METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP

PROBLEM TO BE SOLVED: To provent the occurrence of fine surface flaw at the surface of a hot rolled strip of ferritic stainless steel and to obtain a ferritic stainless steel minimal in surface flaw. SOLUTION: After 2.5-15% working strain is applied to a slab of ferritic stainless steel at 300-900 d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TSUCHINAGA MASAMITSU, SUMITOMO HIDEHIKO, KURE YUKIHIRO, ABE SEISABURO, YAMAJI KIYOSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TSUCHINAGA MASAMITSU
SUMITOMO HIDEHIKO
KURE YUKIHIRO
ABE SEISABURO
YAMAJI KIYOSHI
description PROBLEM TO BE SOLVED: To provent the occurrence of fine surface flaw at the surface of a hot rolled strip of ferritic stainless steel and to obtain a ferritic stainless steel minimal in surface flaw. SOLUTION: After 2.5-15% working strain is applied to a slab of ferritic stainless steel at 300-900 deg.C, the slab is heated to 1100-1300 deg.C to regulate the crystalline grain size in the surface layer part of the slab before hot rolling to
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH0925516A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH0925516A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH0925516A3</originalsourceid><addsrcrecordid>eNrjZPD3dQ3x8HdRcPMPUggIcg1z9Qvx9HNXCA4NcnN0dlVw83EMV_B3U_DwD1EI8vfxcQWqdA0K8gzxdFYIDnH09PNxDQ4GslxdfYBkkGcADwNrWmJOcSovlOZmAGoIcfbQTS3Ij08tLkhMTs1LLYn3CvAwsDQyNTU0czQmQgkA9Ckuqg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP</title><source>esp@cenet</source><creator>TSUCHINAGA MASAMITSU ; SUMITOMO HIDEHIKO ; KURE YUKIHIRO ; ABE SEISABURO ; YAMAJI KIYOSHI</creator><creatorcontrib>TSUCHINAGA MASAMITSU ; SUMITOMO HIDEHIKO ; KURE YUKIHIRO ; ABE SEISABURO ; YAMAJI KIYOSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provent the occurrence of fine surface flaw at the surface of a hot rolled strip of ferritic stainless steel and to obtain a ferritic stainless steel minimal in surface flaw. SOLUTION: After 2.5-15% working strain is applied to a slab of ferritic stainless steel at 300-900 deg.C, the slab is heated to 1100-1300 deg.C to regulate the crystalline grain size in the surface layer part of the slab before hot rolling to &lt;=5mm, by which the occurrence of surface flaw at the surface of hot rolled ferritic stainless steel strip can be prevented.</description><edition>6</edition><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1997</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970128&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0925516A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970128&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0925516A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TSUCHINAGA MASAMITSU</creatorcontrib><creatorcontrib>SUMITOMO HIDEHIKO</creatorcontrib><creatorcontrib>KURE YUKIHIRO</creatorcontrib><creatorcontrib>ABE SEISABURO</creatorcontrib><creatorcontrib>YAMAJI KIYOSHI</creatorcontrib><title>METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP</title><description>PROBLEM TO BE SOLVED: To provent the occurrence of fine surface flaw at the surface of a hot rolled strip of ferritic stainless steel and to obtain a ferritic stainless steel minimal in surface flaw. SOLUTION: After 2.5-15% working strain is applied to a slab of ferritic stainless steel at 300-900 deg.C, the slab is heated to 1100-1300 deg.C to regulate the crystalline grain size in the surface layer part of the slab before hot rolling to &lt;=5mm, by which the occurrence of surface flaw at the surface of hot rolled ferritic stainless steel strip can be prevented.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1997</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPD3dQ3x8HdRcPMPUggIcg1z9Qvx9HNXCA4NcnN0dlVw83EMV_B3U_DwD1EI8vfxcQWqdA0K8gzxdFYIDnH09PNxDQ4GslxdfYBkkGcADwNrWmJOcSovlOZmAGoIcfbQTS3Ij08tLkhMTs1LLYn3CvAwsDQyNTU0czQmQgkA9Ckuqg</recordid><startdate>19970128</startdate><enddate>19970128</enddate><creator>TSUCHINAGA MASAMITSU</creator><creator>SUMITOMO HIDEHIKO</creator><creator>KURE YUKIHIRO</creator><creator>ABE SEISABURO</creator><creator>YAMAJI KIYOSHI</creator><scope>EVB</scope></search><sort><creationdate>19970128</creationdate><title>METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP</title><author>TSUCHINAGA MASAMITSU ; SUMITOMO HIDEHIKO ; KURE YUKIHIRO ; ABE SEISABURO ; YAMAJI KIYOSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH0925516A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1997</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>TSUCHINAGA MASAMITSU</creatorcontrib><creatorcontrib>SUMITOMO HIDEHIKO</creatorcontrib><creatorcontrib>KURE YUKIHIRO</creatorcontrib><creatorcontrib>ABE SEISABURO</creatorcontrib><creatorcontrib>YAMAJI KIYOSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TSUCHINAGA MASAMITSU</au><au>SUMITOMO HIDEHIKO</au><au>KURE YUKIHIRO</au><au>ABE SEISABURO</au><au>YAMAJI KIYOSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP</title><date>1997-01-28</date><risdate>1997</risdate><abstract>PROBLEM TO BE SOLVED: To provent the occurrence of fine surface flaw at the surface of a hot rolled strip of ferritic stainless steel and to obtain a ferritic stainless steel minimal in surface flaw. SOLUTION: After 2.5-15% working strain is applied to a slab of ferritic stainless steel at 300-900 deg.C, the slab is heated to 1100-1300 deg.C to regulate the crystalline grain size in the surface layer part of the slab before hot rolling to &lt;=5mm, by which the occurrence of surface flaw at the surface of hot rolled ferritic stainless steel strip can be prevented.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH0925516A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR PREVENTING SURFACE FLAW OF HOT ROLLED FERRITIC STAINLESS STEEL STRIP
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T09%3A20%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TSUCHINAGA%20MASAMITSU&rft.date=1997-01-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH0925516A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true