METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION

PURPOSE:To prevent the development of center segregation and center porosity at the time of continuously casting a rectangular cast slab. CONSTITUTION:A flatness ratio of the cast slab 1 is made to be >=1.1. Rolling reduction terminals 4 are arranged at the position (y) satisfying the inequality...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUSANO YOSHIAKI, ISOBE KOICHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUSANO YOSHIAKI
ISOBE KOICHI
description PURPOSE:To prevent the development of center segregation and center porosity at the time of continuously casting a rectangular cast slab. CONSTITUTION:A flatness ratio of the cast slab 1 is made to be >=1.1. Rolling reduction terminals 4 are arranged at the position (y) satisfying the inequality I or the inequality II. Casting velocity is adjusted and the solid phase ratio at the center part in the cross section of the cast slab 1 at the inlet side of the rolling reduction terminals 4 is made to be 0.6-0.95. The rolling reduction terminal 4 having >=200mm radius of curvature in the axial direction of the cast slab at the part executing the rolling reduction to the cast slab 1 is used, and the cast slab is drafted in 5-40% draft in the thickness direction of the cast slab 1 at 80-540mm/min rolling reduction speed. Then, the inquality I and the inquality II are expressed as follows, in the case of 0
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH07227657A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH07227657A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH07227657A3</originalsourceid><addsrcrecordid>eNqNjEsKwkAQBbNxIeod2gMIEtGsJ_NJWibdOh8hqxBkXIkGkvujAQ_gqhavXi2zqdGhZgWGHWBzcXxDqgCJtINrFBZDC2xAMgWkyNHbFqTwAbwVJZQtWOEqDY6tnY9OqygDMkEk9U1E8mxRoUGt5ojCeVxni0f_HNPmx1W2NTrIepeGd5fGob-nV5q686XeF3lenI6FOPzjfAD4LzmZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION</title><source>esp@cenet</source><creator>KUSANO YOSHIAKI ; ISOBE KOICHI</creator><creatorcontrib>KUSANO YOSHIAKI ; ISOBE KOICHI</creatorcontrib><description><![CDATA[PURPOSE:To prevent the development of center segregation and center porosity at the time of continuously casting a rectangular cast slab. CONSTITUTION:A flatness ratio of the cast slab 1 is made to be >=1.1. Rolling reduction terminals 4 are arranged at the position (y) satisfying the inequality I or the inequality II. Casting velocity is adjusted and the solid phase ratio at the center part in the cross section of the cast slab 1 at the inlet side of the rolling reduction terminals 4 is made to be 0.6-0.95. The rolling reduction terminal 4 having >=200mm radius of curvature in the axial direction of the cast slab at the part executing the rolling reduction to the cast slab 1 is used, and the cast slab is drafted in 5-40% draft in the thickness direction of the cast slab 1 at 80-540mm/min rolling reduction speed. Then, the inquality I and the inquality II are expressed as follows, in the case of 0<=D<250, 0.02XD<=y (m) <=0.06XD...(1) and in the case of 250<=D, 0.02XD<=y (m) <=0.067X(D-250)+15...(II). Wherein, D: thickness of the cast slab (mm).]]></description><edition>6</edition><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>1995</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19950829&amp;DB=EPODOC&amp;CC=JP&amp;NR=H07227657A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19950829&amp;DB=EPODOC&amp;CC=JP&amp;NR=H07227657A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUSANO YOSHIAKI</creatorcontrib><creatorcontrib>ISOBE KOICHI</creatorcontrib><title>METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION</title><description><![CDATA[PURPOSE:To prevent the development of center segregation and center porosity at the time of continuously casting a rectangular cast slab. CONSTITUTION:A flatness ratio of the cast slab 1 is made to be >=1.1. Rolling reduction terminals 4 are arranged at the position (y) satisfying the inequality I or the inequality II. Casting velocity is adjusted and the solid phase ratio at the center part in the cross section of the cast slab 1 at the inlet side of the rolling reduction terminals 4 is made to be 0.6-0.95. The rolling reduction terminal 4 having >=200mm radius of curvature in the axial direction of the cast slab at the part executing the rolling reduction to the cast slab 1 is used, and the cast slab is drafted in 5-40% draft in the thickness direction of the cast slab 1 at 80-540mm/min rolling reduction speed. Then, the inquality I and the inquality II are expressed as follows, in the case of 0<=D<250, 0.02XD<=y (m) <=0.06XD...(1) and in the case of 250<=D, 0.02XD<=y (m) <=0.067X(D-250)+15...(II). Wherein, D: thickness of the cast slab (mm).]]></description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1995</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEsKwkAQBbNxIeod2gMIEtGsJ_NJWibdOh8hqxBkXIkGkvujAQ_gqhavXi2zqdGhZgWGHWBzcXxDqgCJtINrFBZDC2xAMgWkyNHbFqTwAbwVJZQtWOEqDY6tnY9OqygDMkEk9U1E8mxRoUGt5ojCeVxni0f_HNPmx1W2NTrIepeGd5fGob-nV5q686XeF3lenI6FOPzjfAD4LzmZ</recordid><startdate>19950829</startdate><enddate>19950829</enddate><creator>KUSANO YOSHIAKI</creator><creator>ISOBE KOICHI</creator><scope>EVB</scope></search><sort><creationdate>19950829</creationdate><title>METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION</title><author>KUSANO YOSHIAKI ; ISOBE KOICHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH07227657A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1995</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KUSANO YOSHIAKI</creatorcontrib><creatorcontrib>ISOBE KOICHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUSANO YOSHIAKI</au><au>ISOBE KOICHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION</title><date>1995-08-29</date><risdate>1995</risdate><abstract><![CDATA[PURPOSE:To prevent the development of center segregation and center porosity at the time of continuously casting a rectangular cast slab. CONSTITUTION:A flatness ratio of the cast slab 1 is made to be >=1.1. Rolling reduction terminals 4 are arranged at the position (y) satisfying the inequality I or the inequality II. Casting velocity is adjusted and the solid phase ratio at the center part in the cross section of the cast slab 1 at the inlet side of the rolling reduction terminals 4 is made to be 0.6-0.95. The rolling reduction terminal 4 having >=200mm radius of curvature in the axial direction of the cast slab at the part executing the rolling reduction to the cast slab 1 is used, and the cast slab is drafted in 5-40% draft in the thickness direction of the cast slab 1 at 80-540mm/min rolling reduction speed. Then, the inquality I and the inquality II are expressed as follows, in the case of 0<=D<250, 0.02XD<=y (m) <=0.06XD...(1) and in the case of 250<=D, 0.02XD<=y (m) <=0.067X(D-250)+15...(II). Wherein, D: thickness of the cast slab (mm).]]></abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH07227657A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title METHOD FOR IMPROVING INNER QUALITY OF CONTINUOUSLY CAST SLAB BY LARGE ROLLING REDUCTION UNDER UNSOLIDIFIED CONDITION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T10%3A01%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUSANO%20YOSHIAKI&rft.date=1995-08-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH07227657A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true