcontrib><creatorcontrib>SASABE KIICHIRO</creatorcontrib><title>REDUCING METHOD FOR CHROMIUM ORE</title><description>PURPOSE:To reduce chromium ore at a low cost and high degree by adding a binder to a pulverized powder mixture composed of the chromium ore and carbonaceous reducing agent, molding the mixture to a lump shape, forming a protective film on the surface and subjecting the molding to a heating treatment in a tunnel kiln. CONSTITUTION:The pulverized powder mixture preferably sized about &lt;=100mesh is prepd. by mixing the chromium ore powder and carbonaceous reducing agent powder such as coke and coal. The compounding ratio of the above-mentioned carbonaceous reducing agent is specified to the theoretical ratio or the ratio slightly in excess thereof. The binder such as bentonite or CMC is added to the pulverized powder mixture and the mixture is molded to the lump shape sized about 10-300mm. The protective film which prevents the intrusion of an oxidizable combustion gas is formed by using pulverized powder such as Cr2O2, SiC and fly ash on the surface of the resulted molding. The coated molding is heated to 1,200-1,500 deg.C and reduced in the tunnel kiln. The reduced chromium ore having high reducibility of about &gt;=80% is thus obtd.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1987</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFAIcnUJdfb0c1fwdQ3x8HdRcPMPUnD2CPL39Qz1VfAPcuVhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfFeAcFmRkamZpbGFo7GxKgBAPalIjQ</recordid><startdate>19871109</startdate><enddate>19871109</enddate><creator>MINAGAWA TSUTOMU</creator><creator>UEMURA TADASHI</creator><creator>SASABE KIICHIRO</creator><scope>EVB</scope></search><sort><creationdate>19871109</creationdate><title>REDUCING METHOD FOR CHROMIUM ORE</title><author>MINAGAWA TSUTOMU ; UEMURA TADASHI ; SASABE KIICHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS62256938A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1987</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>MINAGAWA TSUTOMU</creatorcontrib><creatorcontrib>UEMURA TADASHI</creatorcontrib><creatorcontrib>SASABE KIICHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MINAGAWA TSUTOMU</au><au>UEMURA TADASHI</au><au>SASABE KIICHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>REDUCING METHOD FOR CHROMIUM ORE</title><date>1987-11-09</date><risdate>1987</risdate><abstract>PURPOSE:To reduce chromium ore at a low cost and high degree by adding a binder to a pulverized powder mixture composed of the chromium ore and carbonaceous reducing agent, molding the mixture to a lump shape, forming a protective film on the surface and subjecting the molding to a heating treatment in a tunnel kiln. CONSTITUTION:The pulverized powder mixture preferably sized about &lt;=100mesh is prepd. by mixing the chromium ore powder and carbonaceous reducing agent powder such as coke and coal. The compounding ratio of the above-mentioned carbonaceous reducing agent is specified to the theoretical ratio or the ratio slightly in excess thereof. The binder such as bentonite or CMC is added to the pulverized powder mixture and the mixture is molded to the lump shape sized about 10-300mm. The protective film which prevents the intrusion of an oxidizable combustion gas is formed by using pulverized powder such as Cr2O2, SiC and fly ash on the surface of the resulted molding. The coated molding is heated to 1,200-1,500 deg.C and reduced in the tunnel kiln. The reduced chromium ore having high reducibility of about &gt;=80% is thus obtd.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS62256938A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title REDUCING METHOD FOR CHROMIUM ORE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T13%3A44%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MINAGAWA%20TSUTOMU&rft.date=1987-11-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS62256938A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true