COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING

PROBLEM TO BE SOLVED: To obtain the subject composition that can provide molded products having smooth and gloss surfaces by including polyolefin resin, pigment and ionomer resin. SOLUTION: The objective composition is obtained by compounding (A) a polyolefin resin as polyethylene preferably a high-...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SAKUMA KANA, NAKANE IZUMI, IGUCHI AKIYOSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SAKUMA KANA
NAKANE IZUMI
IGUCHI AKIYOSHI
description PROBLEM TO BE SOLVED: To obtain the subject composition that can provide molded products having smooth and gloss surfaces by including polyolefin resin, pigment and ionomer resin. SOLUTION: The objective composition is obtained by compounding (A) a polyolefin resin as polyethylene preferably a high-density or straight-chain low-density polyethylene with a MFR of 0.01-5 g/10 min., (B) pigments, (C) ionomer, namely metal salt of ethylene and unsaturated carboxylic acid polymer, (D) when necessary, metal soap, dispersant selected from medium or low molecular weight polyethylene, antioxidant, ultraviolet absorber. The compounding ratio is preferably, in the case that the pellets are directly subjected to the molding, 100 pts.wt. of the component A, 0.01-10 pts.wt. of the component B, sand 0.001-10 pts.wt. of the component C are used. In the case that the pellent colorant contains a high concentration of pigment 100 pts.wt. of the component A, 0.1-100 pts.wt. of the component B and 0.1-5 pts.wt. of the component C are preferably used.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH111579A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH111579A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH111579A3</originalsourceid><addsrcrecordid>eNrjZNB39vfxD3J1UQhyDfb0U3D29w3wD_YM8fT3U3DzD1JwjQgJCg0G8Xz9fVw8_dx5GFjTEnOKU3mhNDeDvJtriLOHbmpBfnxqcUFicmpeakm8V4CHoaGhqbmlozFhFQCfiiXD</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING</title><source>esp@cenet</source><creator>SAKUMA KANA ; NAKANE IZUMI ; IGUCHI AKIYOSHI</creator><creatorcontrib>SAKUMA KANA ; NAKANE IZUMI ; IGUCHI AKIYOSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To obtain the subject composition that can provide molded products having smooth and gloss surfaces by including polyolefin resin, pigment and ionomer resin. SOLUTION: The objective composition is obtained by compounding (A) a polyolefin resin as polyethylene preferably a high-density or straight-chain low-density polyethylene with a MFR of 0.01-5 g/10 min., (B) pigments, (C) ionomer, namely metal salt of ethylene and unsaturated carboxylic acid polymer, (D) when necessary, metal soap, dispersant selected from medium or low molecular weight polyethylene, antioxidant, ultraviolet absorber. The compounding ratio is preferably, in the case that the pellets are directly subjected to the molding, 100 pts.wt. of the component A, 0.01-10 pts.wt. of the component B, sand 0.001-10 pts.wt. of the component C are used. In the case that the pellent colorant contains a high concentration of pigment 100 pts.wt. of the component A, 0.1-100 pts.wt. of the component B and 0.1-5 pts.wt. of the component C are preferably used.</description><edition>6</edition><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>1999</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990106&amp;DB=EPODOC&amp;CC=JP&amp;NR=H111579A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19990106&amp;DB=EPODOC&amp;CC=JP&amp;NR=H111579A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SAKUMA KANA</creatorcontrib><creatorcontrib>NAKANE IZUMI</creatorcontrib><creatorcontrib>IGUCHI AKIYOSHI</creatorcontrib><title>COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING</title><description>PROBLEM TO BE SOLVED: To obtain the subject composition that can provide molded products having smooth and gloss surfaces by including polyolefin resin, pigment and ionomer resin. SOLUTION: The objective composition is obtained by compounding (A) a polyolefin resin as polyethylene preferably a high-density or straight-chain low-density polyethylene with a MFR of 0.01-5 g/10 min., (B) pigments, (C) ionomer, namely metal salt of ethylene and unsaturated carboxylic acid polymer, (D) when necessary, metal soap, dispersant selected from medium or low molecular weight polyethylene, antioxidant, ultraviolet absorber. The compounding ratio is preferably, in the case that the pellets are directly subjected to the molding, 100 pts.wt. of the component A, 0.01-10 pts.wt. of the component B, sand 0.001-10 pts.wt. of the component C are used. In the case that the pellent colorant contains a high concentration of pigment 100 pts.wt. of the component A, 0.1-100 pts.wt. of the component B and 0.1-5 pts.wt. of the component C are preferably used.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1999</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNB39vfxD3J1UQhyDfb0U3D29w3wD_YM8fT3U3DzD1JwjQgJCg0G8Xz9fVw8_dx5GFjTEnOKU3mhNDeDvJtriLOHbmpBfnxqcUFicmpeakm8V4CHoaGhqbmlozFhFQCfiiXD</recordid><startdate>19990106</startdate><enddate>19990106</enddate><creator>SAKUMA KANA</creator><creator>NAKANE IZUMI</creator><creator>IGUCHI AKIYOSHI</creator><scope>EVB</scope></search><sort><creationdate>19990106</creationdate><title>COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING</title><author>SAKUMA KANA ; NAKANE IZUMI ; IGUCHI AKIYOSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH111579A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1999</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>SAKUMA KANA</creatorcontrib><creatorcontrib>NAKANE IZUMI</creatorcontrib><creatorcontrib>IGUCHI AKIYOSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SAKUMA KANA</au><au>NAKANE IZUMI</au><au>IGUCHI AKIYOSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING</title><date>1999-01-06</date><risdate>1999</risdate><abstract>PROBLEM TO BE SOLVED: To obtain the subject composition that can provide molded products having smooth and gloss surfaces by including polyolefin resin, pigment and ionomer resin. SOLUTION: The objective composition is obtained by compounding (A) a polyolefin resin as polyethylene preferably a high-density or straight-chain low-density polyethylene with a MFR of 0.01-5 g/10 min., (B) pigments, (C) ionomer, namely metal salt of ethylene and unsaturated carboxylic acid polymer, (D) when necessary, metal soap, dispersant selected from medium or low molecular weight polyethylene, antioxidant, ultraviolet absorber. The compounding ratio is preferably, in the case that the pellets are directly subjected to the molding, 100 pts.wt. of the component A, 0.01-10 pts.wt. of the component B, sand 0.001-10 pts.wt. of the component C are used. In the case that the pellent colorant contains a high concentration of pigment 100 pts.wt. of the component A, 0.1-100 pts.wt. of the component B and 0.1-5 pts.wt. of the component C are preferably used.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH111579A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title COLORED RESIN COMPOSITION FOR EXTRUSION MOLDING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T15%3A19%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SAKUMA%20KANA&rft.date=1999-01-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH111579A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true