MANUFACTURE OF INTERNAL CHILL BODY

PROBLEM TO BE SOLVED: To manufacture an internal chill body having a joining surface of the dimension and shape expected in the design by excellently filing the molten metal in the vicinity of a boundary part of a sand mold and an internal chill. SOLUTION: An internal chilled part 9 of an internal c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KURIKUMA TSUTOMU, AKITA NORIHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KURIKUMA TSUTOMU
AKITA NORIHIRO
description PROBLEM TO BE SOLVED: To manufacture an internal chill body having a joining surface of the dimension and shape expected in the design by excellently filing the molten metal in the vicinity of a boundary part of a sand mold and an internal chill. SOLUTION: An internal chilled part 9 of an internal chill 7 is exposed in a cavity 5 of a sand mold 1 to form a heat storage part 10 projected in the cavity 5 from the sand mold 1 on a connection part of the sand mold 1 to the internal chilled part 9. When the molten metal is poured in the cavity 5, the heat of the molten metal in contact with the heat storage part 10 is stored in the heat storage part 10, and temperature drop of the molten metal in contact with the heat storage part 10 is controlled. Fluidity in the vicinity of the heat storage part 10 is kept excellently, and the molten metal is excellently filled in the vicinity of a boundary part 11 of the heat storage part 10 and the internal chilled part 9, and a joining surface of the size and shape approximately same as those expected in the design is formed between the internal chilled material and the material to be internal chilled in.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH1076358A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH1076358A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH1076358A3</originalsourceid><addsrcrecordid>eNrjZFDydfQLdXN0DgkNclXwd1Pw9AtxDfJz9FFw9vD08VFw8neJ5GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8V4BHoYG5mbGphaOxkQoAQDyzCIs</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MANUFACTURE OF INTERNAL CHILL BODY</title><source>esp@cenet</source><creator>KURIKUMA TSUTOMU ; AKITA NORIHIRO</creator><creatorcontrib>KURIKUMA TSUTOMU ; AKITA NORIHIRO</creatorcontrib><description>PROBLEM TO BE SOLVED: To manufacture an internal chill body having a joining surface of the dimension and shape expected in the design by excellently filing the molten metal in the vicinity of a boundary part of a sand mold and an internal chill. SOLUTION: An internal chilled part 9 of an internal chill 7 is exposed in a cavity 5 of a sand mold 1 to form a heat storage part 10 projected in the cavity 5 from the sand mold 1 on a connection part of the sand mold 1 to the internal chilled part 9. When the molten metal is poured in the cavity 5, the heat of the molten metal in contact with the heat storage part 10 is stored in the heat storage part 10, and temperature drop of the molten metal in contact with the heat storage part 10 is controlled. Fluidity in the vicinity of the heat storage part 10 is kept excellently, and the molten metal is excellently filled in the vicinity of a boundary part 11 of the heat storage part 10 and the internal chilled part 9, and a joining surface of the size and shape approximately same as those expected in the design is formed between the internal chilled material and the material to be internal chilled in.</description><edition>6</edition><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>1998</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19980324&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1076358A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19980324&amp;DB=EPODOC&amp;CC=JP&amp;NR=H1076358A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KURIKUMA TSUTOMU</creatorcontrib><creatorcontrib>AKITA NORIHIRO</creatorcontrib><title>MANUFACTURE OF INTERNAL CHILL BODY</title><description>PROBLEM TO BE SOLVED: To manufacture an internal chill body having a joining surface of the dimension and shape expected in the design by excellently filing the molten metal in the vicinity of a boundary part of a sand mold and an internal chill. SOLUTION: An internal chilled part 9 of an internal chill 7 is exposed in a cavity 5 of a sand mold 1 to form a heat storage part 10 projected in the cavity 5 from the sand mold 1 on a connection part of the sand mold 1 to the internal chilled part 9. When the molten metal is poured in the cavity 5, the heat of the molten metal in contact with the heat storage part 10 is stored in the heat storage part 10, and temperature drop of the molten metal in contact with the heat storage part 10 is controlled. Fluidity in the vicinity of the heat storage part 10 is kept excellently, and the molten metal is excellently filled in the vicinity of a boundary part 11 of the heat storage part 10 and the internal chilled part 9, and a joining surface of the size and shape approximately same as those expected in the design is formed between the internal chilled material and the material to be internal chilled in.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1998</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDydfQLdXN0DgkNclXwd1Pw9AtxDfJz9FFw9vD08VFw8neJ5GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8V4BHoYG5mbGphaOxkQoAQDyzCIs</recordid><startdate>19980324</startdate><enddate>19980324</enddate><creator>KURIKUMA TSUTOMU</creator><creator>AKITA NORIHIRO</creator><scope>EVB</scope></search><sort><creationdate>19980324</creationdate><title>MANUFACTURE OF INTERNAL CHILL BODY</title><author>KURIKUMA TSUTOMU ; AKITA NORIHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH1076358A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1998</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KURIKUMA TSUTOMU</creatorcontrib><creatorcontrib>AKITA NORIHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KURIKUMA TSUTOMU</au><au>AKITA NORIHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MANUFACTURE OF INTERNAL CHILL BODY</title><date>1998-03-24</date><risdate>1998</risdate><abstract>PROBLEM TO BE SOLVED: To manufacture an internal chill body having a joining surface of the dimension and shape expected in the design by excellently filing the molten metal in the vicinity of a boundary part of a sand mold and an internal chill. SOLUTION: An internal chilled part 9 of an internal chill 7 is exposed in a cavity 5 of a sand mold 1 to form a heat storage part 10 projected in the cavity 5 from the sand mold 1 on a connection part of the sand mold 1 to the internal chilled part 9. When the molten metal is poured in the cavity 5, the heat of the molten metal in contact with the heat storage part 10 is stored in the heat storage part 10, and temperature drop of the molten metal in contact with the heat storage part 10 is controlled. Fluidity in the vicinity of the heat storage part 10 is kept excellently, and the molten metal is excellently filled in the vicinity of a boundary part 11 of the heat storage part 10 and the internal chilled part 9, and a joining surface of the size and shape approximately same as those expected in the design is formed between the internal chilled material and the material to be internal chilled in.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH1076358A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title MANUFACTURE OF INTERNAL CHILL BODY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T22%3A26%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KURIKUMA%20TSUTOMU&rft.date=1998-03-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH1076358A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true