MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET
PROBLEM TO BE SOLVED: To provide a method of manufacture of a silicon steel sheet excellent in magnetic properties in two directions orthogonal to each other. SOLUTION: A steel, having a composition which contains, by weight, 0.02-0.2% C and in which the contents of Si and Mn satisfy inequalities Si...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | SANO NAOYUKI TOMITA TOSHIRO KAMINOTANI SHIGEO |
description | PROBLEM TO BE SOLVED: To provide a method of manufacture of a silicon steel sheet excellent in magnetic properties in two directions orthogonal to each other. SOLUTION: A steel, having a composition which contains, by weight, 0.02-0.2% C and in which the contents of Si and Mn satisfy inequalities Si(%)+0.5Mn(%)=1.5, and Mn(%)>=0.2, is rolled in two directions orthogonal to each other, by which a steel sheet is prepared. Then, annealing is applied under reduced pressure to the steel sheet by using, as a separation agent at annealing, a substance accelerating decarburization or a substance accelerating decarburization and a substance accelerating Mn removal. Further, rolling in two directions orthogonal to each other is carried out in the α+γ two-phase temp. region and then rolling is performed in one direction in the α-phase temp. region, or, rolling in one direction is carried out in the α+γ two-phase temp. region and then rolling is performed in a direction orthogonal to the rolling direction in the α-phase temp. region. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH1081915A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH1081915A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH1081915A3</originalsourceid><addsrcrecordid>eNrjZDDydfQLdXN0DgkNclXwd1MICfdXcPEMcnUO8fT3c_RRCPb08XT291MIDnF1BfI8XF1DeBhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvFeAh6GBhaGloamjMRFKADmFJqo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET</title><source>esp@cenet</source><creator>SANO NAOYUKI ; TOMITA TOSHIRO ; KAMINOTANI SHIGEO</creator><creatorcontrib>SANO NAOYUKI ; TOMITA TOSHIRO ; KAMINOTANI SHIGEO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method of manufacture of a silicon steel sheet excellent in magnetic properties in two directions orthogonal to each other. SOLUTION: A steel, having a composition which contains, by weight, 0.02-0.2% C and in which the contents of Si and Mn satisfy inequalities Si(%)+0.5Mn(%)<=4, Si(%)-0.5Mn (%)>=1.5, and Mn(%)>=0.2, is rolled in two directions orthogonal to each other, by which a steel sheet is prepared. Then, annealing is applied under reduced pressure to the steel sheet by using, as a separation agent at annealing, a substance accelerating decarburization or a substance accelerating decarburization and a substance accelerating Mn removal. Further, rolling in two directions orthogonal to each other is carried out in the α+γ two-phase temp. region and then rolling is performed in one direction in the α-phase temp. region, or, rolling in one direction is carried out in the α+γ two-phase temp. region and then rolling is performed in a direction orthogonal to the rolling direction in the α-phase temp. region.</description><edition>6</edition><language>eng</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; INDUCTANCES ; MAGNETS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1998</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980331&DB=EPODOC&CC=JP&NR=H1081915A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980331&DB=EPODOC&CC=JP&NR=H1081915A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SANO NAOYUKI</creatorcontrib><creatorcontrib>TOMITA TOSHIRO</creatorcontrib><creatorcontrib>KAMINOTANI SHIGEO</creatorcontrib><title>MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET</title><description>PROBLEM TO BE SOLVED: To provide a method of manufacture of a silicon steel sheet excellent in magnetic properties in two directions orthogonal to each other. SOLUTION: A steel, having a composition which contains, by weight, 0.02-0.2% C and in which the contents of Si and Mn satisfy inequalities Si(%)+0.5Mn(%)<=4, Si(%)-0.5Mn (%)>=1.5, and Mn(%)>=0.2, is rolled in two directions orthogonal to each other, by which a steel sheet is prepared. Then, annealing is applied under reduced pressure to the steel sheet by using, as a separation agent at annealing, a substance accelerating decarburization or a substance accelerating decarburization and a substance accelerating Mn removal. Further, rolling in two directions orthogonal to each other is carried out in the α+γ two-phase temp. region and then rolling is performed in one direction in the α-phase temp. region, or, rolling in one direction is carried out in the α+γ two-phase temp. region and then rolling is performed in a direction orthogonal to the rolling direction in the α-phase temp. region.</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>INDUCTANCES</subject><subject>MAGNETS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1998</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDydfQLdXN0DgkNclXwd1MICfdXcPEMcnUO8fT3c_RRCPb08XT291MIDnF1BfI8XF1DeBhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvFeAh6GBhaGloamjMRFKADmFJqo</recordid><startdate>19980331</startdate><enddate>19980331</enddate><creator>SANO NAOYUKI</creator><creator>TOMITA TOSHIRO</creator><creator>KAMINOTANI SHIGEO</creator><scope>EVB</scope></search><sort><creationdate>19980331</creationdate><title>MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET</title><author>SANO NAOYUKI ; TOMITA TOSHIRO ; KAMINOTANI SHIGEO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH1081915A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1998</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>INDUCTANCES</topic><topic>MAGNETS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SANO NAOYUKI</creatorcontrib><creatorcontrib>TOMITA TOSHIRO</creatorcontrib><creatorcontrib>KAMINOTANI SHIGEO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SANO NAOYUKI</au><au>TOMITA TOSHIRO</au><au>KAMINOTANI SHIGEO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET</title><date>1998-03-31</date><risdate>1998</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method of manufacture of a silicon steel sheet excellent in magnetic properties in two directions orthogonal to each other. SOLUTION: A steel, having a composition which contains, by weight, 0.02-0.2% C and in which the contents of Si and Mn satisfy inequalities Si(%)+0.5Mn(%)<=4, Si(%)-0.5Mn (%)>=1.5, and Mn(%)>=0.2, is rolled in two directions orthogonal to each other, by which a steel sheet is prepared. Then, annealing is applied under reduced pressure to the steel sheet by using, as a separation agent at annealing, a substance accelerating decarburization or a substance accelerating decarburization and a substance accelerating Mn removal. Further, rolling in two directions orthogonal to each other is carried out in the α+γ two-phase temp. region and then rolling is performed in one direction in the α-phase temp. region, or, rolling in one direction is carried out in the α+γ two-phase temp. region and then rolling is performed in a direction orthogonal to the rolling direction in the α-phase temp. region.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JPH1081915A |
source | esp@cenet |
subjects | ALLOYS BASIC ELECTRIC ELEMENTS CHEMISTRY ELECTRICITY FERROUS OR NON-FERROUS ALLOYS GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS INDUCTANCES MAGNETS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES TRANSFORMERS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | MANUFACTURE OF TWO DIRECTIONAL SILICON STEEL SHEET |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-15T14%3A29%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SANO%20NAOYUKI&rft.date=1998-03-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH1081915A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |