METHOD FOR CHARGING COKE INTO BLAST FURNACE

PURPOSE:To make reducing gas flow to a center and to stabilize furnace condition by dividing the charge of coke into two series, concentrically charging them into a center part in the furnace and forming the continuous coke layer at the time of laminating ore and the coke in a blast furnace. CONSTIT...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YASUKAWA AKIO, KIGUCHI MITSURU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YASUKAWA AKIO
KIGUCHI MITSURU
description PURPOSE:To make reducing gas flow to a center and to stabilize furnace condition by dividing the charge of coke into two series, concentrically charging them into a center part in the furnace and forming the continuous coke layer at the time of laminating ore and the coke in a blast furnace. CONSTITUTION:In the blast furnace 1 alternately charging the ore and the coke, the charge of coke is divided into two series, e.g. from a coke charging pipe 2 and from a bell 4. This bell 4 is used for forming the coke layer A and the above-mentioned pipe 2 is used for forming the furnace core coke layer B. Then, the coke for forming the above-mentioned coke layer B from this pipe 2 is concentrically charged into center part in the furnace on the ore layer 3 charged at the last time to be the height adding up the layer thickness of coke forming layer A charged in this time and the layer thickness of ore layer 3 charged at the next time. Successively, the coke is charged from the bell 4 so as to cover the ore layer 3 charged at the last time to form only a continuous coke layer in the center part of furnace.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH04176808A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH04176808A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH04176808A3</originalsourceid><addsrcrecordid>eNrjZND2dQ3x8HdRcPMPUnD2cAxy9_RzV3D293ZV8PQL8Vdw8nEMDlFwCw3yc3R25WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BHgYmhuZmFgYWjsbEqAEAV2wk2Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CHARGING COKE INTO BLAST FURNACE</title><source>esp@cenet</source><creator>YASUKAWA AKIO ; KIGUCHI MITSURU</creator><creatorcontrib>YASUKAWA AKIO ; KIGUCHI MITSURU</creatorcontrib><description>PURPOSE:To make reducing gas flow to a center and to stabilize furnace condition by dividing the charge of coke into two series, concentrically charging them into a center part in the furnace and forming the continuous coke layer at the time of laminating ore and the coke in a blast furnace. CONSTITUTION:In the blast furnace 1 alternately charging the ore and the coke, the charge of coke is divided into two series, e.g. from a coke charging pipe 2 and from a bell 4. This bell 4 is used for forming the coke layer A and the above-mentioned pipe 2 is used for forming the furnace core coke layer B. Then, the coke for forming the above-mentioned coke layer B from this pipe 2 is concentrically charged into center part in the furnace on the ore layer 3 charged at the last time to be the height adding up the layer thickness of coke forming layer A charged in this time and the layer thickness of ore layer 3 charged at the next time. Successively, the coke is charged from the bell 4 so as to cover the ore layer 3 charged at the last time to form only a continuous coke layer in the center part of furnace.</description><language>eng</language><subject>CHEMISTRY ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON</subject><creationdate>1992</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19920624&amp;DB=EPODOC&amp;CC=JP&amp;NR=H04176808A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19920624&amp;DB=EPODOC&amp;CC=JP&amp;NR=H04176808A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YASUKAWA AKIO</creatorcontrib><creatorcontrib>KIGUCHI MITSURU</creatorcontrib><title>METHOD FOR CHARGING COKE INTO BLAST FURNACE</title><description>PURPOSE:To make reducing gas flow to a center and to stabilize furnace condition by dividing the charge of coke into two series, concentrically charging them into a center part in the furnace and forming the continuous coke layer at the time of laminating ore and the coke in a blast furnace. CONSTITUTION:In the blast furnace 1 alternately charging the ore and the coke, the charge of coke is divided into two series, e.g. from a coke charging pipe 2 and from a bell 4. This bell 4 is used for forming the coke layer A and the above-mentioned pipe 2 is used for forming the furnace core coke layer B. Then, the coke for forming the above-mentioned coke layer B from this pipe 2 is concentrically charged into center part in the furnace on the ore layer 3 charged at the last time to be the height adding up the layer thickness of coke forming layer A charged in this time and the layer thickness of ore layer 3 charged at the next time. Successively, the coke is charged from the bell 4 so as to cover the ore layer 3 charged at the last time to form only a continuous coke layer in the center part of furnace.</description><subject>CHEMISTRY</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1992</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND2dQ3x8HdRcPMPUnD2cAxy9_RzV3D293ZV8PQL8Vdw8nEMDlFwCw3yc3R25WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8V4BHgYmhuZmFgYWjsbEqAEAV2wk2Q</recordid><startdate>19920624</startdate><enddate>19920624</enddate><creator>YASUKAWA AKIO</creator><creator>KIGUCHI MITSURU</creator><scope>EVB</scope></search><sort><creationdate>19920624</creationdate><title>METHOD FOR CHARGING COKE INTO BLAST FURNACE</title><author>YASUKAWA AKIO ; KIGUCHI MITSURU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH04176808A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1992</creationdate><topic>CHEMISTRY</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><toplevel>online_resources</toplevel><creatorcontrib>YASUKAWA AKIO</creatorcontrib><creatorcontrib>KIGUCHI MITSURU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YASUKAWA AKIO</au><au>KIGUCHI MITSURU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CHARGING COKE INTO BLAST FURNACE</title><date>1992-06-24</date><risdate>1992</risdate><abstract>PURPOSE:To make reducing gas flow to a center and to stabilize furnace condition by dividing the charge of coke into two series, concentrically charging them into a center part in the furnace and forming the continuous coke layer at the time of laminating ore and the coke in a blast furnace. CONSTITUTION:In the blast furnace 1 alternately charging the ore and the coke, the charge of coke is divided into two series, e.g. from a coke charging pipe 2 and from a bell 4. This bell 4 is used for forming the coke layer A and the above-mentioned pipe 2 is used for forming the furnace core coke layer B. Then, the coke for forming the above-mentioned coke layer B from this pipe 2 is concentrically charged into center part in the furnace on the ore layer 3 charged at the last time to be the height adding up the layer thickness of coke forming layer A charged in this time and the layer thickness of ore layer 3 charged at the next time. Successively, the coke is charged from the bell 4 so as to cover the ore layer 3 charged at the last time to form only a continuous coke layer in the center part of furnace.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH04176808A
source esp@cenet
subjects CHEMISTRY
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
title METHOD FOR CHARGING COKE INTO BLAST FURNACE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-29T02%3A54%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YASUKAWA%20AKIO&rft.date=1992-06-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH04176808A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true