MAGNETIC DISK

PURPOSE:To increase the number of times of contact start stop (CSS) by coating a CrO2 magnetic medium layer on a non-magnetic hardened layer consisting of an Ni-Cu-P alloy contg. 1-95wt% copper. CONSTITUTION:The hardened layer 2 on a non-magnetic substrate 1 is subjected to a heat treatment at >=...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NISHINAKAGAWA ISATO, FUTAMI TERUJI, OKAMURA YASUHIRO, MORITA TOMOJI, OUCHI HIROBUMI, UMEZAKI MITSUMASA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NISHINAKAGAWA ISATO
FUTAMI TERUJI
OKAMURA YASUHIRO
MORITA TOMOJI
OUCHI HIROBUMI
UMEZAKI MITSUMASA
description PURPOSE:To increase the number of times of contact start stop (CSS) by coating a CrO2 magnetic medium layer on a non-magnetic hardened layer consisting of an Ni-Cu-P alloy contg. 1-95wt% copper. CONSTITUTION:The hardened layer 2 on a non-magnetic substrate 1 is subjected to a heat treatment at >=350 deg.C to form a non-magnetized Ni-Cu-P alloy layer, by which the magnetization of the hardened layer is obviated even if a thin CrO2 film to be formed by heating is used. The decrease in the reproduced output is obviated and since the layer has substantial hardness, the number of times of CSS increases and a magnetic disk having high reliability is obtd. The Ni-Cu-P plating film which is not magnetized even if the film is subjected to the heat treatment of, for example, 350 deg.C contains 1-95wt% Cu.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS61202326A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS61202326A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS61202326A3</originalsourceid><addsrcrecordid>eNrjZOD1dXT3cw3xdFZw8Qz25mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWaGRgZGxkZmjsbEqAEAqDMcyw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MAGNETIC DISK</title><source>esp@cenet</source><creator>NISHINAKAGAWA ISATO ; FUTAMI TERUJI ; OKAMURA YASUHIRO ; MORITA TOMOJI ; OUCHI HIROBUMI ; UMEZAKI MITSUMASA</creator><creatorcontrib>NISHINAKAGAWA ISATO ; FUTAMI TERUJI ; OKAMURA YASUHIRO ; MORITA TOMOJI ; OUCHI HIROBUMI ; UMEZAKI MITSUMASA</creatorcontrib><description>PURPOSE:To increase the number of times of contact start stop (CSS) by coating a CrO2 magnetic medium layer on a non-magnetic hardened layer consisting of an Ni-Cu-P alloy contg. 1-95wt% copper. CONSTITUTION:The hardened layer 2 on a non-magnetic substrate 1 is subjected to a heat treatment at &gt;=350 deg.C to form a non-magnetized Ni-Cu-P alloy layer, by which the magnetization of the hardened layer is obviated even if a thin CrO2 film to be formed by heating is used. The decrease in the reproduced output is obviated and since the layer has substantial hardness, the number of times of CSS increases and a magnetic disk having high reliability is obtd. The Ni-Cu-P plating film which is not magnetized even if the film is subjected to the heat treatment of, for example, 350 deg.C contains 1-95wt% Cu.</description><language>eng</language><subject>INFORMATION STORAGE ; INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER ; PHYSICS</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860908&amp;DB=EPODOC&amp;CC=JP&amp;NR=S61202326A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860908&amp;DB=EPODOC&amp;CC=JP&amp;NR=S61202326A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NISHINAKAGAWA ISATO</creatorcontrib><creatorcontrib>FUTAMI TERUJI</creatorcontrib><creatorcontrib>OKAMURA YASUHIRO</creatorcontrib><creatorcontrib>MORITA TOMOJI</creatorcontrib><creatorcontrib>OUCHI HIROBUMI</creatorcontrib><creatorcontrib>UMEZAKI MITSUMASA</creatorcontrib><title>MAGNETIC DISK</title><description>PURPOSE:To increase the number of times of contact start stop (CSS) by coating a CrO2 magnetic medium layer on a non-magnetic hardened layer consisting of an Ni-Cu-P alloy contg. 1-95wt% copper. CONSTITUTION:The hardened layer 2 on a non-magnetic substrate 1 is subjected to a heat treatment at &gt;=350 deg.C to form a non-magnetized Ni-Cu-P alloy layer, by which the magnetization of the hardened layer is obviated even if a thin CrO2 film to be formed by heating is used. The decrease in the reproduced output is obviated and since the layer has substantial hardness, the number of times of CSS increases and a magnetic disk having high reliability is obtd. The Ni-Cu-P plating film which is not magnetized even if the film is subjected to the heat treatment of, for example, 350 deg.C contains 1-95wt% Cu.</description><subject>INFORMATION STORAGE</subject><subject>INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER</subject><subject>PHYSICS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOD1dXT3cw3xdFZw8Qz25mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWaGRgZGxkZmjsbEqAEAqDMcyw</recordid><startdate>19860908</startdate><enddate>19860908</enddate><creator>NISHINAKAGAWA ISATO</creator><creator>FUTAMI TERUJI</creator><creator>OKAMURA YASUHIRO</creator><creator>MORITA TOMOJI</creator><creator>OUCHI HIROBUMI</creator><creator>UMEZAKI MITSUMASA</creator><scope>EVB</scope></search><sort><creationdate>19860908</creationdate><title>MAGNETIC DISK</title><author>NISHINAKAGAWA ISATO ; FUTAMI TERUJI ; OKAMURA YASUHIRO ; MORITA TOMOJI ; OUCHI HIROBUMI ; UMEZAKI MITSUMASA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS61202326A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1986</creationdate><topic>INFORMATION STORAGE</topic><topic>INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER</topic><topic>PHYSICS</topic><toplevel>online_resources</toplevel><creatorcontrib>NISHINAKAGAWA ISATO</creatorcontrib><creatorcontrib>FUTAMI TERUJI</creatorcontrib><creatorcontrib>OKAMURA YASUHIRO</creatorcontrib><creatorcontrib>MORITA TOMOJI</creatorcontrib><creatorcontrib>OUCHI HIROBUMI</creatorcontrib><creatorcontrib>UMEZAKI MITSUMASA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NISHINAKAGAWA ISATO</au><au>FUTAMI TERUJI</au><au>OKAMURA YASUHIRO</au><au>MORITA TOMOJI</au><au>OUCHI HIROBUMI</au><au>UMEZAKI MITSUMASA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MAGNETIC DISK</title><date>1986-09-08</date><risdate>1986</risdate><abstract>PURPOSE:To increase the number of times of contact start stop (CSS) by coating a CrO2 magnetic medium layer on a non-magnetic hardened layer consisting of an Ni-Cu-P alloy contg. 1-95wt% copper. CONSTITUTION:The hardened layer 2 on a non-magnetic substrate 1 is subjected to a heat treatment at &gt;=350 deg.C to form a non-magnetized Ni-Cu-P alloy layer, by which the magnetization of the hardened layer is obviated even if a thin CrO2 film to be formed by heating is used. The decrease in the reproduced output is obviated and since the layer has substantial hardness, the number of times of CSS increases and a magnetic disk having high reliability is obtd. The Ni-Cu-P plating film which is not magnetized even if the film is subjected to the heat treatment of, for example, 350 deg.C contains 1-95wt% Cu.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS61202326A
source esp@cenet
subjects INFORMATION STORAGE
INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORDCARRIER AND TRANSDUCER
PHYSICS
title MAGNETIC DISK
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T22%3A59%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NISHINAKAGAWA%20ISATO&rft.date=1986-09-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS61202326A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true