LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY

PROBLEM TO BE SOLVED: To obtain the steel that is suitable for use in a ferromagnetic field and corrosive environment and that is superior in corrosion resistance and weldability by specifying the composition made up of C, Si, Mn, Cr, N and Fe and regulating Ni quantity in inevitable impurities. SOL...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SOKAWA TSUNEHIKO, SATO IKUO, ETO MOTOKUNI, KUSUHASHI MIKIO, ISHIYAMA SHINTARO, FUKAYA KIYOSHI, HATAKEYAMA TAKESHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SOKAWA TSUNEHIKO
SATO IKUO
ETO MOTOKUNI
KUSUHASHI MIKIO
ISHIYAMA SHINTARO
FUKAYA KIYOSHI
HATAKEYAMA TAKESHI
description PROBLEM TO BE SOLVED: To obtain the steel that is suitable for use in a ferromagnetic field and corrosive environment and that is superior in corrosion resistance and weldability by specifying the composition made up of C, Si, Mn, Cr, N and Fe and regulating Ni quantity in inevitable impurities. SOLUTION: The superior nonmagnetic steel is obtained by which contains 0.05-0.25 wt.% C, 1.0% or less Si, 10.0-18.0% Mn, 15.0 plus-18.0% Cr, and 0.30% or less N, with the balance essentially consisting of Fe and inevitable impurities, in which Ni content in the inevitable impurities is desirably regulated at 0.2% or less, in which nuclear exothermic and activation are suppressed, with the components satisfying an expression, i.e., A/B>=1.45 (A=24C+21N, B=Cr+0.5Si+0.07Mn-13.2), and in which no δ ferrite is contained. This nonmagnetic steel is provided with the mechanical characteristics, weldability and nonmagnetism equivalent to stainless steel, and also indicative of excellent corrosion resistance in the real environment, so that it is suitable as a material for the vacuum container of a nuclear fusion reactor.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH1161340A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH1161340A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH1161340A3</originalsourceid><addsrcrecordid>eNqNi8EKgkAQQL10iOof5gekxOg-rlNOrDOyrlknkdjoECXY_1NCH9DpweO9eXS32oI0xhI6oLP6glzJZj1pNJ5P6FkFSomNA1GJSzwIeTZQeyILdVORY3XAAihfr85pPS0oObRkc8zYsr8so9mtf4xh9eMigj15U8RheHVhHPpreIZ3d6yKJNkl6XaD6R_JB-1VNbc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY</title><source>esp@cenet</source><creator>SOKAWA TSUNEHIKO ; SATO IKUO ; ETO MOTOKUNI ; KUSUHASHI MIKIO ; ISHIYAMA SHINTARO ; FUKAYA KIYOSHI ; HATAKEYAMA TAKESHI</creator><creatorcontrib>SOKAWA TSUNEHIKO ; SATO IKUO ; ETO MOTOKUNI ; KUSUHASHI MIKIO ; ISHIYAMA SHINTARO ; FUKAYA KIYOSHI ; HATAKEYAMA TAKESHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To obtain the steel that is suitable for use in a ferromagnetic field and corrosive environment and that is superior in corrosion resistance and weldability by specifying the composition made up of C, Si, Mn, Cr, N and Fe and regulating Ni quantity in inevitable impurities. SOLUTION: The superior nonmagnetic steel is obtained by which contains 0.05-0.25 wt.% C, 1.0% or less Si, 10.0-18.0% Mn, 15.0 plus-18.0% Cr, and 0.30% or less N, with the balance essentially consisting of Fe and inevitable impurities, in which Ni content in the inevitable impurities is desirably regulated at 0.2% or less, in which nuclear exothermic and activation are suppressed, with the components satisfying an expression, i.e., A/B&gt;=1.45 (A=24C+21N, B=Cr+0.5Si+0.07Mn-13.2), and in which no δ ferrite is contained. This nonmagnetic steel is provided with the mechanical characteristics, weldability and nonmagnetism equivalent to stainless steel, and also indicative of excellent corrosion resistance in the real environment, so that it is suitable as a material for the vacuum container of a nuclear fusion reactor.</description><edition>6</edition><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; FUSION REACTORS ; METALLURGY ; NUCLEAR ENGINEERING ; NUCLEAR PHYSICS ; PHYSICS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1999</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990305&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1161340A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25547,76298</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990305&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1161340A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SOKAWA TSUNEHIKO</creatorcontrib><creatorcontrib>SATO IKUO</creatorcontrib><creatorcontrib>ETO MOTOKUNI</creatorcontrib><creatorcontrib>KUSUHASHI MIKIO</creatorcontrib><creatorcontrib>ISHIYAMA SHINTARO</creatorcontrib><creatorcontrib>FUKAYA KIYOSHI</creatorcontrib><creatorcontrib>HATAKEYAMA TAKESHI</creatorcontrib><title>LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY</title><description>PROBLEM TO BE SOLVED: To obtain the steel that is suitable for use in a ferromagnetic field and corrosive environment and that is superior in corrosion resistance and weldability by specifying the composition made up of C, Si, Mn, Cr, N and Fe and regulating Ni quantity in inevitable impurities. SOLUTION: The superior nonmagnetic steel is obtained by which contains 0.05-0.25 wt.% C, 1.0% or less Si, 10.0-18.0% Mn, 15.0 plus-18.0% Cr, and 0.30% or less N, with the balance essentially consisting of Fe and inevitable impurities, in which Ni content in the inevitable impurities is desirably regulated at 0.2% or less, in which nuclear exothermic and activation are suppressed, with the components satisfying an expression, i.e., A/B&gt;=1.45 (A=24C+21N, B=Cr+0.5Si+0.07Mn-13.2), and in which no δ ferrite is contained. This nonmagnetic steel is provided with the mechanical characteristics, weldability and nonmagnetism equivalent to stainless steel, and also indicative of excellent corrosion resistance in the real environment, so that it is suitable as a material for the vacuum container of a nuclear fusion reactor.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>FUSION REACTORS</subject><subject>METALLURGY</subject><subject>NUCLEAR ENGINEERING</subject><subject>NUCLEAR PHYSICS</subject><subject>PHYSICS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1999</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi8EKgkAQQL10iOof5gekxOg-rlNOrDOyrlknkdjoECXY_1NCH9DpweO9eXS32oI0xhI6oLP6glzJZj1pNJ5P6FkFSomNA1GJSzwIeTZQeyILdVORY3XAAihfr85pPS0oObRkc8zYsr8so9mtf4xh9eMigj15U8RheHVhHPpreIZ3d6yKJNkl6XaD6R_JB-1VNbc</recordid><startdate>19990305</startdate><enddate>19990305</enddate><creator>SOKAWA TSUNEHIKO</creator><creator>SATO IKUO</creator><creator>ETO MOTOKUNI</creator><creator>KUSUHASHI MIKIO</creator><creator>ISHIYAMA SHINTARO</creator><creator>FUKAYA KIYOSHI</creator><creator>HATAKEYAMA TAKESHI</creator><scope>EVB</scope></search><sort><creationdate>19990305</creationdate><title>LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY</title><author>SOKAWA TSUNEHIKO ; SATO IKUO ; ETO MOTOKUNI ; KUSUHASHI MIKIO ; ISHIYAMA SHINTARO ; FUKAYA KIYOSHI ; HATAKEYAMA TAKESHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH1161340A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1999</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>FUSION REACTORS</topic><topic>METALLURGY</topic><topic>NUCLEAR ENGINEERING</topic><topic>NUCLEAR PHYSICS</topic><topic>PHYSICS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SOKAWA TSUNEHIKO</creatorcontrib><creatorcontrib>SATO IKUO</creatorcontrib><creatorcontrib>ETO MOTOKUNI</creatorcontrib><creatorcontrib>KUSUHASHI MIKIO</creatorcontrib><creatorcontrib>ISHIYAMA SHINTARO</creatorcontrib><creatorcontrib>FUKAYA KIYOSHI</creatorcontrib><creatorcontrib>HATAKEYAMA TAKESHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SOKAWA TSUNEHIKO</au><au>SATO IKUO</au><au>ETO MOTOKUNI</au><au>KUSUHASHI MIKIO</au><au>ISHIYAMA SHINTARO</au><au>FUKAYA KIYOSHI</au><au>HATAKEYAMA TAKESHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY</title><date>1999-03-05</date><risdate>1999</risdate><abstract>PROBLEM TO BE SOLVED: To obtain the steel that is suitable for use in a ferromagnetic field and corrosive environment and that is superior in corrosion resistance and weldability by specifying the composition made up of C, Si, Mn, Cr, N and Fe and regulating Ni quantity in inevitable impurities. SOLUTION: The superior nonmagnetic steel is obtained by which contains 0.05-0.25 wt.% C, 1.0% or less Si, 10.0-18.0% Mn, 15.0 plus-18.0% Cr, and 0.30% or less N, with the balance essentially consisting of Fe and inevitable impurities, in which Ni content in the inevitable impurities is desirably regulated at 0.2% or less, in which nuclear exothermic and activation are suppressed, with the components satisfying an expression, i.e., A/B&gt;=1.45 (A=24C+21N, B=Cr+0.5Si+0.07Mn-13.2), and in which no δ ferrite is contained. This nonmagnetic steel is provided with the mechanical characteristics, weldability and nonmagnetism equivalent to stainless steel, and also indicative of excellent corrosion resistance in the real environment, so that it is suitable as a material for the vacuum container of a nuclear fusion reactor.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH1161340A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
FUSION REACTORS
METALLURGY
NUCLEAR ENGINEERING
NUCLEAR PHYSICS
PHYSICS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title LOW NUCLEAR EXOTHERMIC/LOW ACTIVATION MN-CR NON-MAGNETIC STEEL SUPERIOR IN ANTICORROSION AND WELDABILITY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T20%3A46%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SOKAWA%20TSUNEHIKO&rft.date=1999-03-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH1161340A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true