PRODUCTION OF CASTING PIG IRON

PURPOSE:To prevent the generation of bad shaped appearance of a mold pig iron by using steam having the specific value or lower of droplet diameter, cooling with atomized water spreading and making the specific temp. or lower of super heat at near surface layer of molten pig iron in the mold before...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SATO TADASHI, SUZUKI HIDEYUKI, KAMAKARI HIROYUKI, ABE YUKIMASA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SATO TADASHI
SUZUKI HIDEYUKI
KAMAKARI HIROYUKI
ABE YUKIMASA
description PURPOSE:To prevent the generation of bad shaped appearance of a mold pig iron by using steam having the specific value or lower of droplet diameter, cooling with atomized water spreading and making the specific temp. or lower of super heat at near surface layer of molten pig iron in the mold before cooling with much water spraying. CONSTITUTION:In this invention, the super heat at near the surface layer of molten pig iron in the mold before cooling with water spreading is made to be >=50 deg.C. In the case of the general casting pig iron, this can apply the well- known cooling method, but in the case of high Si pig iron having >=2.0% Si, as this solidifying temp. is low, the case, which can not cool to the prescribed temp., is developed. In this case, in this invention, by colliding atomized water particles having very fine, such as
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH0481246A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH0481246A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH0481246A3</originalsourceid><addsrcrecordid>eNrjZJALCPJ3CXUO8fT3U_B3U3B2DA7x9HNXCPB0V_AM8vfjYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxXgEeBiYWhkYmZo7GRCgBAHPRIRQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION OF CASTING PIG IRON</title><source>esp@cenet</source><creator>SATO TADASHI ; SUZUKI HIDEYUKI ; KAMAKARI HIROYUKI ; ABE YUKIMASA</creator><creatorcontrib>SATO TADASHI ; SUZUKI HIDEYUKI ; KAMAKARI HIROYUKI ; ABE YUKIMASA</creatorcontrib><description>PURPOSE:To prevent the generation of bad shaped appearance of a mold pig iron by using steam having the specific value or lower of droplet diameter, cooling with atomized water spreading and making the specific temp. or lower of super heat at near surface layer of molten pig iron in the mold before cooling with much water spraying. CONSTITUTION:In this invention, the super heat at near the surface layer of molten pig iron in the mold before cooling with water spreading is made to be &gt;=50 deg.C. In the case of the general casting pig iron, this can apply the well- known cooling method, but in the case of high Si pig iron having &gt;=2.0% Si, as this solidifying temp. is low, the case, which can not cool to the prescribed temp., is developed. In this case, in this invention, by colliding atomized water particles having very fine, such as &lt;=20mum particle size, to a material to be cooled with the air force, sensible heat according to the vaporization of water particles, is utilized. By this method, as the surface of molding pig iron is scarcely wetted and cooling capacity as the same degree as the ordinary water spraying, is obtd., cooling water is not invaded into inner part of the molded pig iron and the bad appearance is not developed.</description><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>1992</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19920313&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0481246A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19920313&amp;DB=EPODOC&amp;CC=JP&amp;NR=H0481246A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SATO TADASHI</creatorcontrib><creatorcontrib>SUZUKI HIDEYUKI</creatorcontrib><creatorcontrib>KAMAKARI HIROYUKI</creatorcontrib><creatorcontrib>ABE YUKIMASA</creatorcontrib><title>PRODUCTION OF CASTING PIG IRON</title><description>PURPOSE:To prevent the generation of bad shaped appearance of a mold pig iron by using steam having the specific value or lower of droplet diameter, cooling with atomized water spreading and making the specific temp. or lower of super heat at near surface layer of molten pig iron in the mold before cooling with much water spraying. CONSTITUTION:In this invention, the super heat at near the surface layer of molten pig iron in the mold before cooling with water spreading is made to be &gt;=50 deg.C. In the case of the general casting pig iron, this can apply the well- known cooling method, but in the case of high Si pig iron having &gt;=2.0% Si, as this solidifying temp. is low, the case, which can not cool to the prescribed temp., is developed. In this case, in this invention, by colliding atomized water particles having very fine, such as &lt;=20mum particle size, to a material to be cooled with the air force, sensible heat according to the vaporization of water particles, is utilized. By this method, as the surface of molding pig iron is scarcely wetted and cooling capacity as the same degree as the ordinary water spraying, is obtd., cooling water is not invaded into inner part of the molded pig iron and the bad appearance is not developed.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1992</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJALCPJ3CXUO8fT3U_B3U3B2DA7x9HNXCPB0V_AM8vfjYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxXgEeBiYWhkYmZo7GRCgBAHPRIRQ</recordid><startdate>19920313</startdate><enddate>19920313</enddate><creator>SATO TADASHI</creator><creator>SUZUKI HIDEYUKI</creator><creator>KAMAKARI HIROYUKI</creator><creator>ABE YUKIMASA</creator><scope>EVB</scope></search><sort><creationdate>19920313</creationdate><title>PRODUCTION OF CASTING PIG IRON</title><author>SATO TADASHI ; SUZUKI HIDEYUKI ; KAMAKARI HIROYUKI ; ABE YUKIMASA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH0481246A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1992</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>SATO TADASHI</creatorcontrib><creatorcontrib>SUZUKI HIDEYUKI</creatorcontrib><creatorcontrib>KAMAKARI HIROYUKI</creatorcontrib><creatorcontrib>ABE YUKIMASA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SATO TADASHI</au><au>SUZUKI HIDEYUKI</au><au>KAMAKARI HIROYUKI</au><au>ABE YUKIMASA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION OF CASTING PIG IRON</title><date>1992-03-13</date><risdate>1992</risdate><abstract>PURPOSE:To prevent the generation of bad shaped appearance of a mold pig iron by using steam having the specific value or lower of droplet diameter, cooling with atomized water spreading and making the specific temp. or lower of super heat at near surface layer of molten pig iron in the mold before cooling with much water spraying. CONSTITUTION:In this invention, the super heat at near the surface layer of molten pig iron in the mold before cooling with water spreading is made to be &gt;=50 deg.C. In the case of the general casting pig iron, this can apply the well- known cooling method, but in the case of high Si pig iron having &gt;=2.0% Si, as this solidifying temp. is low, the case, which can not cool to the prescribed temp., is developed. In this case, in this invention, by colliding atomized water particles having very fine, such as &lt;=20mum particle size, to a material to be cooled with the air force, sensible heat according to the vaporization of water particles, is utilized. By this method, as the surface of molding pig iron is scarcely wetted and cooling capacity as the same degree as the ordinary water spraying, is obtd., cooling water is not invaded into inner part of the molded pig iron and the bad appearance is not developed.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH0481246A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title PRODUCTION OF CASTING PIG IRON
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T23%3A59%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SATO%20TADASHI&rft.date=1992-03-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH0481246A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true