COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE

PURPOSE:To obtain a titled welding rod which is capable of obtaining a weld metal which is excellent in a crack opening displacement (COD) characteristic and low temperature toughness, by covering a soft steel core wire with a coating flux which contains Ti and B of a proper quantity, and also has a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TANIGAKI TAKASHI, YAMADA TERUHISA, OOTAWA MOTOHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TANIGAKI TAKASHI
YAMADA TERUHISA
OOTAWA MOTOHIRO
description PURPOSE:To obtain a titled welding rod which is capable of obtaining a weld metal which is excellent in a crack opening displacement (COD) characteristic and low temperature toughness, by covering a soft steel core wire with a coating flux which contains Ti and B of a proper quantity, and also has added carbonate, fluoride, Si, Mn, Al, etc. CONSTITUTION:A covered arc welding rod generating low hydrogen atmosphere is obtained by covering a soft steel core wire with a coating flux constituted by mixing 25-55% one kind or more of CaCO3, MgCO3 and BaCO3, 2-10% titanium oxide (expressed in terms of TiO2), 1-25% one kind or more of CaF2, Na3AlF6, MgF2 and AlF3, 1-8% Si, 0.1-0.6% one kind or more of an alloy of B or a carbide of B (expressed in terms of B) of Ti, Al, Zr, Cr, Mo, Mn and Ni, also in total 2-6% an alloy of B and Mn except Mn-B alloys in total 0.5-3.0% an alloy of B and Ti except Ti-B of alloys, and in total 0.1-4.0% one kind or more or Al, Mg, Ca and Zr (as for Al and Zr, that which is added as an alloy with B is contained), and also a slag agent, an arc stabilizer and a tackifier, other than above described components, as other contents.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS5853393A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS5853393A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS5853393A3</originalsourceid><addsrcrecordid>eNrjZLBy9g9zDXJ1UXAMclYId_Vx8fRzVwjyd1Fwd_VzDXIMAXF9_MMVPCJdgvyBYgqOIb7-wQEeQD08DKxpiTnFqbxQmptBwc01xNlDN7UgPz61uCAxOTUvtSTeKyDY1MLU2NjS2NGYCCUAZzwo-g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE</title><source>esp@cenet</source><creator>TANIGAKI TAKASHI ; YAMADA TERUHISA ; OOTAWA MOTOHIRO</creator><creatorcontrib>TANIGAKI TAKASHI ; YAMADA TERUHISA ; OOTAWA MOTOHIRO</creatorcontrib><description>PURPOSE:To obtain a titled welding rod which is capable of obtaining a weld metal which is excellent in a crack opening displacement (COD) characteristic and low temperature toughness, by covering a soft steel core wire with a coating flux which contains Ti and B of a proper quantity, and also has added carbonate, fluoride, Si, Mn, Al, etc. CONSTITUTION:A covered arc welding rod generating low hydrogen atmosphere is obtained by covering a soft steel core wire with a coating flux constituted by mixing 25-55% one kind or more of CaCO3, MgCO3 and BaCO3, 2-10% titanium oxide (expressed in terms of TiO2), 1-25% one kind or more of CaF2, Na3AlF6, MgF2 and AlF3, 1-8% Si, 0.1-0.6% one kind or more of an alloy of B or a carbide of B (expressed in terms of B) of Ti, Al, Zr, Cr, Mo, Mn and Ni, also in total 2-6% an alloy of B and Mn except Mn-B alloys in total 0.5-3.0% an alloy of B and Ti except Ti-B of alloys, and in total 0.1-4.0% one kind or more or Al, Mg, Ca and Zr (as for Al and Zr, that which is added as an alloy with B is contained), and also a slag agent, an arc stabilizer and a tackifier, other than above described components, as other contents.</description><language>eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>1983</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19830329&amp;DB=EPODOC&amp;CC=JP&amp;NR=S5853393A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19830329&amp;DB=EPODOC&amp;CC=JP&amp;NR=S5853393A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TANIGAKI TAKASHI</creatorcontrib><creatorcontrib>YAMADA TERUHISA</creatorcontrib><creatorcontrib>OOTAWA MOTOHIRO</creatorcontrib><title>COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE</title><description>PURPOSE:To obtain a titled welding rod which is capable of obtaining a weld metal which is excellent in a crack opening displacement (COD) characteristic and low temperature toughness, by covering a soft steel core wire with a coating flux which contains Ti and B of a proper quantity, and also has added carbonate, fluoride, Si, Mn, Al, etc. CONSTITUTION:A covered arc welding rod generating low hydrogen atmosphere is obtained by covering a soft steel core wire with a coating flux constituted by mixing 25-55% one kind or more of CaCO3, MgCO3 and BaCO3, 2-10% titanium oxide (expressed in terms of TiO2), 1-25% one kind or more of CaF2, Na3AlF6, MgF2 and AlF3, 1-8% Si, 0.1-0.6% one kind or more of an alloy of B or a carbide of B (expressed in terms of B) of Ti, Al, Zr, Cr, Mo, Mn and Ni, also in total 2-6% an alloy of B and Mn except Mn-B alloys in total 0.5-3.0% an alloy of B and Ti except Ti-B of alloys, and in total 0.1-4.0% one kind or more or Al, Mg, Ca and Zr (as for Al and Zr, that which is added as an alloy with B is contained), and also a slag agent, an arc stabilizer and a tackifier, other than above described components, as other contents.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1983</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBy9g9zDXJ1UXAMclYId_Vx8fRzVwjyd1Fwd_VzDXIMAXF9_MMVPCJdgvyBYgqOIb7-wQEeQD08DKxpiTnFqbxQmptBwc01xNlDN7UgPz61uCAxOTUvtSTeKyDY1MLU2NjS2NGYCCUAZzwo-g</recordid><startdate>19830329</startdate><enddate>19830329</enddate><creator>TANIGAKI TAKASHI</creator><creator>YAMADA TERUHISA</creator><creator>OOTAWA MOTOHIRO</creator><scope>EVB</scope></search><sort><creationdate>19830329</creationdate><title>COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE</title><author>TANIGAKI TAKASHI ; YAMADA TERUHISA ; OOTAWA MOTOHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS5853393A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1983</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>TANIGAKI TAKASHI</creatorcontrib><creatorcontrib>YAMADA TERUHISA</creatorcontrib><creatorcontrib>OOTAWA MOTOHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TANIGAKI TAKASHI</au><au>YAMADA TERUHISA</au><au>OOTAWA MOTOHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE</title><date>1983-03-29</date><risdate>1983</risdate><abstract>PURPOSE:To obtain a titled welding rod which is capable of obtaining a weld metal which is excellent in a crack opening displacement (COD) characteristic and low temperature toughness, by covering a soft steel core wire with a coating flux which contains Ti and B of a proper quantity, and also has added carbonate, fluoride, Si, Mn, Al, etc. CONSTITUTION:A covered arc welding rod generating low hydrogen atmosphere is obtained by covering a soft steel core wire with a coating flux constituted by mixing 25-55% one kind or more of CaCO3, MgCO3 and BaCO3, 2-10% titanium oxide (expressed in terms of TiO2), 1-25% one kind or more of CaF2, Na3AlF6, MgF2 and AlF3, 1-8% Si, 0.1-0.6% one kind or more of an alloy of B or a carbide of B (expressed in terms of B) of Ti, Al, Zr, Cr, Mo, Mn and Ni, also in total 2-6% an alloy of B and Mn except Mn-B alloys in total 0.5-3.0% an alloy of B and Ti except Ti-B of alloys, and in total 0.1-4.0% one kind or more or Al, Mg, Ca and Zr (as for Al and Zr, that which is added as an alloy with B is contained), and also a slag agent, an arc stabilizer and a tackifier, other than above described components, as other contents.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS5853393A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title COVERED ARC WELDING ROD GENERATING LOW HYDROGEN ATMOSPHERE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T03%3A20%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TANIGAKI%20TAKASHI&rft.date=1983-03-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS5853393A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true