ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR

PROBLEM TO BE SOLVED: To restrain corrosion of a nickel sintered base board, to restrain reduction in a strength characteristic of the nickel sintered base board, and to restrain conversion of an active material into γ-NiOOH at charging time by covering the surface of the nickel sintered base board...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HASHIMOTO SATORU, KURATSUKA MAKI, MURAOKA YOSHIYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HASHIMOTO SATORU
KURATSUKA MAKI
MURAOKA YOSHIYUKI
description PROBLEM TO BE SOLVED: To restrain corrosion of a nickel sintered base board, to restrain reduction in a strength characteristic of the nickel sintered base board, and to restrain conversion of an active material into γ-NiOOH at charging time by covering the surface of the nickel sintered base board with a mixed oxide layer being mainly composed of cobalt oxide and containing a small quantity of iron oxide. SOLUTION: In a mixed oxide layer, and in the mole ratio of iron oxide to cobalt oxide, when the cobalt oxide is denoted by 100, the iron oxide is 0.5 to 5, and both are desirably uniformly mixed together. Cobalt oxyhydroxide is desirable as the cobalt oxide, and iron hydroxide is desirable as the iron oxide. A nickel sintered base board by forming a sintered body of nickel powder on both surfaces of a metallic core material, is dried at 80 to 150 deg.C after being soaked and impregnated into a mixed salt aqueous solution of a cobalt nitrate and an iron sulfate, and then, is soaked in an alkali aqueous solution to perform oxidation treatment at 100 to 180 deg.C in the air after substituting salt sticking to this base board with hydroxide.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH11273684A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH11273684A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH11273684A3</originalsourceid><addsrcrecordid>eNrjZPB09PF29PH0c1UIDvEPcnR3VXByDAlxDYpUcPRzUfB19At1c3QOCQ1yVfB3U3D1cXUOCfJ3ASkKBhL-jkEuCiEerkGubv5BPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3ivAw9DQyNzYzMLE0ZgYNQAc-S0f</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR</title><source>esp@cenet</source><creator>HASHIMOTO SATORU ; KURATSUKA MAKI ; MURAOKA YOSHIYUKI</creator><creatorcontrib>HASHIMOTO SATORU ; KURATSUKA MAKI ; MURAOKA YOSHIYUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To restrain corrosion of a nickel sintered base board, to restrain reduction in a strength characteristic of the nickel sintered base board, and to restrain conversion of an active material into γ-NiOOH at charging time by covering the surface of the nickel sintered base board with a mixed oxide layer being mainly composed of cobalt oxide and containing a small quantity of iron oxide. SOLUTION: In a mixed oxide layer, and in the mole ratio of iron oxide to cobalt oxide, when the cobalt oxide is denoted by 100, the iron oxide is 0.5 to 5, and both are desirably uniformly mixed together. Cobalt oxyhydroxide is desirable as the cobalt oxide, and iron hydroxide is desirable as the iron oxide. A nickel sintered base board by forming a sintered body of nickel powder on both surfaces of a metallic core material, is dried at 80 to 150 deg.C after being soaked and impregnated into a mixed salt aqueous solution of a cobalt nitrate and an iron sulfate, and then, is soaked in an alkali aqueous solution to perform oxidation treatment at 100 to 180 deg.C in the air after substituting salt sticking to this base board with hydroxide.</description><edition>6</edition><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>1999</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19991008&amp;DB=EPODOC&amp;CC=JP&amp;NR=H11273684A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19991008&amp;DB=EPODOC&amp;CC=JP&amp;NR=H11273684A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HASHIMOTO SATORU</creatorcontrib><creatorcontrib>KURATSUKA MAKI</creatorcontrib><creatorcontrib>MURAOKA YOSHIYUKI</creatorcontrib><title>ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR</title><description>PROBLEM TO BE SOLVED: To restrain corrosion of a nickel sintered base board, to restrain reduction in a strength characteristic of the nickel sintered base board, and to restrain conversion of an active material into γ-NiOOH at charging time by covering the surface of the nickel sintered base board with a mixed oxide layer being mainly composed of cobalt oxide and containing a small quantity of iron oxide. SOLUTION: In a mixed oxide layer, and in the mole ratio of iron oxide to cobalt oxide, when the cobalt oxide is denoted by 100, the iron oxide is 0.5 to 5, and both are desirably uniformly mixed together. Cobalt oxyhydroxide is desirable as the cobalt oxide, and iron hydroxide is desirable as the iron oxide. A nickel sintered base board by forming a sintered body of nickel powder on both surfaces of a metallic core material, is dried at 80 to 150 deg.C after being soaked and impregnated into a mixed salt aqueous solution of a cobalt nitrate and an iron sulfate, and then, is soaked in an alkali aqueous solution to perform oxidation treatment at 100 to 180 deg.C in the air after substituting salt sticking to this base board with hydroxide.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1999</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPB09PF29PH0c1UIDvEPcnR3VXByDAlxDYpUcPRzUfB19At1c3QOCQ1yVfB3U3D1cXUOCfJ3ASkKBhL-jkEuCiEerkGubv5BPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3ivAw9DQyNzYzMLE0ZgYNQAc-S0f</recordid><startdate>19991008</startdate><enddate>19991008</enddate><creator>HASHIMOTO SATORU</creator><creator>KURATSUKA MAKI</creator><creator>MURAOKA YOSHIYUKI</creator><scope>EVB</scope></search><sort><creationdate>19991008</creationdate><title>ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR</title><author>HASHIMOTO SATORU ; KURATSUKA MAKI ; MURAOKA YOSHIYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH11273684A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1999</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>HASHIMOTO SATORU</creatorcontrib><creatorcontrib>KURATSUKA MAKI</creatorcontrib><creatorcontrib>MURAOKA YOSHIYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HASHIMOTO SATORU</au><au>KURATSUKA MAKI</au><au>MURAOKA YOSHIYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR</title><date>1999-10-08</date><risdate>1999</risdate><abstract>PROBLEM TO BE SOLVED: To restrain corrosion of a nickel sintered base board, to restrain reduction in a strength characteristic of the nickel sintered base board, and to restrain conversion of an active material into γ-NiOOH at charging time by covering the surface of the nickel sintered base board with a mixed oxide layer being mainly composed of cobalt oxide and containing a small quantity of iron oxide. SOLUTION: In a mixed oxide layer, and in the mole ratio of iron oxide to cobalt oxide, when the cobalt oxide is denoted by 100, the iron oxide is 0.5 to 5, and both are desirably uniformly mixed together. Cobalt oxyhydroxide is desirable as the cobalt oxide, and iron hydroxide is desirable as the iron oxide. A nickel sintered base board by forming a sintered body of nickel powder on both surfaces of a metallic core material, is dried at 80 to 150 deg.C after being soaked and impregnated into a mixed salt aqueous solution of a cobalt nitrate and an iron sulfate, and then, is soaked in an alkali aqueous solution to perform oxidation treatment at 100 to 180 deg.C in the air after substituting salt sticking to this base board with hydroxide.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH11273684A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title ALKALINE STORAGE BATTERY AND MANUFACTURE OF ELECTRODE BASE BOARD THEREFOR
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T14%3A35%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HASHIMOTO%20SATORU&rft.date=1999-10-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH11273684A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true