METHOD FOR DESILICONIZING MOLTEN MANGANESE IRON ALLOY
PROBLEM TO BE SOLVED: To lower [Si] in molten manganese iron alloy by executing desiliconizing treatment of molten metal tapped from a blast furnace without lowering [Mn] yield, at the time of producing the molten manganese iron alloy from Mn ore by using the blast furnace and a reducing furnace. SO...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To lower [Si] in molten manganese iron alloy by executing desiliconizing treatment of molten metal tapped from a blast furnace without lowering [Mn] yield, at the time of producing the molten manganese iron alloy from Mn ore by using the blast furnace and a reducing furnace. SOLUTION: At the time of flowing down the molten manganese iron alloy 9 tapped from the blast furnace 1 from the dropping hole of a molten metal tapping trough 2, desiliconizing agent composed of oxidizer containing manganese oxide and/or carbonate of alkaline earth metal and flux containing neither alkali metal compound nor halogen compound or |
---|