JP2575430B

In a process for producing poly (p-phenylenesulfide) from an alkali metal sulfide and a p-dihalobenzene, a product polymer of an advantageously increased molecular weight is obtained by: providing a mixture comprising an alkali metal sulfide, a polar aprotic solvent, a sodium salt of an aliphatic ca...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KATO RIICHI, INOE HIROSHI, OGAWARA KENSUKE
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KATO RIICHI
INOE HIROSHI
OGAWARA KENSUKE
description In a process for producing poly (p-phenylenesulfide) from an alkali metal sulfide and a p-dihalobenzene, a product polymer of an advantageously increased molecular weight is obtained by: providing a mixture comprising an alkali metal sulfide, a polar aprotic solvent, a sodium salt of an aliphatic carboxylic acid represented by the general formula: RCOONa (where R is an aliphtic hydrocarbon group having 1 - 20 carbon atoms), the content of water present in said mixture apart from any water of hydration or crystallization which may be contained in said sulfide and sodium salt being in the range of 5 to 20 moles per mole of said sulfide; removing at least part of the water from said mixture, preferably so as to at least partially dehydrate the said sulphide component; and then contacting the resulting dehydrated mixture with a p-dihalobenzene.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2575430BB2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2575430BB2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2575430BB23</originalsourceid><addsrcrecordid>eNrjZODyCjAyNTc1MTZw4mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8QgNTkbGxKgBACU2G2c</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>JP2575430B</title><source>esp@cenet</source><creator>KATO RIICHI ; INOE HIROSHI ; OGAWARA KENSUKE</creator><creatorcontrib>KATO RIICHI ; INOE HIROSHI ; OGAWARA KENSUKE</creatorcontrib><description>In a process for producing poly (p-phenylenesulfide) from an alkali metal sulfide and a p-dihalobenzene, a product polymer of an advantageously increased molecular weight is obtained by: providing a mixture comprising an alkali metal sulfide, a polar aprotic solvent, a sodium salt of an aliphatic carboxylic acid represented by the general formula: RCOONa (where R is an aliphtic hydrocarbon group having 1 - 20 carbon atoms), the content of water present in said mixture apart from any water of hydration or crystallization which may be contained in said sulfide and sodium salt being in the range of 5 to 20 moles per mole of said sulfide; removing at least part of the water from said mixture, preferably so as to at least partially dehydrate the said sulphide component; and then contacting the resulting dehydrated mixture with a p-dihalobenzene.</description><edition>6</edition><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1997</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970122&amp;DB=EPODOC&amp;CC=JP&amp;NR=2575430B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19970122&amp;DB=EPODOC&amp;CC=JP&amp;NR=2575430B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KATO RIICHI</creatorcontrib><creatorcontrib>INOE HIROSHI</creatorcontrib><creatorcontrib>OGAWARA KENSUKE</creatorcontrib><title>JP2575430B</title><description>In a process for producing poly (p-phenylenesulfide) from an alkali metal sulfide and a p-dihalobenzene, a product polymer of an advantageously increased molecular weight is obtained by: providing a mixture comprising an alkali metal sulfide, a polar aprotic solvent, a sodium salt of an aliphatic carboxylic acid represented by the general formula: RCOONa (where R is an aliphtic hydrocarbon group having 1 - 20 carbon atoms), the content of water present in said mixture apart from any water of hydration or crystallization which may be contained in said sulfide and sodium salt being in the range of 5 to 20 moles per mole of said sulfide; removing at least part of the water from said mixture, preferably so as to at least partially dehydrate the said sulphide component; and then contacting the resulting dehydrated mixture with a p-dihalobenzene.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1997</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZODyCjAyNTc1MTZw4mFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8QgNTkbGxKgBACU2G2c</recordid><startdate>19970122</startdate><enddate>19970122</enddate><creator>KATO RIICHI</creator><creator>INOE HIROSHI</creator><creator>OGAWARA KENSUKE</creator><scope>EVB</scope></search><sort><creationdate>19970122</creationdate><title>JP2575430B</title><author>KATO RIICHI ; INOE HIROSHI ; OGAWARA KENSUKE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2575430BB23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1997</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>KATO RIICHI</creatorcontrib><creatorcontrib>INOE HIROSHI</creatorcontrib><creatorcontrib>OGAWARA KENSUKE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KATO RIICHI</au><au>INOE HIROSHI</au><au>OGAWARA KENSUKE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>JP2575430B</title><date>1997-01-22</date><risdate>1997</risdate><abstract>In a process for producing poly (p-phenylenesulfide) from an alkali metal sulfide and a p-dihalobenzene, a product polymer of an advantageously increased molecular weight is obtained by: providing a mixture comprising an alkali metal sulfide, a polar aprotic solvent, a sodium salt of an aliphatic carboxylic acid represented by the general formula: RCOONa (where R is an aliphtic hydrocarbon group having 1 - 20 carbon atoms), the content of water present in said mixture apart from any water of hydration or crystallization which may be contained in said sulfide and sodium salt being in the range of 5 to 20 moles per mole of said sulfide; removing at least part of the water from said mixture, preferably so as to at least partially dehydrate the said sulphide component; and then contacting the resulting dehydrated mixture with a p-dihalobenzene.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2575430BB2
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title JP2575430B
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T08%3A15%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KATO%20RIICHI&rft.date=1997-01-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2575430BB2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true