JPS6140602B

A process for the manufacture of acicular ferrimagnetic iron oxide by dehydrating acicular iron(III) oxide hydroxides to give acicular iron(III) oxides, then reducing these iron(III) oxides at from 300 DEG to 650 DEG C. by means of an organic compound which decomposes in this temperature range, and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: UERUNERU SHUTETSUKU, UERUNERU REEZERU, RUUDORUFU BUROOTO, HERUMUUTO YAKUUSHU, EEBERUHARUTO KESUTERU, MANFUREETO OORINGERU, UIRUHERUMU ZARUNETSUKII
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator UERUNERU SHUTETSUKU
UERUNERU REEZERU
RUUDORUFU BUROOTO
HERUMUUTO YAKUUSHU
EEBERUHARUTO KESUTERU
MANFUREETO OORINGERU
UIRUHERUMU ZARUNETSUKII
description A process for the manufacture of acicular ferrimagnetic iron oxide by dehydrating acicular iron(III) oxide hydroxides to give acicular iron(III) oxides, then reducing these iron(III) oxides at from 300 DEG to 650 DEG C. by means of an organic compound which decomposes in this temperature range, and oxidizing the reduced product with an oxygen-containing gas at from 200 DEG to 500 DEG C., wherein the acicular iron(III) oxide hydroxides employed consist of a mixture of goethite and lepidocrocite, containing at least 60% of the latter, and the dehydration is carried out at from 250 DEG to 700 DEG C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS6140602BB2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS6140602BB2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS6140602BB23</originalsourceid><addsrcrecordid>eNrjZOD2Cgg2MzQxMDMwcuJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFIOpyMjIlSBAB-RBxO</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>JPS6140602B</title><source>esp@cenet</source><creator>UERUNERU SHUTETSUKU ; UERUNERU REEZERU ; RUUDORUFU BUROOTO ; HERUMUUTO YAKUUSHU ; EEBERUHARUTO KESUTERU ; MANFUREETO OORINGERU ; UIRUHERUMU ZARUNETSUKII</creator><creatorcontrib>UERUNERU SHUTETSUKU ; UERUNERU REEZERU ; RUUDORUFU BUROOTO ; HERUMUUTO YAKUUSHU ; EEBERUHARUTO KESUTERU ; MANFUREETO OORINGERU ; UIRUHERUMU ZARUNETSUKII</creatorcontrib><description>A process for the manufacture of acicular ferrimagnetic iron oxide by dehydrating acicular iron(III) oxide hydroxides to give acicular iron(III) oxides, then reducing these iron(III) oxides at from 300 DEG to 650 DEG C. by means of an organic compound which decomposes in this temperature range, and oxidizing the reduced product with an oxygen-containing gas at from 200 DEG to 500 DEG C., wherein the acicular iron(III) oxide hydroxides employed consist of a mixture of goethite and lepidocrocite, containing at least 60% of the latter, and the dehydration is carried out at from 250 DEG to 700 DEG C.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INDUCTANCES ; INFORMATION STORAGE ; INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER ; INORGANIC CHEMISTRY ; MAGNETS ; METALLURGY ; PHYSICS ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860910&amp;DB=EPODOC&amp;CC=JP&amp;NR=S6140602B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860910&amp;DB=EPODOC&amp;CC=JP&amp;NR=S6140602B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>UERUNERU SHUTETSUKU</creatorcontrib><creatorcontrib>UERUNERU REEZERU</creatorcontrib><creatorcontrib>RUUDORUFU BUROOTO</creatorcontrib><creatorcontrib>HERUMUUTO YAKUUSHU</creatorcontrib><creatorcontrib>EEBERUHARUTO KESUTERU</creatorcontrib><creatorcontrib>MANFUREETO OORINGERU</creatorcontrib><creatorcontrib>UIRUHERUMU ZARUNETSUKII</creatorcontrib><title>JPS6140602B</title><description>A process for the manufacture of acicular ferrimagnetic iron oxide by dehydrating acicular iron(III) oxide hydroxides to give acicular iron(III) oxides, then reducing these iron(III) oxides at from 300 DEG to 650 DEG C. by means of an organic compound which decomposes in this temperature range, and oxidizing the reduced product with an oxygen-containing gas at from 200 DEG to 500 DEG C., wherein the acicular iron(III) oxide hydroxides employed consist of a mixture of goethite and lepidocrocite, containing at least 60% of the latter, and the dehydration is carried out at from 250 DEG to 700 DEG C.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INDUCTANCES</subject><subject>INFORMATION STORAGE</subject><subject>INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER</subject><subject>INORGANIC CHEMISTRY</subject><subject>MAGNETS</subject><subject>METALLURGY</subject><subject>PHYSICS</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOD2Cgg2MzQxMDMwcuJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFIOpyMjIlSBAB-RBxO</recordid><startdate>19860910</startdate><enddate>19860910</enddate><creator>UERUNERU SHUTETSUKU</creator><creator>UERUNERU REEZERU</creator><creator>RUUDORUFU BUROOTO</creator><creator>HERUMUUTO YAKUUSHU</creator><creator>EEBERUHARUTO KESUTERU</creator><creator>MANFUREETO OORINGERU</creator><creator>UIRUHERUMU ZARUNETSUKII</creator><scope>EVB</scope></search><sort><creationdate>19860910</creationdate><title>JPS6140602B</title><author>UERUNERU SHUTETSUKU ; UERUNERU REEZERU ; RUUDORUFU BUROOTO ; HERUMUUTO YAKUUSHU ; EEBERUHARUTO KESUTERU ; MANFUREETO OORINGERU ; UIRUHERUMU ZARUNETSUKII</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS6140602BB23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1986</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INDUCTANCES</topic><topic>INFORMATION STORAGE</topic><topic>INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER</topic><topic>INORGANIC CHEMISTRY</topic><topic>MAGNETS</topic><topic>METALLURGY</topic><topic>PHYSICS</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><toplevel>online_resources</toplevel><creatorcontrib>UERUNERU SHUTETSUKU</creatorcontrib><creatorcontrib>UERUNERU REEZERU</creatorcontrib><creatorcontrib>RUUDORUFU BUROOTO</creatorcontrib><creatorcontrib>HERUMUUTO YAKUUSHU</creatorcontrib><creatorcontrib>EEBERUHARUTO KESUTERU</creatorcontrib><creatorcontrib>MANFUREETO OORINGERU</creatorcontrib><creatorcontrib>UIRUHERUMU ZARUNETSUKII</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>UERUNERU SHUTETSUKU</au><au>UERUNERU REEZERU</au><au>RUUDORUFU BUROOTO</au><au>HERUMUUTO YAKUUSHU</au><au>EEBERUHARUTO KESUTERU</au><au>MANFUREETO OORINGERU</au><au>UIRUHERUMU ZARUNETSUKII</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>JPS6140602B</title><date>1986-09-10</date><risdate>1986</risdate><abstract>A process for the manufacture of acicular ferrimagnetic iron oxide by dehydrating acicular iron(III) oxide hydroxides to give acicular iron(III) oxides, then reducing these iron(III) oxides at from 300 DEG to 650 DEG C. by means of an organic compound which decomposes in this temperature range, and oxidizing the reduced product with an oxygen-containing gas at from 200 DEG to 500 DEG C., wherein the acicular iron(III) oxide hydroxides employed consist of a mixture of goethite and lepidocrocite, containing at least 60% of the latter, and the dehydration is carried out at from 250 DEG to 700 DEG C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS6140602BB2
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
ELECTRICITY
INDUCTANCES
INFORMATION STORAGE
INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER
INORGANIC CHEMISTRY
MAGNETS
METALLURGY
PHYSICS
SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
TRANSFORMERS
title JPS6140602B
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T20%3A27%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=UERUNERU%20SHUTETSUKU&rft.date=1986-09-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS6140602BB2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true