SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF

PURPOSE: To obtain a sintered compact of silicon nitride which has mechanical properties sufficient to be used as a part for motor vehicles from room temperature up to elevated one and parts for a gas turbine engine, particularly excellent in flexural strength at from room temperature to 1,000 deg.C...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SATO MASAHIRO, FUKUTOME TAKEO, HAMADA NORIAKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SATO MASAHIRO
FUKUTOME TAKEO
HAMADA NORIAKI
description PURPOSE: To obtain a sintered compact of silicon nitride which has mechanical properties sufficient to be used as a part for motor vehicles from room temperature up to elevated one and parts for a gas turbine engine, particularly excellent in flexural strength at from room temperature to 1,000 deg.C. CONSTITUTION: This sintered compact of silicon nitride comprises the main phase of β-silicon nitride crystals and the grain boundary phase containing rare-earth elements, silicon, aluminum, oxygen and nitrogen where Si2 N2 O particles of 5-20μm average particle size are dispersed in the grain boundary phase. A molded compact containing, as auxiliary components, 1-10wt.% silicon oxide of less than 3μm average particle size together with rare earth element oxides and aluminum oxide is heated at 800-1,400 deg.C under a reduced pressure lower than 10Torr to precipitate Si2 N2 O particles, then sintered at 1,600-1,900 deg.C in a non-oxidizing atmosphere.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH0867566A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH0867566A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH0867566A3</originalsourceid><addsrcrecordid>eNrjZDAP9vTxdPb3U_DzDAnydHFVCPb0C3ENcnVRcPb3DXB0DlFw9HNRCAjydwl1DvEEqgvxAMr6u_EwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUknivAA8DCzNzUzMzR2MilAAAA3AoNg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF</title><source>esp@cenet</source><creator>SATO MASAHIRO ; FUKUTOME TAKEO ; HAMADA NORIAKI</creator><creatorcontrib>SATO MASAHIRO ; FUKUTOME TAKEO ; HAMADA NORIAKI</creatorcontrib><description>PURPOSE: To obtain a sintered compact of silicon nitride which has mechanical properties sufficient to be used as a part for motor vehicles from room temperature up to elevated one and parts for a gas turbine engine, particularly excellent in flexural strength at from room temperature to 1,000 deg.C. CONSTITUTION: This sintered compact of silicon nitride comprises the main phase of β-silicon nitride crystals and the grain boundary phase containing rare-earth elements, silicon, aluminum, oxygen and nitrogen where Si2 N2 O particles of 5-20μm average particle size are dispersed in the grain boundary phase. A molded compact containing, as auxiliary components, 1-10wt.% silicon oxide of less than 3μm average particle size together with rare earth element oxides and aluminum oxide is heated at 800-1,400 deg.C under a reduced pressure lower than 10Torr to precipitate Si2 N2 O particles, then sintered at 1,600-1,900 deg.C in a non-oxidizing atmosphere.</description><edition>6</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960312&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0867566A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960312&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0867566A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SATO MASAHIRO</creatorcontrib><creatorcontrib>FUKUTOME TAKEO</creatorcontrib><creatorcontrib>HAMADA NORIAKI</creatorcontrib><title>SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF</title><description>PURPOSE: To obtain a sintered compact of silicon nitride which has mechanical properties sufficient to be used as a part for motor vehicles from room temperature up to elevated one and parts for a gas turbine engine, particularly excellent in flexural strength at from room temperature to 1,000 deg.C. CONSTITUTION: This sintered compact of silicon nitride comprises the main phase of β-silicon nitride crystals and the grain boundary phase containing rare-earth elements, silicon, aluminum, oxygen and nitrogen where Si2 N2 O particles of 5-20μm average particle size are dispersed in the grain boundary phase. A molded compact containing, as auxiliary components, 1-10wt.% silicon oxide of less than 3μm average particle size together with rare earth element oxides and aluminum oxide is heated at 800-1,400 deg.C under a reduced pressure lower than 10Torr to precipitate Si2 N2 O particles, then sintered at 1,600-1,900 deg.C in a non-oxidizing atmosphere.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAP9vTxdPb3U_DzDAnydHFVCPb0C3ENcnVRcPb3DXB0DlFw9HNRCAjydwl1DvEEqgvxAMr6u_EwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTigsTk1LzUknivAA8DCzNzUzMzR2MilAAAA3AoNg</recordid><startdate>19960312</startdate><enddate>19960312</enddate><creator>SATO MASAHIRO</creator><creator>FUKUTOME TAKEO</creator><creator>HAMADA NORIAKI</creator><scope>EVB</scope></search><sort><creationdate>19960312</creationdate><title>SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF</title><author>SATO MASAHIRO ; FUKUTOME TAKEO ; HAMADA NORIAKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH0867566A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1996</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SATO MASAHIRO</creatorcontrib><creatorcontrib>FUKUTOME TAKEO</creatorcontrib><creatorcontrib>HAMADA NORIAKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SATO MASAHIRO</au><au>FUKUTOME TAKEO</au><au>HAMADA NORIAKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF</title><date>1996-03-12</date><risdate>1996</risdate><abstract>PURPOSE: To obtain a sintered compact of silicon nitride which has mechanical properties sufficient to be used as a part for motor vehicles from room temperature up to elevated one and parts for a gas turbine engine, particularly excellent in flexural strength at from room temperature to 1,000 deg.C. CONSTITUTION: This sintered compact of silicon nitride comprises the main phase of β-silicon nitride crystals and the grain boundary phase containing rare-earth elements, silicon, aluminum, oxygen and nitrogen where Si2 N2 O particles of 5-20μm average particle size are dispersed in the grain boundary phase. A molded compact containing, as auxiliary components, 1-10wt.% silicon oxide of less than 3μm average particle size together with rare earth element oxides and aluminum oxide is heated at 800-1,400 deg.C under a reduced pressure lower than 10Torr to precipitate Si2 N2 O particles, then sintered at 1,600-1,900 deg.C in a non-oxidizing atmosphere.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH0867566A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title SILICON NITRIDE SINTERED COMPACT AND PRODUCTION THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-05T11%3A20%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SATO%20MASAHIRO&rft.date=1996-03-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH0867566A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true