MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM

PROBLEM TO BE SOLVED: To improve the sintering characteristic of Li2 O micro balls and reduce the manufacturing cost by shortening the heat decomposition time of Li2 CO3 in a method of manufacturing Li2 O micro balls for breeding tritium. SOLUTION: A large number of micro fibrous compounds evaporate...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OHASHI JUNPEI, FUCHINOUE KATSUHIRO, SAWADA HIROSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator OHASHI JUNPEI
FUCHINOUE KATSUHIRO
SAWADA HIROSHI
description PROBLEM TO BE SOLVED: To improve the sintering characteristic of Li2 O micro balls and reduce the manufacturing cost by shortening the heat decomposition time of Li2 CO3 in a method of manufacturing Li2 O micro balls for breeding tritium. SOLUTION: A large number of micro fibrous compounds evaporated and scattered by heating are added and uniformly dispersed in a drip stock solution with Li2 CO3 powder mixed in a gel medium. Gel balls containing Li2 CO3 are manufactured from this drip stock solution, and the gel balls containing Li2 CO3 are subjected to heat treatment. The gel medium and the fibrous compounds are therefore evaporated and scattered to form micro balls of Li2 CO3 , and pores communicating from the interior to the exterior through the surface of the ball are formed in the micro balls of Li2 CO3 by evaporation and scattering of the fibrous compounds. The micro balls of Li2 CO3 with pores are heat- decomposed to obtain micro balls of Li2 O.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH1164556A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH1164556A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH1164556A3</originalsourceid><addsrcrecordid>eNrjZLDxdfQLdXN0DgkNclXwd1Pw8Qzx8Az1VfCP8HRxVfD1dA7yV3By9PFRcPMPUnAKcnV18fRzVwgJ8gwBquJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFeAR6GhmYmpqZmjsZEKAEAsCkpSg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM</title><source>esp@cenet</source><creator>OHASHI JUNPEI ; FUCHINOUE KATSUHIRO ; SAWADA HIROSHI</creator><creatorcontrib>OHASHI JUNPEI ; FUCHINOUE KATSUHIRO ; SAWADA HIROSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To improve the sintering characteristic of Li2 O micro balls and reduce the manufacturing cost by shortening the heat decomposition time of Li2 CO3 in a method of manufacturing Li2 O micro balls for breeding tritium. SOLUTION: A large number of micro fibrous compounds evaporated and scattered by heating are added and uniformly dispersed in a drip stock solution with Li2 CO3 powder mixed in a gel medium. Gel balls containing Li2 CO3 are manufactured from this drip stock solution, and the gel balls containing Li2 CO3 are subjected to heat treatment. The gel medium and the fibrous compounds are therefore evaporated and scattered to form micro balls of Li2 CO3 , and pores communicating from the interior to the exterior through the surface of the ball are formed in the micro balls of Li2 CO3 by evaporation and scattering of the fibrous compounds. The micro balls of Li2 CO3 with pores are heat- decomposed to obtain micro balls of Li2 O.</description><edition>6</edition><language>eng</language><subject>FUSION REACTORS ; NUCLEAR ENGINEERING ; NUCLEAR PHYSICS ; NUCLEAR REACTORS ; PHYSICS</subject><creationdate>1999</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990305&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1164556A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990305&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1164556A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OHASHI JUNPEI</creatorcontrib><creatorcontrib>FUCHINOUE KATSUHIRO</creatorcontrib><creatorcontrib>SAWADA HIROSHI</creatorcontrib><title>MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM</title><description>PROBLEM TO BE SOLVED: To improve the sintering characteristic of Li2 O micro balls and reduce the manufacturing cost by shortening the heat decomposition time of Li2 CO3 in a method of manufacturing Li2 O micro balls for breeding tritium. SOLUTION: A large number of micro fibrous compounds evaporated and scattered by heating are added and uniformly dispersed in a drip stock solution with Li2 CO3 powder mixed in a gel medium. Gel balls containing Li2 CO3 are manufactured from this drip stock solution, and the gel balls containing Li2 CO3 are subjected to heat treatment. The gel medium and the fibrous compounds are therefore evaporated and scattered to form micro balls of Li2 CO3 , and pores communicating from the interior to the exterior through the surface of the ball are formed in the micro balls of Li2 CO3 by evaporation and scattering of the fibrous compounds. The micro balls of Li2 CO3 with pores are heat- decomposed to obtain micro balls of Li2 O.</description><subject>FUSION REACTORS</subject><subject>NUCLEAR ENGINEERING</subject><subject>NUCLEAR PHYSICS</subject><subject>NUCLEAR REACTORS</subject><subject>PHYSICS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1999</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDxdfQLdXN0DgkNclXwd1Pw8Qzx8Az1VfCP8HRxVfD1dA7yV3By9PFRcPMPUnAKcnV18fRzVwgJ8gwBquJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfFeAR6GhmYmpqZmjsZEKAEAsCkpSg</recordid><startdate>19990305</startdate><enddate>19990305</enddate><creator>OHASHI JUNPEI</creator><creator>FUCHINOUE KATSUHIRO</creator><creator>SAWADA HIROSHI</creator><scope>EVB</scope></search><sort><creationdate>19990305</creationdate><title>MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM</title><author>OHASHI JUNPEI ; FUCHINOUE KATSUHIRO ; SAWADA HIROSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH1164556A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1999</creationdate><topic>FUSION REACTORS</topic><topic>NUCLEAR ENGINEERING</topic><topic>NUCLEAR PHYSICS</topic><topic>NUCLEAR REACTORS</topic><topic>PHYSICS</topic><toplevel>online_resources</toplevel><creatorcontrib>OHASHI JUNPEI</creatorcontrib><creatorcontrib>FUCHINOUE KATSUHIRO</creatorcontrib><creatorcontrib>SAWADA HIROSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OHASHI JUNPEI</au><au>FUCHINOUE KATSUHIRO</au><au>SAWADA HIROSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM</title><date>1999-03-05</date><risdate>1999</risdate><abstract>PROBLEM TO BE SOLVED: To improve the sintering characteristic of Li2 O micro balls and reduce the manufacturing cost by shortening the heat decomposition time of Li2 CO3 in a method of manufacturing Li2 O micro balls for breeding tritium. SOLUTION: A large number of micro fibrous compounds evaporated and scattered by heating are added and uniformly dispersed in a drip stock solution with Li2 CO3 powder mixed in a gel medium. Gel balls containing Li2 CO3 are manufactured from this drip stock solution, and the gel balls containing Li2 CO3 are subjected to heat treatment. The gel medium and the fibrous compounds are therefore evaporated and scattered to form micro balls of Li2 CO3 , and pores communicating from the interior to the exterior through the surface of the ball are formed in the micro balls of Li2 CO3 by evaporation and scattering of the fibrous compounds. The micro balls of Li2 CO3 with pores are heat- decomposed to obtain micro balls of Li2 O.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH1164556A
source esp@cenet
subjects FUSION REACTORS
NUCLEAR ENGINEERING
NUCLEAR PHYSICS
NUCLEAR REACTORS
PHYSICS
title MANUFACTURE OF LITHIUM OXIDE MICRO BALL FOR BREEDING TRITIUM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-21T17%3A50%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OHASHI%20JUNPEI&rft.date=1999-03-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH1164556A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true