SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF

PURPOSE:To easily lower a heat of hydration and improve strength development by compounding SiO2, Al2, Fe2O3 and CaO at the ratios to make a composition in a specified range. CONSTITUTION:SiO2 is expressed as S, Al2O3 as A, Fe2O3 as F, CaO as C and 3A+2.25F as X. S, A, F and C are compounded as main...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SAITO TETSUO, ASAKURA ETSURO, NAKANAGA HIDEHIKO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SAITO TETSUO
ASAKURA ETSURO
NAKANAGA HIDEHIKO
description PURPOSE:To easily lower a heat of hydration and improve strength development by compounding SiO2, Al2, Fe2O3 and CaO at the ratios to make a composition in a specified range. CONSTITUTION:SiO2 is expressed as S, Al2O3 as A, Fe2O3 as F, CaO as C and 3A+2.25F as X. S, A, F and C are compounded as main components. The objective super low exothermic cement clinker is obtained by burning a raw material mixture which has the composition, after burning, in the region confined with the surfaces, etc., of a solid formed by connecting point a (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.576), point b (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.925), point c (C3S is 30wt.%, X is 20wt.%, C3A/C4(AF is 0.576), point d (C3S is 30wt.%, X is 20wt.%, C3A/C4AF is 0.925), point e (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.576), point f (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.925), point g (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.576) and point h (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.925).
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH06279074A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH06279074A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH06279074A3</originalsourceid><addsrcrecordid>eNrjZLAPDg1wDVLw8Q9XcI3wD_FwDfL1dFZwdvV19QtRcPbx9PMGyjr6ucCEAoL8XUKdXV0UQEpd_d14GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8V4CHgZmRuaWBuYmjMTFqAIjEKp0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF</title><source>esp@cenet</source><creator>SAITO TETSUO ; ASAKURA ETSURO ; NAKANAGA HIDEHIKO</creator><creatorcontrib>SAITO TETSUO ; ASAKURA ETSURO ; NAKANAGA HIDEHIKO</creatorcontrib><description>PURPOSE:To easily lower a heat of hydration and improve strength development by compounding SiO2, Al2, Fe2O3 and CaO at the ratios to make a composition in a specified range. CONSTITUTION:SiO2 is expressed as S, Al2O3 as A, Fe2O3 as F, CaO as C and 3A+2.25F as X. S, A, F and C are compounded as main components. The objective super low exothermic cement clinker is obtained by burning a raw material mixture which has the composition, after burning, in the region confined with the surfaces, etc., of a solid formed by connecting point a (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.576), point b (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.925), point c (C3S is 30wt.%, X is 20wt.%, C3A/C4(AF is 0.576), point d (C3S is 30wt.%, X is 20wt.%, C3A/C4AF is 0.925), point e (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.576), point f (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.925), point g (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.576) and point h (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.925).</description><edition>5</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1994</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19941004&amp;DB=EPODOC&amp;CC=JP&amp;NR=H06279074A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19941004&amp;DB=EPODOC&amp;CC=JP&amp;NR=H06279074A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SAITO TETSUO</creatorcontrib><creatorcontrib>ASAKURA ETSURO</creatorcontrib><creatorcontrib>NAKANAGA HIDEHIKO</creatorcontrib><title>SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF</title><description>PURPOSE:To easily lower a heat of hydration and improve strength development by compounding SiO2, Al2, Fe2O3 and CaO at the ratios to make a composition in a specified range. CONSTITUTION:SiO2 is expressed as S, Al2O3 as A, Fe2O3 as F, CaO as C and 3A+2.25F as X. S, A, F and C are compounded as main components. The objective super low exothermic cement clinker is obtained by burning a raw material mixture which has the composition, after burning, in the region confined with the surfaces, etc., of a solid formed by connecting point a (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.576), point b (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.925), point c (C3S is 30wt.%, X is 20wt.%, C3A/C4(AF is 0.576), point d (C3S is 30wt.%, X is 20wt.%, C3A/C4AF is 0.925), point e (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.576), point f (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.925), point g (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.576) and point h (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.925).</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1994</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAPDg1wDVLw8Q9XcI3wD_FwDfL1dFZwdvV19QtRcPbx9PMGyjr6ucCEAoL8XUKdXV0UQEpd_d14GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8V4CHgZmRuaWBuYmjMTFqAIjEKp0</recordid><startdate>19941004</startdate><enddate>19941004</enddate><creator>SAITO TETSUO</creator><creator>ASAKURA ETSURO</creator><creator>NAKANAGA HIDEHIKO</creator><scope>EVB</scope></search><sort><creationdate>19941004</creationdate><title>SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF</title><author>SAITO TETSUO ; ASAKURA ETSURO ; NAKANAGA HIDEHIKO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH06279074A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1994</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SAITO TETSUO</creatorcontrib><creatorcontrib>ASAKURA ETSURO</creatorcontrib><creatorcontrib>NAKANAGA HIDEHIKO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SAITO TETSUO</au><au>ASAKURA ETSURO</au><au>NAKANAGA HIDEHIKO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF</title><date>1994-10-04</date><risdate>1994</risdate><abstract>PURPOSE:To easily lower a heat of hydration and improve strength development by compounding SiO2, Al2, Fe2O3 and CaO at the ratios to make a composition in a specified range. CONSTITUTION:SiO2 is expressed as S, Al2O3 as A, Fe2O3 as F, CaO as C and 3A+2.25F as X. S, A, F and C are compounded as main components. The objective super low exothermic cement clinker is obtained by burning a raw material mixture which has the composition, after burning, in the region confined with the surfaces, etc., of a solid formed by connecting point a (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.576), point b (C3S is 10wt.%, X is 20wt.%, C3A/C4AF is 0.925), point c (C3S is 30wt.%, X is 20wt.%, C3A/C4(AF is 0.576), point d (C3S is 30wt.%, X is 20wt.%, C3A/C4AF is 0.925), point e (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.576), point f (C3S is 10wt.%, X is 5wt.%, C3A/C4AF is 0.925), point g (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.576) and point h (C3S is 60wt.%, X is 5wt.%, C3A/C4AF is 0.925).</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH06279074A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title SUPER LOW EXOTHERMIC CEMENT CLINKER AND CEMENT PRODUCED THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-15T06%3A35%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SAITO%20TETSUO&rft.date=1994-10-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH06279074A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true