METHOD FOR PRODUCING OXO-ACID METAL SALT

To provide a method for producing an oxo-acid metal salt having high degree of freedom in material design and excellent mass productivity.SOLUTION: A method for producing an oxo-acid metal salt includes a step of making an oxo-acid salt react with an alkali-free metal salt in a solvent containing wa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: AKIMOTO JUNJI, NAKAJIMA TOMOHIKO, KATAOKA KUNIMITSU, NAGATA YUTAKA
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator AKIMOTO JUNJI
NAKAJIMA TOMOHIKO
KATAOKA KUNIMITSU
NAGATA YUTAKA
description To provide a method for producing an oxo-acid metal salt having high degree of freedom in material design and excellent mass productivity.SOLUTION: A method for producing an oxo-acid metal salt includes a step of making an oxo-acid salt react with an alkali-free metal salt in a solvent containing water and/or alcohol to obtain a precipitate, and recovering the obtained precipitate by solid-liquid separation, and a step of heat-treating the recovered precipitate at a temperature of 50°C or higher and 1600°C or lower to obtain a heat-treated product. The oxo-acid salt is either one or both of an oxo-acid alkali metal salt and an oxo-acid ammonium salt. The metal element contained in the alkali-free metal salt is at least one kind selected from the group consisting of a typical element, a transition element, and a rare earth element. The final pKa of the conjugate acid of the anion of the alkali-free metal salt is 7.0 or less. The reaction is carried out at a temperature of 0°C or higher and less than 100°C under a pressure of 0.8 atm or more and 1.2 atm or less.SELECTED DRAWING: Figure 1 【課題】物質設計の自由度が高いとともに量産性に優れた、オキソ酸金属塩の製造方法を提供すること。【解決手段】オキソ酸金属塩の製造方法であって、オキソ酸塩とアルカリ非含有金属塩とを水及び/又はアルコールを含有する溶媒中で反応させて沈殿物を得、得られた沈殿物を固液分離にて回収する工程、及び回収した前記沈殿物を50℃以上1600℃以下の温度で熱処理して熱処理物を得る工程、を含み、前記オキソ酸塩は、オキソ酸アルカリ金属塩及びオキソ酸アンモニウム塩のいずれか一方又は両方であり、前記アルカリ非含有金属塩に含まれる金属元素は、典型元素、遷移元素、及び希土類元素からなる群から選択される少なくとも一種であり、前記アルカリ非含有金属塩は、そのアニオンの共役酸の最終pKaが7.0以下であり、前記反応を0.8気圧以上1.2気圧以下の圧力下で0℃以上100℃未満の温度で行う、方法。【選択図】図1
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2024042658A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2024042658A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2024042658A3</originalsourceid><addsrcrecordid>eNrjZNDwdQ3x8HdRcPMPUggI8ncJdfb0c1fwj_DXdXT2dFEAyjr6KAQ7-oTwMLCmJeYUp_JCaW4GJTfXEGcP3dSC_PjU4oLE5NS81JJ4rwAjAyMTAxMjM1MLR2OiFAEAOaYkUw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING OXO-ACID METAL SALT</title><source>esp@cenet</source><creator>AKIMOTO JUNJI ; NAKAJIMA TOMOHIKO ; KATAOKA KUNIMITSU ; NAGATA YUTAKA</creator><creatorcontrib>AKIMOTO JUNJI ; NAKAJIMA TOMOHIKO ; KATAOKA KUNIMITSU ; NAGATA YUTAKA</creatorcontrib><description>To provide a method for producing an oxo-acid metal salt having high degree of freedom in material design and excellent mass productivity.SOLUTION: A method for producing an oxo-acid metal salt includes a step of making an oxo-acid salt react with an alkali-free metal salt in a solvent containing water and/or alcohol to obtain a precipitate, and recovering the obtained precipitate by solid-liquid separation, and a step of heat-treating the recovered precipitate at a temperature of 50°C or higher and 1600°C or lower to obtain a heat-treated product. The oxo-acid salt is either one or both of an oxo-acid alkali metal salt and an oxo-acid ammonium salt. The metal element contained in the alkali-free metal salt is at least one kind selected from the group consisting of a typical element, a transition element, and a rare earth element. The final pKa of the conjugate acid of the anion of the alkali-free metal salt is 7.0 or less. The reaction is carried out at a temperature of 0°C or higher and less than 100°C under a pressure of 0.8 atm or more and 1.2 atm or less.SELECTED DRAWING: Figure 1 【課題】物質設計の自由度が高いとともに量産性に優れた、オキソ酸金属塩の製造方法を提供すること。【解決手段】オキソ酸金属塩の製造方法であって、オキソ酸塩とアルカリ非含有金属塩とを水及び/又はアルコールを含有する溶媒中で反応させて沈殿物を得、得られた沈殿物を固液分離にて回収する工程、及び回収した前記沈殿物を50℃以上1600℃以下の温度で熱処理して熱処理物を得る工程、を含み、前記オキソ酸塩は、オキソ酸アルカリ金属塩及びオキソ酸アンモニウム塩のいずれか一方又は両方であり、前記アルカリ非含有金属塩に含まれる金属元素は、典型元素、遷移元素、及び希土類元素からなる群から選択される少なくとも一種であり、前記アルカリ非含有金属塩は、そのアニオンの共役酸の最終pKaが7.0以下であり、前記反応を0.8気圧以上1.2気圧以下の圧力下で0℃以上100℃未満の温度で行う、方法。【選択図】図1</description><language>eng ; jpn</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240328&amp;DB=EPODOC&amp;CC=JP&amp;NR=2024042658A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240328&amp;DB=EPODOC&amp;CC=JP&amp;NR=2024042658A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>AKIMOTO JUNJI</creatorcontrib><creatorcontrib>NAKAJIMA TOMOHIKO</creatorcontrib><creatorcontrib>KATAOKA KUNIMITSU</creatorcontrib><creatorcontrib>NAGATA YUTAKA</creatorcontrib><title>METHOD FOR PRODUCING OXO-ACID METAL SALT</title><description>To provide a method for producing an oxo-acid metal salt having high degree of freedom in material design and excellent mass productivity.SOLUTION: A method for producing an oxo-acid metal salt includes a step of making an oxo-acid salt react with an alkali-free metal salt in a solvent containing water and/or alcohol to obtain a precipitate, and recovering the obtained precipitate by solid-liquid separation, and a step of heat-treating the recovered precipitate at a temperature of 50°C or higher and 1600°C or lower to obtain a heat-treated product. The oxo-acid salt is either one or both of an oxo-acid alkali metal salt and an oxo-acid ammonium salt. The metal element contained in the alkali-free metal salt is at least one kind selected from the group consisting of a typical element, a transition element, and a rare earth element. The final pKa of the conjugate acid of the anion of the alkali-free metal salt is 7.0 or less. The reaction is carried out at a temperature of 0°C or higher and less than 100°C under a pressure of 0.8 atm or more and 1.2 atm or less.SELECTED DRAWING: Figure 1 【課題】物質設計の自由度が高いとともに量産性に優れた、オキソ酸金属塩の製造方法を提供すること。【解決手段】オキソ酸金属塩の製造方法であって、オキソ酸塩とアルカリ非含有金属塩とを水及び/又はアルコールを含有する溶媒中で反応させて沈殿物を得、得られた沈殿物を固液分離にて回収する工程、及び回収した前記沈殿物を50℃以上1600℃以下の温度で熱処理して熱処理物を得る工程、を含み、前記オキソ酸塩は、オキソ酸アルカリ金属塩及びオキソ酸アンモニウム塩のいずれか一方又は両方であり、前記アルカリ非含有金属塩に含まれる金属元素は、典型元素、遷移元素、及び希土類元素からなる群から選択される少なくとも一種であり、前記アルカリ非含有金属塩は、そのアニオンの共役酸の最終pKaが7.0以下であり、前記反応を0.8気圧以上1.2気圧以下の圧力下で0℃以上100℃未満の温度で行う、方法。【選択図】図1</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDwdQ3x8HdRcPMPUggI8ncJdfb0c1fwj_DXdXT2dFEAyjr6KAQ7-oTwMLCmJeYUp_JCaW4GJTfXEGcP3dSC_PjU4oLE5NS81JJ4rwAjAyMTAxMjM1MLR2OiFAEAOaYkUw</recordid><startdate>20240328</startdate><enddate>20240328</enddate><creator>AKIMOTO JUNJI</creator><creator>NAKAJIMA TOMOHIKO</creator><creator>KATAOKA KUNIMITSU</creator><creator>NAGATA YUTAKA</creator><scope>EVB</scope></search><sort><creationdate>20240328</creationdate><title>METHOD FOR PRODUCING OXO-ACID METAL SALT</title><author>AKIMOTO JUNJI ; NAKAJIMA TOMOHIKO ; KATAOKA KUNIMITSU ; NAGATA YUTAKA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2024042658A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>AKIMOTO JUNJI</creatorcontrib><creatorcontrib>NAKAJIMA TOMOHIKO</creatorcontrib><creatorcontrib>KATAOKA KUNIMITSU</creatorcontrib><creatorcontrib>NAGATA YUTAKA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>AKIMOTO JUNJI</au><au>NAKAJIMA TOMOHIKO</au><au>KATAOKA KUNIMITSU</au><au>NAGATA YUTAKA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING OXO-ACID METAL SALT</title><date>2024-03-28</date><risdate>2024</risdate><abstract>To provide a method for producing an oxo-acid metal salt having high degree of freedom in material design and excellent mass productivity.SOLUTION: A method for producing an oxo-acid metal salt includes a step of making an oxo-acid salt react with an alkali-free metal salt in a solvent containing water and/or alcohol to obtain a precipitate, and recovering the obtained precipitate by solid-liquid separation, and a step of heat-treating the recovered precipitate at a temperature of 50°C or higher and 1600°C or lower to obtain a heat-treated product. The oxo-acid salt is either one or both of an oxo-acid alkali metal salt and an oxo-acid ammonium salt. The metal element contained in the alkali-free metal salt is at least one kind selected from the group consisting of a typical element, a transition element, and a rare earth element. The final pKa of the conjugate acid of the anion of the alkali-free metal salt is 7.0 or less. The reaction is carried out at a temperature of 0°C or higher and less than 100°C under a pressure of 0.8 atm or more and 1.2 atm or less.SELECTED DRAWING: Figure 1 【課題】物質設計の自由度が高いとともに量産性に優れた、オキソ酸金属塩の製造方法を提供すること。【解決手段】オキソ酸金属塩の製造方法であって、オキソ酸塩とアルカリ非含有金属塩とを水及び/又はアルコールを含有する溶媒中で反応させて沈殿物を得、得られた沈殿物を固液分離にて回収する工程、及び回収した前記沈殿物を50℃以上1600℃以下の温度で熱処理して熱処理物を得る工程、を含み、前記オキソ酸塩は、オキソ酸アルカリ金属塩及びオキソ酸アンモニウム塩のいずれか一方又は両方であり、前記アルカリ非含有金属塩に含まれる金属元素は、典型元素、遷移元素、及び希土類元素からなる群から選択される少なくとも一種であり、前記アルカリ非含有金属塩は、そのアニオンの共役酸の最終pKaが7.0以下であり、前記反応を0.8気圧以上1.2気圧以下の圧力下で0℃以上100℃未満の温度で行う、方法。【選択図】図1</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2024042658A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title METHOD FOR PRODUCING OXO-ACID METAL SALT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T13%3A39%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=AKIMOTO%20JUNJI&rft.date=2024-03-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2024042658A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true