CEMENT COMPOSITION

PURPOSE:To improve compression strength and flexural strength at an early period, a middle period and a long period, comprising specific cement, anhydrous gypsum, aluminum sulfate, an alkali metal aluminate and steel fibers. CONSTITUTION:100 pts.wt. of cement composed of >=60wt.% of 3CaO.SiO2, ha...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MORIOKA MINORU, NIKAIDO YASUYUKI, MIHARA TOSHIO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MORIOKA MINORU
NIKAIDO YASUYUKI
MIHARA TOSHIO
description PURPOSE:To improve compression strength and flexural strength at an early period, a middle period and a long period, comprising specific cement, anhydrous gypsum, aluminum sulfate, an alkali metal aluminate and steel fibers. CONSTITUTION:100 pts.wt. of cement composed of >=60wt.% of 3CaO.SiO2, having 3,500-7,000cm /g Blaine value is blended with 100 pts.wt. of total amount of 1-5 pts.wt. of anhydrous gypsum having 2,500cm /g Blaine value, 0.2-3 pts.wt. (calculated as anhydride) of aluminum sulfate and 0.1-0.8 pt.wt. of an alkali metal aluminate and 5-25 pts.wt. of steel fibers having 29-80mm fiber length and 50-100 aspect ratio.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH07247153A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH07247153A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH07247153A3</originalsourceid><addsrcrecordid>eNrjZBBydvV19QtRcPb3DfAP9gzx9PfjYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgEeBuZGJuaGpsaOxsSoAQBObR5l</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CEMENT COMPOSITION</title><source>esp@cenet</source><creator>MORIOKA MINORU ; NIKAIDO YASUYUKI ; MIHARA TOSHIO</creator><creatorcontrib>MORIOKA MINORU ; NIKAIDO YASUYUKI ; MIHARA TOSHIO</creatorcontrib><description>PURPOSE:To improve compression strength and flexural strength at an early period, a middle period and a long period, comprising specific cement, anhydrous gypsum, aluminum sulfate, an alkali metal aluminate and steel fibers. CONSTITUTION:100 pts.wt. of cement composed of &gt;=60wt.% of 3CaO.SiO2, having 3,500-7,000cm /g Blaine value is blended with 100 pts.wt. of total amount of 1-5 pts.wt. of anhydrous gypsum having 2,500cm /g Blaine value, 0.2-3 pts.wt. (calculated as anhydride) of aluminum sulfate and 0.1-0.8 pt.wt. of an alkali metal aluminate and 5-25 pts.wt. of steel fibers having 29-80mm fiber length and 50-100 aspect ratio.</description><edition>6</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1995</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19950926&amp;DB=EPODOC&amp;CC=JP&amp;NR=H07247153A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19950926&amp;DB=EPODOC&amp;CC=JP&amp;NR=H07247153A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MORIOKA MINORU</creatorcontrib><creatorcontrib>NIKAIDO YASUYUKI</creatorcontrib><creatorcontrib>MIHARA TOSHIO</creatorcontrib><title>CEMENT COMPOSITION</title><description>PURPOSE:To improve compression strength and flexural strength at an early period, a middle period and a long period, comprising specific cement, anhydrous gypsum, aluminum sulfate, an alkali metal aluminate and steel fibers. CONSTITUTION:100 pts.wt. of cement composed of &gt;=60wt.% of 3CaO.SiO2, having 3,500-7,000cm /g Blaine value is blended with 100 pts.wt. of total amount of 1-5 pts.wt. of anhydrous gypsum having 2,500cm /g Blaine value, 0.2-3 pts.wt. (calculated as anhydride) of aluminum sulfate and 0.1-0.8 pt.wt. of an alkali metal aluminate and 5-25 pts.wt. of steel fibers having 29-80mm fiber length and 50-100 aspect ratio.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1995</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBBydvV19QtRcPb3DfAP9gzx9PfjYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgEeBuZGJuaGpsaOxsSoAQBObR5l</recordid><startdate>19950926</startdate><enddate>19950926</enddate><creator>MORIOKA MINORU</creator><creator>NIKAIDO YASUYUKI</creator><creator>MIHARA TOSHIO</creator><scope>EVB</scope></search><sort><creationdate>19950926</creationdate><title>CEMENT COMPOSITION</title><author>MORIOKA MINORU ; NIKAIDO YASUYUKI ; MIHARA TOSHIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH07247153A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1995</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>MORIOKA MINORU</creatorcontrib><creatorcontrib>NIKAIDO YASUYUKI</creatorcontrib><creatorcontrib>MIHARA TOSHIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MORIOKA MINORU</au><au>NIKAIDO YASUYUKI</au><au>MIHARA TOSHIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CEMENT COMPOSITION</title><date>1995-09-26</date><risdate>1995</risdate><abstract>PURPOSE:To improve compression strength and flexural strength at an early period, a middle period and a long period, comprising specific cement, anhydrous gypsum, aluminum sulfate, an alkali metal aluminate and steel fibers. CONSTITUTION:100 pts.wt. of cement composed of &gt;=60wt.% of 3CaO.SiO2, having 3,500-7,000cm /g Blaine value is blended with 100 pts.wt. of total amount of 1-5 pts.wt. of anhydrous gypsum having 2,500cm /g Blaine value, 0.2-3 pts.wt. (calculated as anhydride) of aluminum sulfate and 0.1-0.8 pt.wt. of an alkali metal aluminate and 5-25 pts.wt. of steel fibers having 29-80mm fiber length and 50-100 aspect ratio.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH07247153A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title CEMENT COMPOSITION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T23%3A30%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MORIOKA%20MINORU&rft.date=1995-09-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH07247153A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true