METHOD FOR REMOVING IMPURITY FROM MAGNESIUM

PURPOSE:To obtain high purity Mg by bringing molten Mg contg. impurities such as Fe and Mn into contact with boric acid or a borate so as to separate and remove the impurities. CONSTITUTION:Mg contg. impurities such as Fe and Mn is melted, diboron trioxide, boric acid such as orthoboric acid or an a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OKI SHIYUUJIROU, HIRASAWA YOSHIKAZU, KIKUTA TOSHIHARU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator OKI SHIYUUJIROU
HIRASAWA YOSHIKAZU
KIKUTA TOSHIHARU
description PURPOSE:To obtain high purity Mg by bringing molten Mg contg. impurities such as Fe and Mn into contact with boric acid or a borate so as to separate and remove the impurities. CONSTITUTION:Mg contg. impurities such as Fe and Mn is melted, diboron trioxide, boric acid such as orthoboric acid or an alkali metallic borate such as sodium tetraborate is mixed with a flux for melting Mg by 1-20kg (expressed in terms of boron) per 1 ton Mg, and the molten Mg is brought into contact with the mixture at >=700 deg.C. Boron produced by the reduction of the borate with the Mg bonds to the Fe, Mn, etc., and the resulting compounds settle and form sludge together with oxides and nitrides absorbed in the flux. The sludge is then separated to obtain high purity Mg usable as a reducing agent in the manufacture of Ti or Zr.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS61201742A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS61201742A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS61201742A3</originalsourceid><addsrcrecordid>eNrjZND2dQ3x8HdRcPMPUghy9fUP8_RzV_D0DQgN8gyJVHAL8vdV8HV093MN9gz15WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWaGRgaG5iZGjsbEqAEAkgElZA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR REMOVING IMPURITY FROM MAGNESIUM</title><source>esp@cenet</source><creator>OKI SHIYUUJIROU ; HIRASAWA YOSHIKAZU ; KIKUTA TOSHIHARU</creator><creatorcontrib>OKI SHIYUUJIROU ; HIRASAWA YOSHIKAZU ; KIKUTA TOSHIHARU</creatorcontrib><description>PURPOSE:To obtain high purity Mg by bringing molten Mg contg. impurities such as Fe and Mn into contact with boric acid or a borate so as to separate and remove the impurities. CONSTITUTION:Mg contg. impurities such as Fe and Mn is melted, diboron trioxide, boric acid such as orthoboric acid or an alkali metallic borate such as sodium tetraborate is mixed with a flux for melting Mg by 1-20kg (expressed in terms of boron) per 1 ton Mg, and the molten Mg is brought into contact with the mixture at &gt;=700 deg.C. Boron produced by the reduction of the borate with the Mg bonds to the Fe, Mn, etc., and the resulting compounds settle and form sludge together with oxides and nitrides absorbed in the flux. The sludge is then separated to obtain high purity Mg usable as a reducing agent in the manufacture of Ti or Zr.</description><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860906&amp;DB=EPODOC&amp;CC=JP&amp;NR=S61201742A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25553,76306</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860906&amp;DB=EPODOC&amp;CC=JP&amp;NR=S61201742A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OKI SHIYUUJIROU</creatorcontrib><creatorcontrib>HIRASAWA YOSHIKAZU</creatorcontrib><creatorcontrib>KIKUTA TOSHIHARU</creatorcontrib><title>METHOD FOR REMOVING IMPURITY FROM MAGNESIUM</title><description>PURPOSE:To obtain high purity Mg by bringing molten Mg contg. impurities such as Fe and Mn into contact with boric acid or a borate so as to separate and remove the impurities. CONSTITUTION:Mg contg. impurities such as Fe and Mn is melted, diboron trioxide, boric acid such as orthoboric acid or an alkali metallic borate such as sodium tetraborate is mixed with a flux for melting Mg by 1-20kg (expressed in terms of boron) per 1 ton Mg, and the molten Mg is brought into contact with the mixture at &gt;=700 deg.C. Boron produced by the reduction of the borate with the Mg bonds to the Fe, Mn, etc., and the resulting compounds settle and form sludge together with oxides and nitrides absorbed in the flux. The sludge is then separated to obtain high purity Mg usable as a reducing agent in the manufacture of Ti or Zr.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND2dQ3x8HdRcPMPUghy9fUP8_RzV_D0DQgN8gyJVHAL8vdV8HV093MN9gz15WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BwWaGRgaG5iZGjsbEqAEAkgElZA</recordid><startdate>19860906</startdate><enddate>19860906</enddate><creator>OKI SHIYUUJIROU</creator><creator>HIRASAWA YOSHIKAZU</creator><creator>KIKUTA TOSHIHARU</creator><scope>EVB</scope></search><sort><creationdate>19860906</creationdate><title>METHOD FOR REMOVING IMPURITY FROM MAGNESIUM</title><author>OKI SHIYUUJIROU ; HIRASAWA YOSHIKAZU ; KIKUTA TOSHIHARU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS61201742A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1986</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>OKI SHIYUUJIROU</creatorcontrib><creatorcontrib>HIRASAWA YOSHIKAZU</creatorcontrib><creatorcontrib>KIKUTA TOSHIHARU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OKI SHIYUUJIROU</au><au>HIRASAWA YOSHIKAZU</au><au>KIKUTA TOSHIHARU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR REMOVING IMPURITY FROM MAGNESIUM</title><date>1986-09-06</date><risdate>1986</risdate><abstract>PURPOSE:To obtain high purity Mg by bringing molten Mg contg. impurities such as Fe and Mn into contact with boric acid or a borate so as to separate and remove the impurities. CONSTITUTION:Mg contg. impurities such as Fe and Mn is melted, diboron trioxide, boric acid such as orthoboric acid or an alkali metallic borate such as sodium tetraborate is mixed with a flux for melting Mg by 1-20kg (expressed in terms of boron) per 1 ton Mg, and the molten Mg is brought into contact with the mixture at &gt;=700 deg.C. Boron produced by the reduction of the borate with the Mg bonds to the Fe, Mn, etc., and the resulting compounds settle and form sludge together with oxides and nitrides absorbed in the flux. The sludge is then separated to obtain high purity Mg usable as a reducing agent in the manufacture of Ti or Zr.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS61201742A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR REMOVING IMPURITY FROM MAGNESIUM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T08%3A53%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OKI%20SHIYUUJIROU&rft.date=1986-09-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS61201742A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true